EASA Part-66 Module 6 Cheat Sheet

Practice this exam

Ferrous and Non-Ferrous (6.1-6.2)

  • 20% of exam
  • Steel Codes Steel Heat Treatment Aluminium Alloys Aluminium Tempers Other Metals Metal Testing NDT Method Picker Material Identification Picker

Composites and Non-Metallic (6.3)

  • 22.5% of exam
  • Fibres and Resins Core and Sandwich Composite Damage Wood and Fabric Plastics and Sealants

Corrosion (6.4)

  • 10% of exam
  • Corrosion Types Corrosion Control Detection Methods Corrosion Type Picker

Fasteners (6.5)

  • 18.75% of exam
  • Threads and Bolts Nuts and Locking Solid Rivets Blind and Special Fasteners Locking Device Picker

Pipes, Springs, Bearings (6.6-6.8)

  • 10% of exam
  • Rigid Pipes Hoses and Fittings Springs Bearing Types Bearing Defects Tube and Hose Picker

Transmissions and Cables (6.9-6.11)

  • 18.75% of exam
  • Gears and Drives Control Cables Cable Terminals EWIS Wiring Connectors and Bonding

Quick Facts

  • Module 6 Materials and Hardware
  • B1 and B3 80 questions, 100 minutes
  • B2 and B2L 60 questions, 75 minutes
  • Category A 52 questions, 65 minutes
  • Pass mark 75%, no penalty marking
  • Format 3-option multiple choice
  • Pace About 75 seconds each
  • Essays None in Module 6
  • Retake 90 days, 30 retrained
  • Attempts Three per 12 months
  • Validity 10 years for licence
  • Syllabus Applicable 12 June 2024

Temper Codes ME

  • T3 cold work, T6 oven, T73 overaged
  • T3: cold worked T4: naturally aged T6: artificially aged T73: resists stress corrosion

Ferrous vs Non-Ferrous ME

Ferrous

  • Iron based
  • Usually magnetic
  • Red-brown rust

Non-ferrous

  • No iron
  • Non-magnetic
  • White powder product
  • Magnet is the first test

NDT Method Picker ME

  • Crack in steel part → Magnetic particle ( Ferrous only )
  • Crack in aluminium → Dye penetrant ( Surface breaking )
  • Corrosion in lap joint → Eddy current ( Low frequency )
  • Thickness left after blend → Ultrasonic ( Thickness gauge )
  • Hidden internal structure → Radiography ( Sealed areas )
  • Suspect composite disbond → Tap test ( Dull sound )
  • Water inside honeycomb → Radiography ( Shows trapped water )
  • Enclosed bay access → Borescope ( Visual aid )

Steel Codes ME

  • SAE 4130 Chrome-moly, weldable thin tubing
  • SAE 4340 Nickel-chrome-moly, deep hardening
  • First digit Main alloying element class
  • Last two digits Carbon in hundredths percent
  • 300 series Austenitic, non-magnetic, not hardenable
  • 321 and 347 Stabilised against weld decay
  • 400 series Martensitic or ferritic, magnetic
  • PH grades Precipitation hardening stainless steels
  • Ferrite Body-centred cubic, low temperature
  • Austenite Face-centred cubic, above 912 deg C
  • Martensite Hard strained quench structure

T3 vs T6 ME

T3

  • Cold worked
  • Naturally aged
  • Sheet and rivets

T6

  • No cold work
  • Artificially aged
  • Higher yield strength
  • Room ageing vs oven ageing

Material Identification Picker ME

  • Magnet sticks strongly → Carbon or alloy steel ( Ferromagnetic )
  • Stainless but non-magnetic → 300 series ( Austenitic )
  • Lightest metal, very reactive → Magnesium ( Class D fire )
  • Light, grey, very strong → Titanium ( Avoid cadmium )
  • White powdery corrosion → Aluminium alloy ( Oxide product )
  • Red-brown scale → Steel ( Iron oxide )
  • Gold coloured weave → Aramid ( Absorbs moisture )
  • Black stiff fibres → Carbon ( Galvanic risk )

Steel Heat Treatment ME

  • Annealing Furnace cool, softest result
  • Normalising Air cool, finer grain
  • Hardening Quench to form martensite
  • Tempering Reheat, restores some toughness
  • Eutectoid point 727 deg C, 0.77% carbon
  • Carburising Case hardens low-carbon steel
  • Nitriding 500-550 deg C, no quench
  • Case hardening Hard skin, tough core
  • Hydrogen bake 190-205 deg C after plating
  • Stress relief Removes residual working stress

Annealing vs Normalising ME

Annealing

  • Furnace cool
  • Softest, most ductile
  • Coarse pearlite

Normalising

  • Still air cool
  • Tougher and stronger
  • Finer pearlite
  • Furnace cool vs air cool

Aluminium Alloys ME

  • 1xxx Commercially pure aluminium
  • 2xxx Copper alloyed, such as 2024
  • 5xxx Magnesium, good corrosion resistance
  • 6xxx Magnesium and silicon, 6061
  • 7xxx Zinc alloyed, such as 7075
  • 2024-T3 Tough, lower wing skins
  • 7075-T6 Strongest, upper wing skins
  • Alclad Pure aluminium sacrificial cladding
  • Clad layer About 5% each side
  • Cast codes Three digits plus decimal
  • Fusion welding Not for 2024 or 7075

Aluminium Tempers ME

  • F As fabricated, no control
  • O Annealed, softest condition
  • H Strain hardened, not heat treated
  • W Unstable after solution treatment
  • T3 Solution, cold worked, naturally aged
  • T4 Solution treated, naturally aged
  • T6 Solution treated, artificially aged
  • T73 Overaged, resists stress corrosion
  • Quench delay Risks intergranular corrosion
  • Natural ageing Room temperature, over days

Other Metals ME

  • Titanium Strong, light, corrosion resistant
  • Ti-6Al-4V Common alpha-beta titanium alloy
  • Titanium enemies Chlorinated solvents, cadmium contact
  • Magnesium Lightest structural metal, flammable
  • Magnesium fire Class D powder only
  • Inconel Nickel superalloy, hot sections
  • Beryllium copper Non-sparking hand tools
  • Monel Nickel-copper, corrosion resistant
  • Copper High conductivity, bus bars

Metal Testing ME

  • Tensile test Proof stress, tensile strength, elongation
  • Brinell 10 mm ball, 3000 kgf
  • Rockwell C Diamond cone, 150 kgf
  • Vickers Diamond pyramid indenter
  • Charpy Impact energy at notch
  • Ductile-brittle transition Steel goes brittle cold
  • Fatigue limit Steel has endurance limit
  • Aluminium fatigue No true endurance limit
  • Creep Slow strain under sustained load
  • Elastic modulus Stiffness, about 205 GPa steel

B1 Question Shares CO

  • Composites 18, metals 16, fasteners 15
  • 6.3 composites: 18 6.1-6.2 metals: 16 6.5 fasteners: 15 6.9-6.11 drives: 15 6.4 corrosion: 8 6.6-6.8 hardware: 8

Thermoset vs Thermoplastic CO

Thermoset

  • Cures once
  • Frozen prepreg storage
  • Chars if overheated

Thermoplastic

  • Remelts and reshapes
  • Ambient storage
  • Softens with heat
  • One cure vs re-melt

Fibres and Resins CO

  • Carbon fibre Stiff, conductive, galvanically noble
  • Glass fibre Cheaper, insulating, lower stiffness
  • Aramid fibre Tough, absorbs water, fuzzes
  • Boron fibre Very stiff, hard to cut
  • Thermoset Cures once, cannot remelt
  • Thermoplastic Remelts and reshapes repeatedly
  • Matrix job Transfers shear, protects fibres
  • Prepreg storage Frozen at minus 18 deg C
  • Isolation ply Glass between carbon and aluminium

Core and Sandwich CO

  • Nomex core Aramid paper honeycomb
  • Aluminium core 5052 or 5056 honeycomb
  • Foam core Closed cell, easily machined
  • Balsa core End-grain wood core
  • Sandwich action Skins bend, core shears
  • Ribbon direction Cell orientation of core
  • Water ingress Adds weight, freezes, disbonds
  • Potting compound Fills core at fastenings

Composite Damage CO

  • Delamination Plies separated inside laminate
  • Disbond Skin separated from core
  • BVID Barely visible impact damage
  • Resin starvation Too little resin, dry fibres
  • Coin tap Dull note means defect
  • Scarf ratio Typically 30:1 to 60:1
  • Stepped repair Ply by ply landings
  • Vacuum bag About 1 bar consolidation
  • Hot bonder Controlled cure with thermocouples
  • Lightning mesh Copper or aluminium foil

Wood and Fabric CO

  • Sitka spruce Reference aircraft structural wood
  • Grain slope 1 in 15 limit
  • Moisture content 8 to 12 percent
  • Plywood scarf 1 in 12 steepest
  • Decay Any rot means rejection
  • Compression failure Buckled fibres across grain
  • Plywood web Never replace with solid wood
  • Fabric limit 70% of required new strength
  • Grade A cotton 80 lb new, 56 minimum
  • Aluminium dope Blocks ultraviolet from fabric
  • Rib stitching Holds fabric to ribs

Plastics and Sealants CO

  • Acrylic Clear canopies, crazes easily
  • Polycarbonate High impact, scratches easily
  • Transparency cleaning No alcohol or esters
  • Thermoplastic Softens and reforms with heat
  • Thermosetting plastic Chars, cannot be reformed
  • Polysulfide Two-part fuel tank sealant
  • Faying seal Sealant between mating surfaces
  • Fillet seal Bead along joint edge
  • Application life Working time after mixing

Corrosion Cell CO

  • Anode, cathode, electrolyte, path
  • Break one and it stops Anode corrodes Electrolyte carries current Path completes circuit

Galvanic vs Stress Corrosion CO

Galvanic

  • Two dissimilar metals
  • Electrolyte bridge
  • Anode corrodes away

Stress corrosion

  • One susceptible alloy
  • Sustained tensile stress
  • Brittle branching cracks
  • Two metals vs one stressed

Corrosion Type Picker CO

  • Two dissimilar metals touching → Galvanic ( Needs electrolyte )
  • Layers lifting apart → Exfoliation ( Rolled sections )
  • Cracks under steady tension → Stress corrosion ( Susceptible alloy )
  • Black powder at joint → Fretting ( Micro-movement )
  • Worm tracks under paint → Filiform ( High humidity )
  • Deep local holes → Pitting ( Chloride attack )
  • Attack along grain boundaries → Intergranular ( Quench delay )
  • Sludge in fuel tank → Microbial ( Water present )
  • Trapped moisture in gap → Crevice ( Oxygen cell )
  • Uniform dull etched surface → Surface corrosion ( General attack )

Corrosion Types CO

  • Surface General uniform oxide attack
  • Pitting Deep local holes, chlorides
  • Galvanic Dissimilar metals plus electrolyte
  • Intergranular Attack along grain boundaries
  • Exfoliation Layers lift in rolled sections
  • Stress corrosion Tension plus corrosive environment
  • Fretting Micro-movement between clamped parts
  • Filiform Worm tracks under paint
  • Crevice Trapped moisture, oxygen difference
  • Microbial Fuel tank fungus acids
  • Area effect Big cathode, small anode

Intergranular vs Exfoliation CO

Intergranular

  • Grain boundary attack
  • Often invisible outside
  • Heat treatment fault

Exfoliation

  • Layers lift and flake
  • Rolled or extruded parts
  • Visible swelling
  • Same attack, visible layering

Corrosion Control CO

  • Four requirements Anode, cathode, electrolyte, path
  • Anodising Electrolytic thickened oxide film
  • Alodine Chromate conversion, self-healing
  • Cadmium plate Sacrificial coating on steel
  • Epoxy primer Inhibiting pigment under topcoat
  • CIC Penetrating water-displacing compound
  • Banned on aluminium Steel wool and steel brushes
  • Blend out Smooth taper within manual limits
  • Drain holes Keep clear of sealant
  • Humidity threshold Attack rises above 60%

Detection Methods CO

  • Visual First and primary method
  • Eddy current Second layer lap joint
  • Ultrasonic Remaining thickness measurement
  • Radiography Sealed or hidden structure
  • Borescope Enclosed bays and ducts
  • Blistering Paint lifted by product
  • White powder Aluminium corrosion product
  • Red-brown scale Iron oxide on steel
  • Black powder Fretting on aluminium joints

Rivet Head Marks FA

  • A plain, AD dimple, D dot, DD dash
  • A: 1100 AD: 2117 D: 2017 DD: 2024 B: 5056 cross

AN vs MS FA

AN

  • Air Force-Navy standard
  • Older hardware series
  • Common general bolts

MS

  • Military Standard
  • Newer replacement series
  • Tighter definition
  • Older AN, newer MS

Locking Device Picker FA

  • Drilled bolt, tension joint → Castellated nut ( Cotter pin )
  • Hot zone near exhaust → All-metal stiffnut ( No nylon )
  • Cool accessible joint → Nylon insert nut ( Under 121 deg C )
  • No access behind panel → Anchor nut ( Riveted plate )
  • Group of drilled fittings → Safety wire ( Pull to tighten )
  • Turnbuckle needs locking → Clip or safety wire ( Clip single use )
  • Shaft end retention → Circlip ( No clamp load )
  • Quick panel removal → Turnlock fastener ( Non-structural only )
  • Permanent high clamp load → Lockbolt ( Swaged collar )

Threads and Bolts FA

  • UNC Coarse, soft metals and castings
  • UNF Fine, aircraft structural fasteners
  • Class 3 Tight fit for structure
  • Pitch Distance between adjacent threads
  • Lead Axial advance per turn
  • Pitch diameter Where tooth equals groove
  • AN bolt diameter Digit equals 16ths inch
  • AN bolt dash Inches then eighths length
  • Grip length Match clamped material thickness
  • Alloy steel head Raised cross or asterisk
  • Stainless bolt head Single raised dash
  • Aluminium bolt head Two raised dashes
  • Close tolerance Raised triangle, reamed hole
  • Stud Coarse into casting, fine outside

Thread Choice FA

  • Coarse into soft, fine into steel
  • UNC: castings UNF: structure Class 3: tight fit

Castellated vs Self-Locking FA

Castellated

  • Cotter pin fitted
  • Positive mechanical lock
  • Needs drilled bolt

Self-locking

  • Prevailing torque
  • No drilling needed
  • Limited reuse
  • Positive lock vs friction

Nuts and Locking FA

  • Castellated nut Cotter pin through drilled bolt
  • Never slacken Tighten to align holes
  • Nylon insert nut Not above 121 deg C
  • All-metal stiffnut For high temperature joints
  • Thread showing At least one past nut
  • Anchor nut Riveted plate, blind access
  • Shear nut Thin nut, shear loads
  • Safety wire size 0.032 inch usual minimum
  • Wire twists Tight, even, per the manual
  • Wire direction Pull toward tightening rotation
  • Tab washer Bent against nut flat
  • Torque rule Turn the nut, not bolt
  • Torque adapter Reduce the wrench setting
  • Self-tapping screw Never structural on aircraft

Solid Rivets FA

  • A = 1100 Plain head, non-structural
  • AD = 2117 Dimple head, field standard
  • D = 2017 Raised dot, higher strength
  • DD = 2024 Double dash, icebox rivet
  • B = 5056 Raised cross, for magnesium
  • M = Monel Two dimples, stainless structure
  • Icebox storage Below minus 18 deg C
  • Drive window Minutes after leaving freezer
  • Shop head 1.5D wide, 0.5D high
  • Protrusion 1.5D of shank before driving
  • Edge distance 2D minimum from edge
  • Rivet pitch 3D minimum along row
  • Rivet number 32nds diameter, 16ths length
  • MS20470 Universal head solid rivet
  • Dimple or countersink Thin sheet must dimple

Blind and Special Fasteners FA

  • Friction lock Stem can vibrate out
  • Mechanical lock Locked collar, structural use
  • CherryMAX One tool, all grips
  • Hi-Lok Hex socket, shear-off collar
  • Hi-Shear Steel pin, swaged collar
  • Lockbolt Swaged collar, pintail breaks
  • Dzus Spiral cam, quarter turn
  • Camloc Cross-pin into cam receptacle
  • Turnlock grip Match total panel thickness
  • Circlip Axial retention, no clamping
  • Smoking rivet Grey streak, loose fastener

Bearing Damage PI

  • True is a hit, false is a shake
  • True: shock load False: vibration in transit Spalling: fatigue flakes Fluting: electrical arcing

37 vs 45 Degree Flare PI

37 degree

  • Aircraft AN standard
  • Sleeve and nut
  • Fuel and hydraulics

45 degree

  • Automotive commercial
  • Not for aircraft
  • Crushes AN flare
  • Never mix flare angles

Tube and Hose Picker PI

  • Low pressure fuel line → 5052-O aluminium ( Soft tube )
  • High pressure hydraulics → Stainless steel tube ( Fire zones too )
  • Weight critical, high pressure → Titanium tube ( 3Al-2.5V )
  • Relative movement between parts → Flexible hose ( Allow slack )
  • Skydrol system hose → Butyl or PTFE ( Never Buna-N )
  • Fuel or oil hose → Buna-N or PTFE ( Never butyl )
  • Soft tube, small diameter → Double flare ( 37 degrees )
  • Flare not permitted → Flareless fitting ( Bite ferrule )

Rigid Pipes PI

  • Tube size Outside diameter in 16ths
  • Wall thickness Quoted in thousandths inch
  • 5052-O Low pressure fuel lines
  • 6061-T6 Higher strength aluminium lines
  • Stainless tube High pressure and fire zones
  • Titanium tube Weight critical high pressure
  • Bend radius About three times diameter
  • Flattening limit Keep 75% of diameter
  • Never straight Add bends to absorb flex
  • Cushioned clamp Supports line, bonds structure

Brinelling vs Spalling PI

Brinelling

  • Indentations in raceway
  • Shock or press load
  • Grinding marks remain

Spalling

  • Metal flakes away
  • Subsurface fatigue
  • Gets worse quickly
  • Dents vs flaking

Hoses and Fittings PI

  • AN flare 37 degree flare angle
  • Automotive flare 45 degrees, never mixed
  • Double flare Soft tube, 3/8 and smaller
  • Flareless fitting Ferrule bites tube wall
  • Three-piece union Nut, sleeve and union
  • Sleeve job Protects flare from twisting
  • Lay line Straight means no twist
  • Hose slack 5 to 8 percent
  • Buna-N Fuel and oil, not Skydrol
  • Butyl Skydrol only, not petroleum
  • PTFE Suits all aircraft fluids
  • Fuel line marking Red band with stars
  • Oxygen line marking Green band with rectangles

Springs PI

  • Compression spring Resists being pushed shorter
  • Extension spring Resists being pulled longer
  • Torsion spring Resists twist about axis
  • Leaf spring Bending strip, high load
  • Belleville washer Coned disc, very stiff
  • Series stack More deflection, same load
  • Parallel stack More load, same deflection
  • Spring rate Load per unit deflection
  • Spring index Mean diameter over wire
  • Free length Checked for permanent set
  • Shot peening Compressive skin, longer life
  • Never stretch A sagged spring is scrap

Bearing Types PI

  • Plain bearing Sliding contact, high shock
  • Bushing Renewable plain bearing liner
  • Sintered bronze Oil impregnated, never degrease
  • Ball bearing Point contact, high speed
  • Roller bearing Line contact, heavy radial
  • Needle roller Compact, high radial capacity
  • Taper roller Combined radial and thrust
  • Angular contact Thrust from one direction
  • Spherical bearing Self-aligning rod ends
  • Cage Keeps elements evenly spaced
  • Hydrodynamic film Oil wedge lifts journal

Bearing Defects PI

  • True brinelling Static shock load indentations
  • False brinelling Vibration while not turning
  • Spalling Fatigue flaking of raceway
  • Fluting Electrical arcing washboard marks
  • Overheating Discoloured rings and elements
  • Contamination Scratches and dull raceways
  • Grease fill 30 to 50 percent
  • Press rule Press only the fitted ring
  • Never spin dry Compressed air wrecks bearings

Cable Codes TR

  • 7x19 flies, 7x7 guides, 1x19 stays
  • 7x19: primary controls 7x7: secondary runs 1x19: rigid ties 1/8 in minimum

7x7 vs 7x19 TR

7x7

  • 49 wires total
  • Less flexible
  • Secondary and trim runs

7x19

  • 133 wires total
  • Extra flexible
  • Primary controls over pulleys
  • More wires, more flexible

Gears and Drives TR

  • Spur gear Parallel shafts, no thrust
  • Helical gear Smoother, creates axial thrust
  • Double helical Cancels the axial thrust
  • Bevel gear Drives intersecting shafts
  • Worm drive High reduction, often self-locking
  • Rack and pinion Rotary into linear motion
  • Epicyclic gear Sun, planets, ring, carrier
  • Gear ratio Driven teeth over driving
  • Idler gear Reverses direction, same ratio
  • Compound train Multiply the stage ratios
  • Backlash Clearance between mating teeth
  • Pressure angle Usually 20 degree involute
  • Tooth contact Centred oval marking pattern
  • Chain stretch Pin and bushing wear
  • Timing belt Toothed, positive no-slip drive

Swaged vs Nicopress TR

Swaged terminal

  • Machine swaged fitting
  • Full cable strength
  • Gauge checked

Nicopress sleeve

  • Hand tool compression
  • Field repair method
  • Sleeve and thimble
  • Shop terminal vs field loop

Control Cables TR

  • 7x7 Seven strands of seven
  • 7x19 Extra flexible, primary controls
  • 1x19 Non-flexible, straight tie rods
  • Galvanised cable Better bending fatigue life
  • Stainless cable Better corrosion, lower fatigue
  • Minimum size 1/8 in, primary controls
  • Measure across Strand crowns, not valleys
  • Pre-stretch Removes constructional stretch first
  • Proof load 60% of breaking strength
  • Reject cable Popped core or loose strands
  • Critical fatigue area One broken wire rejects
  • Fairlead limit 3 degrees maximum deflection
  • Tension regulator Holds tension despite temperature

Cable Terminals TR

  • MS20668 Swaged eye end fitting
  • MS20667 Swaged fork end fitting
  • MS20664 Single shank ball end
  • Go/No-Go gauge Checks swaged shank size
  • Witness mark Paint shows terminal slip
  • Nicopress sleeve Field swaged compression sleeve
  • Turnbuckle threads Maximum three exposed each end
  • Left-hand end Grooved or knurled terminal
  • Turnbuckle wire Four wraps around the shank
  • Locking clip Single use, never reused
  • Tensiometer Riser plus temperature chart
  • Pulley guard Stops cable leaving groove

EWIS Wiring TR

  • Stranded only Solid airframe wire banned
  • AWG Bigger number, smaller wire
  • Tin plating Up to 150 deg C
  • Silver plating Up to 200 deg C
  • Nickel plating Up to 260 deg C
  • Red plague Silver plated copper corrosion
  • Kapton Arc tracking risk, legacy
  • ETFE Modern non-arc-tracking insulation
  • Bundle bend radius 10 times bundle diameter
  • Coax bend radius 6 times outside diameter
  • Route wires Above fuel and hydraulic lines
  • Drip loop Before connectors and bulkheads
  • Cable tie Cut flush with proper tool
  • Voltage drop Sizes long continuous runs

Connectors and Bonding TR

  • MIL-DTL-38999 Standard circular aircraft connector
  • Scoop proof Shell reaches pins first
  • Polarising keys Prevent cross-mating connectors
  • Crimp Gas-tight, vibration resistant joint
  • Solder Brittle joint, wicking risk
  • M22520 Ratcheting calibrated crimp tool
  • Red tool Inserts size 20 contacts
  • White tool Extracts size 20 contacts
  • Coax 50 ohm Aircraft radio transmission line
  • Coax 75 ohm Video, not aircraft radio
  • Bond resistance Typically under 0.003 ohm
  • Screen earthing One end only, short
  • Ignition screen Suppresses interference and flashover

Common Traps

Tempering vs annealing

  • Tempering follows a quench ≠ Annealing softens from scratch

Galvanic vs intergranular

  • Galvanic needs two metals ≠ Intergranular follows heat treatment

Hardness vs strength

  • Hardness resists indentation ≠ Strength resists breaking load

Rivet AD vs DD

  • AD is 2117 dimple ≠ DD is 2024 icebox

Flare angle mix

  • Aircraft flares 37 degrees ≠ Automotive flares 45 degrees

Idler gear myth

  • Idler reverses direction ≠ Idler keeps the ratio

MPI on light alloy

  • Magnetic particle needs iron ≠ Aluminium needs eddy current

Turnbuckle threads

  • Three threads may show ≠ More means weak engagement

Nylon nut heat

  • Nylon fails above 121 deg C ≠ All-metal nut for heat

Skydrol hose liner

  • Butyl suits Skydrol ≠ Buna-N swells in Skydrol

Stop-drilling is not repair

  • Stop-drill halts the crack ≠ Reinforcement restores the strength

Last Minute

  • 1. B1: 80 questions in 100 minutes
  • 2. Pass 75%, no penalty marking
  • 3. Composites 22.5% is the heaviest band
  • 4. T3 cold worked; T6 oven aged
  • 5. AD 2117 dimple; DD 2024 icebox
  • 6. Shop head 1.5D wide, 0.5D high
  • 7. Edge distance 2D; rivet pitch 3D
  • 8. Galvanic needs two metals plus electrolyte
  • 9. Stress corrosion needs sustained tension
  • 10. Magnetic particle works on steel only
  • 11. Aircraft flare angle is 37 degrees
  • 12. 7x19 cable for primary controls
  • 13. Turnbuckle: three threads maximum showing
  • 14. Nylon nut limit 121 deg C
  • 15. Gear ratio is driven over driving
  • 16. Wire bundle bend: 10 times diameter
  • 17. Press only on the fitted ring
  • 18. Never stretch a sagged spring

EASA Part-66 Module 06 — Materials and Hardware

  • Practice Questions 125 questions Study Guide 40 topics Cheat Sheet 314 facts Flashcards 50 cards