Study guide

2.4 Forms of Corrosion: Uniform, Galvanic, Pitting & Crevice

AMPP CP1 Cathodic Protection Tester Study Guide Exam

Track your progress as you read

Finished sections get a check mark.

1 Chapter 1: Introduction & CP Exam Overview

About the AMPP CP1 Tester Exam & Certification Path How to Study for CP1 & Navigate This Guide Corrosion Science & Industry Terminology Glossary Field Mathematics & Ohm's Law Fundamentals AMPP Ethics for the Corrosion Professional

2 Chapter 2: Fundamentals of Electrochemistry & Corrosion Cells

2.1 The Corrosion Cell: Anode, Cathode, Electrolyte & Metallic Path 2.2 Anodic & Cathodic Reactions on Carbon Steel 2.3 Galvanic Series & Electromotive Force (EMF) Series 2.4 Forms of Corrosion: Uniform, Galvanic, Pitting & Crevice 2.5 Factors Affecting Corrosion Rates: Oxygen, pH, Temperature & Flow

3 Chapter 3: Principles of Cathodic Protection

3.1 Cathodic Protection Theory & Mixed-Potential Diagrams 3.2 Galvanic (Sacrificial Anode) CP Systems 3.3 Impressed Current Cathodic Protection (ICCP) Systems 3.4 Sacrificial Anode Materials: Mg, Zn, & Al Alloys 3.5 ICCP Anode Materials: MMO, Graphite, HSCI, & Platinum

4 Chapter 4: Electrical Circuit Analysis for CP

4.1 Ohm's Law Applications in CP Circuits 4.2 Series & Parallel Resistance in CP Groundbeds & Piping 4.3 Kirchhoff's Voltage & Current Laws in Network Piping 4.4 Shunts: Types, Ratings & Current Calculations 4.5 Rectifier Operation & Transformer Tap Adjustments

5 Chapter 5: Reference Electrodes & Half-Cell Potentials

5.1 Copper/Copper Sulfate (CSE) Reference Electrode Construction & Maintenance 5.2 Silver/Silver Chloride (Ag/AgCl) & Zinc Reference Electrodes 5.3 Converting Potentials Between Reference Electrodes 5.4 Reference Electrode Care, Temperature Correction & Contamination Checks 5.5 High-Impedance Voltmeters & Contact Resistance Errors

6 Chapter 6: Field Measurement & Potential Criteria

6.1 Structure-to-Electrolyte Potential Measurement Procedures 6.2 The -850 mV CSE Polarized Criterion (NACE SP0169) 6.3 The 100 mV Polarization Decay Criterion 6.4 Understanding IR Drop & The Instant-Off Interruption Technique 6.5 Native, On, Polarized, & Off Potentials Comparison

7 Chapter 7: Advanced Field Survey Techniques

Soil Resistivity Testing: Wenner 4-Pin Method (ASTM G57) Soil Pin Spacing, Layering & Corrosivity Classification Close Interval Potential Surveys (CIPS) Direct Current Voltage Gradient (DCVG) Coating Fault Surveys Cathodic Protection Coupons for IR-Free Potential Measurements

8 Chapter 8: Test Stations, Isolation & Stray Current

8.1 Test Station Types, Lead Wires & Commissioning Inspection 8.2 Electrical Isolation Joints & Dielectric Flange Testing 8.3 Casing Isolation & Shorted Casing Testing 8.4 DC Stray Current Interference: Detection & Mitigation 8.5 AC Stray Current Interference & Induction Hazards (NACE SP0177)

9 Chapter 9: Industry Standards & Field Documentation

9.1 NACE SP0169: External Corrosion Control Overview 9.2 NACE TM0497: Measurement Techniques Standard 9.3 Regulatory Compliance: PHMSA, DOT, & EPA Requirements 9.4 CP Data Collection, Logging & Quality Assurance 9.5 Rectifier Maintenance & Routine Inspection Logs 9.6 Anode Groundbed Testing & Resistance Measurements

10 Chapter 10: Electrical & Operational Safety for CP Personnel

10.1 Rectifier Electrical Safety, Lockout/Tagout (LOTO) & NFPA 70E 10.2 AC Induction Hazards Near High-Voltage Power Lines 10.3 Hazardous Atmospheres & Confined Space Safety at Test Vaults 10.4 Personal Protective Equipment (PPE) & Arc Flash Protection 10.5 Excavation, Trenching & Underground Utility Location (811) 10.6 Stop-Work Authority & Emergency Response Procedures

2.4 Forms of Corrosion: Uniform, Galvanic, Pitting & Crevice

Key Takeaways Explain This Topic AI

Uniform corrosion is characterized by relatively even metal loss over the entire surface and is generally predictable.

Galvanic corrosion occurs when two dissimilar metals are electrically coupled in a common electrolyte.

Pitting corrosion is highly localized, penetrating deeply into the metal while surrounding areas remain largely unaffected.

Crevice corrosion occurs in narrow spaces where stagnant electrolyte accumulates, leading to localized chemistry changes.

Localized forms of corrosion (like pitting and crevice) are often more dangerous than uniform corrosion because they can cause rapid failure with little overall mass loss.

Last updated: July 2026

  • Forms of Corrosion: Uniform, Galvanic, Pitting & Crevice
  • Recognizing Corrosion Types

Corrosion does not always manifest in the same way. The specific mechanism of degradation depends on the metal, the environment, the structural design, and the presence of other materials. Corrosion professionals generally categorize corrosion into several distinct forms. Recognizing the form of corrosion is the first step in diagnosing the root cause of a failure and designing an appropriate mitigation strategy.

While there are many specific forms of corrosion (such as stress corrosion cracking, erosion-corrosion, and intergranular corrosion), this section focuses on the four fundamental types most frequently encountered in general infrastructure and pipeline systems: Uniform, Galvanic, Pitting, and Crevice corrosion.

1. Uniform (General) Corrosion

Uniform corrosion, also known as general corrosion, is characterized by an electrochemical reaction that proceeds relatively evenly over the entire exposed surface of the metal.

In uniform corrosion, the anodic and cathodic sites are not fixed; they constantly shift across the surface of the metal. This results in a relatively uniform thinning of the material over time. A common example is a piece of unprotected carbon steel left exposed to the atmosphere, which will develop a relatively even layer of rust over its entire surface.

Characteristics of Uniform Corrosion:

Predictability: Because the metal loss is even, uniform corrosion is the easiest form to predict and manage. Engineers can calculate the corrosion rate (e.g., in mils per year, mpy) and design the structure with a "corrosion allowance"—extra thickness specifically intended to be corroded away over the design life of the asset.

Total Mass Loss: Uniform corrosion accounts for the greatest total amount of metal destroyed on a global scale.

Mitigation: It is relatively easy to mitigate using protective coatings, cathodic protection, or by changing the environment (e.g., using inhibitors).

Despite being responsible for the most metal loss by tonnage, it is rarely the cause of sudden, catastrophic structural failures because its progress is visible and predictable.

2. Galvanic (Bimetallic) Corrosion

Galvanic corrosion occurs when two electrochemically dissimilar metals are electrically connected and exposed to the same electrolyte. As discussed in the previous section on the Galvanic Series, this creates a macro-corrosion cell.

Mechanism of Galvanic Corrosion:

The more active metal (higher on the Galvanic Series) becomes the anode and suffers accelerated corrosion.

The more noble metal (lower on the Galvanic Series) becomes the cathode and its corrosion rate is reduced or halted.

The driving force is the potential difference between the two metals.

Factors Influencing Galvanic Corrosion:

Area Ratio: This is the most critical factor. A small anode connected to a large cathode (e.g., a steel rivet in a large copper plate) will result in extremely rapid, severe corrosion of the small anode because the large cathode demands a massive amount of electrons. Conversely, a large anode connected to a small cathode (e.g., a copper rivet in a large steel plate) will result in minor, widely distributed corrosion on the anode.

Electrolyte Conductivity: A highly conductive electrolyte (like seawater) allows the galvanic current to spread over a larger area. A low-conductivity electrolyte restricts the severe galvanic corrosion to the immediate area where the two metals meet.

3. Pitting Corrosion

Pitting is an extremely localized form of corrosion that leads to the creation of small holes or "pits" in the metal. It is one of the most destructive and insidious forms of corrosion.

Mechanism of Pitting:

Pitting often initiates at localized defects in a protective coating or at weak spots in a metal's naturally occurring passive oxide film (common in stainless steels and aluminum). Once a pit initiates, the chemistry inside the pit changes drastically compared to the bulk electrolyte outside.

The inside of the pit becomes the anode.

The large surrounding surface area remains the cathode.

The environment inside the pit becomes highly acidic and concentrated with aggressive ions (like chlorides), accelerating the dissolution of metal at the base of the pit.

Characteristics of Pitting:

Unpredictable: Pits are hard to detect because they are small, often covered by corrosion products, and grow rapidly inward.

Dangerous: Pitting can cause a pipeline to leak or a pressure vessel to fail even when the total weight loss of the structure is virtually zero. It bypasses corrosion allowances designed for uniform corrosion.

Autocatalytic: Once started, the conditions inside the pit drive the reaction faster and faster.

4. Crevice Corrosion

Crevice corrosion is another highly localized form of corrosion that occurs within narrow crevices or shielded areas on metal surfaces where a stagnant solution can accumulate.

Mechanism of Crevice Corrosion:

Crevices can be created by structural features (lap joints, flanges, threads, under gasket materials) or by environmental factors (deposits of sand, dirt, or bio-fouling). The mechanism is very similar to pitting.

Initially, uniform corrosion occurs both inside and outside the crevice.

Because the crevice is narrow and stagnant, the dissolved oxygen inside the crevice is quickly depleted by the cathodic reaction.

Oxygen remains plentiful on the surfaces outside the crevice. This creates a concentration cell.

The oxygen-depleted area inside the crevice becomes a fixed anode, while the oxygen-rich area outside becomes the cathode.

Like pitting, the chemistry inside the crevice becomes highly acidic and concentrated with aggressive ions, leading to rapid, localized metal loss.

Mitigation of Localized Corrosion

Preventing pitting and crevice corrosion involves careful material selection (e.g., using alloys resistant to specific environments), designing structures to eliminate crevices and stagnant pooling, maintaining clean surfaces, and applying effective cathodic protection, which can suppress the anodic reactions even within pits and crevices if sufficient current can reach those areas.

Form of Corrosion Characteristics Primary Cause Danger Level (Structural)

Uniform Even metal loss, predictable rate General exposure to aggressive environment Low to Moderate (predictable)

Galvanic Accelerated corrosion near a dissimilar metal Electrical coupling of dissimilar metals Moderate to High (depends on area ratio)

Pitting Deep, narrow holes, minimal surface metal loss Breakdown of passive films, localized chemical changes High (rapid penetration, hard to detect)

Crevice Localized attack in narrow gaps Stagnant electrolyte, oxygen depletion cells High (rapid penetration in hidden areas)