Study guide
4.3 How Discontinuities Distort Magnetic Fields
ASNT NDT Level II Certification Exam
Track your progress as you read
Finished sections get a check mark.
1 Introduction & Exam Overview
1.1 Current Exam Facts 1.2 Certification Paths: SNT-TC-1A, CP-189, and ASNT Central Certification 1.3 Level I vs Level II vs Level III Responsibilities 1.4 Application, Scheduling, Identification, and Retake Rules
2 Eligibility, Fees & Recertification
2.1 Training Hours, Experience Days, and Documentation 2.2 Vision, Practical Exams, and the Employer's Written Practice 2.3 Fees, Validity, Recertification, and 529 Funding
3 NDT Fundamentals & Method Selection
3.1 What NDT Can and Cannot Detect 3.2 Surface vs Subsurface and Method Selection Logic 3.3 Product Forms: Welds, Castings, Forgings, Wrought, In-Service Damage
4 MT Principles & Flux Fields
4.1 Magnetism, Permeability, and Flux Leakage 4.2 Flux Fields: Circular vs Longitudinal 4.3 How Discontinuities Distort Magnetic Fields
5 MT Magnetization & Demagnetization
5.1 Magnetization by Electric Current: Contact, Prods, Central Conductor 5.2 Selecting the Proper Magnetization Method: Coils, Yokes, Current Type 5.3 Demagnetization Procedures and Residual Field Limits
6 MT Equipment, Evaluation & Process Control
6.1 MT Equipment, Media, and Lighting 6.2 Types of Discontinuities Detected by MT 6.3 MT Evaluation Techniques 6.4 Quality Control of MT Equipment and Processes
7 PT Principles & Materials
7.1 PT Principles: Capillarity, Wetting, and Process Physics 7.2 Penetrant Types, Methods, and Sensitivity Classes 7.3 Developers and Process Sequence Controls
8 PT Method Selection & Process Control
8.1 Selecting the Appropriate PT Method for the Job 8.2 Surface Preparation, Dwell, Removal, and Lighting 8.3 Station Equipment, Process Control, and Safety
9 PT Indications, Evaluation & Standards
9.1 Relevant, Nonrelevant, and False Indications 9.2 Evaluating Indication Size, Shape, and Persistence 9.3 PT Procedures, ASTM/ASME Standards, and Acceptance
10 RT Principles & Exposure Technique
10.1 Radiation Physics: X-ray vs Gamma, Energy, and Attenuation 10.2 Exposure Geometry, Inverse Square Law, and Geometric Unsharpness 10.3 Radiographic Technique: kV, mA-min, Screens, and Source Selection
11 RT Image Quality, Processing & Indications
11.1 Film, Digital Detectors, Density, and Image Quality Indicators 11.2 Darkroom Facilities, Processing, and Artifact Control 11.3 Radiographic Indications, Discontinuities, and Defects
12 RT Product Discontinuities & Radiation Safety
12.1 Manufacturing Processes and Associated Discontinuities 12.2 Radiological Safety: Time, Distance, Shielding, and Dose Limits 12.3 RT Procedures, Codes, and Viewing Practice
13 UT Principles & Techniques
13.1 Sound Propagation, Modes, Velocity, and Wavelength 13.2 Transducers, Couplant, and Straight-Beam Techniques 13.3 Angle-Beam Techniques, Snell's Law, and Skip Distance
14 UT Calibration & Base Material
14.1 Calibration Blocks, DAC, TCG, and Sensitivity Setting 14.2 Evaluating Base-Material Product Forms 14.3 Evaluating Weldments
15 UT Bonds, Detection & Evaluation
15.1 Evaluating Bonded Structures 15.2 Discontinuity Detection and Characterization 15.3 General Evaluation, Sizing, and Acceptance Logic
16 VT Scope, Vision & Lighting
16.1 Purpose and Scope of VT 16.2 Elements of Vision 16.3 Elements of Lighting 16.4 Contrast and Resolution
17 VT Optics, Equipment & Discontinuities
17.1 Optics and Magnification 17.2 VT Equipment: Direct, Remote, and Measuring Tools 17.3 Visual Appearance of Discontinuities
18 VT Evaluation, Codes & Employer Topics
18.1 Evaluation and Reporting 18.2 Codes, Standards, and Specifications 18.3 Employer-Specific Topics and Written-Practice Controls
19 Specific Exam: Codes & Sectors
19.1 How the Specific Exam Differs from the General Exam 19.2 General Industry Codes and Procedure Use 19.3 Pressure Equipment Sector Codes (ASME, NBIC, API context)
20 Specific Exam: Applications & Techniques
20.1 Applications: Matching Method to Product Form and Access 20.2 Technique Selection and Essential Variables 20.3 Procedure Compliance, Reporting, and Acceptance/Rejection
21 Exam Strategy & Maintenance
21.1 Timed 50+40 Strategy and CBT Rules 21.2 Common Traps by Method 21.3 Weak-Area Review and Recertification Planning
4.3 How Discontinuities Distort Magnetic Fields
Key Takeaways Explain This Topic AI
Leakage is strongest when the discontinuity cuts the flux lines, ideally near 90°; a tight crack parallel to the field may produce no reportable indication.
Surface-breaking cracks produce sharp linear leakage; subsurface inclusions leak more weakly and broadly; rounded porosity is a poor magnetic-particle target.
A permeability change without a void — cold work, a hard heat-affected zone, or magnetic writing — can collect particles and is often nonrelevant.
Alternating current is surface-only because of skin effect; half-wave and direct current reach deeper, and half-wave pulses help keep dry particles mobile.
Classify particle buildups as relevant (evaluate the discontinuity), nonrelevant (geometry or a permitted condition), or false (no leakage field).
Last updated: August 2026
The third official MT general topic prior to 15 December 2026 is Effects of Discontinuities on Materials . The exam is asking how a real crack, a buried inclusion, a pore, a hardness change, or a keyway each distorts the flux — and how that distortion looks in particles.
Leakage is strongest when the discontinuity cuts the flux
Flux lines behave like a crowd in a corridor. A door that stands across the corridor stops people; a door that lies along the wall barely does. A discontinuity that is perpendicular to the flux (the crack length cuts the lines at about 90° ) produces the strongest leakage field. As the angle closes, leakage falls. A tight crack parallel to the flux may produce no reportable indication even though the crack is real and rejectable by another method.
That is the same 90° rule as Flux Fields, now stated from the discontinuity's point of view. Interpretation items use it: a longitudinal seam that showed on the head shot and vanished on the coil shot is behaving exactly as physics predicts, not 'healing' between stations.
A 45° crack still leaks, but more weakly. Do not treat 45° as a substitute for two perpendicular magnetizations. The procedure still requires the second direction so that some shot is close to 90° for every possible crack orientation.
Surface-breaking cracks, subsurface inclusions, and rounded porosity
Not every void leaks the same way. Shape, sharpness, and depth decide how much flux is forced out of the surface where particles live.
Condition How it distorts flux Typical particle pattern Easy to miss when
Surface-breaking crack (fatigue, quench, grinding, open seam) Thin, sharp air gap at the surface; flux is forced out over a short path Sharp, tight, linear buildup Field is parallel to the crack; particles or lighting are wrong
Near-surface / subsurface crack or stringer Flux can still detour inside the metal; weaker, broader leakage reaches the surface Fuzzy, wider, often weaker line Deep; AC only; low magnetization
Subsurface inclusion (slag, oxide stringer) Local permeability drop and a volume that flux avoids Broad, low-contrast smudge if it is close enough Rounded, deep, or aligned with the field
Rounded porosity Sphere or pore lets flux flow around in three dimensions; little preferred leak path Faint rounded cluster, or nothing Small, isolated, subsurface
Linear aligned porosity or a chain of pores Several weak leaks add along a line Broken or beaded line that can mimic a crack Interpreted as one crack without checking morphology
A surface-breaking crack is the condition MT was built for. Tight fatigue and grinding cracks are planar, high length-to-width slots. They interrupt a large fraction of the near-surface flux and print a crisp line.
A rounded pore of similar opening width is a much weaker magnet. Flux slips around a sphere in three dimensions instead of being forced out through a long slot. That is why MT is a poor porosity survey compared with radiographic testing (RT) , and why a single faint rounded particle cluster is not automatically 'a crack we almost missed.'
A subsurface inclusion sits under a ligament of sound metal. Some flux never leaves the steel. The leakage that does reach the surface is spread out, so the particle pile is wider and less intense than a surface crack of the same length. If the inclusion is deep enough, there is no surface indication at all.
Permeability change versus a void
A crack is a void : permeability drops from that of steel to that of air. A permeability change without a void — cold work, a hard heat-affected zone (HAZ) , a brazed interface, magnetic writing from a previous residual field, or a local alloy difference — also bends flux lines. Particles can collect there even though there is no opening.
Interpretation rule:
A void (crack, seam, lap, open inclusion) is a candidate relevant indication . Evaluate it against the acceptance standard.
A permeability variation is often a nonrelevant indication . Confirm by residual-field mapping, demagnetizing and retesting, etching, hardness check, or another method.
Mechanical hold-up of particles on roughness, lint, or drain lines is a false indication — there was no leakage field.
Do not call every particle pile a defect . Defect is an accept/reject decision after evaluation against the specified standard. The general exam punishes that word when the stem has only given you a buildup.
Depth sensitivity: AC versus HWDC and DC
How deep a discontinuity can still leak to the surface depends on how the field is produced.
Alternating current (AC) is confined to a thin skin by eddy currents ( skin effect ). It is outstanding for surface-breaking fatigue and grinding cracks and is the usual yoke current for in-service weld toes. It is the wrong current if the procedure is hunting a subsurface shrinkage crack in a casting.
Half-wave direct current (HWDC) (single-phase rectified) penetrates deeper than AC. The pulses also agitate dry particles so they remain mobile instead of sitting wherever they first land. HWDC plus dry powder is a classic casting and weld technique when some near-surface depth is required.
Direct current (DC) and full-wave direct current (FWDC) penetrate deepest. Particle mobility is poorer unless the bath is flowing or the part is gently moved, because there is no AC vibration. Residual techniques after a DC shot are common on high-retentivity parts.
There is no single published 'AC sees 0.040 in, DC sees 0.250 in' number that ASNT posts as an exam constant. Depth is procedure-, material-, and magnetization-dependent. Teach the order : AC = surface; HWDC = deeper with particle mobility; DC/FWDC = deepest field, watch particle mobility. If a stem gives a procedure depth claim, use the procedure.
A surface fatigue crack on a girder toe is an AC-yoke problem. A subsurface hot tear a few millimetres under the surface of a ferromagnetic steel casting is an HWDC or DC problem. Using the wrong current type is not a 'light indication of the same crack'; it can be a complete miss.
Geometry, cold work, scratches, and other look-alikes
Real parts generate leakage that is not a crack.
Geometry. Threads, keyways, spline roots, sudden section changes, hole edges, and weld toes are flux concentrators. Particles collect along the geometric contour. That is usually nonrelevant after you recognize the feature. A crack in a thread root sits off the geometric helix or is sharper than the thread; do not dismiss every root line as 'just the thread.'
Cold work. Localized plastic deformation changes permeability. A press-fit, a stamped identification number, a peened repair, or a badly dressed grind can print a fuzzy indication that follows the worked zone rather than a single crack path.
Permeability changes from heat. A hard HAZ or a local hard spot in a plate can attract particles in a broad band. Demagnetize and retest, or confirm with hardness or another NDT method, before you write a crack.
Scratches and tool marks. A shallow scratch may simply trap dry powder ( false ). A deeper gouge can leak like a weak crack (relevant, or at least requiring evaluation). Wipe, re-apply with lighter particle density, and look at sharpness and whether the mark is visible under white light as a geometric groove.
Magnetic writing. Residual fields from a previous magnetizing shot, from contact with another magnetized part, or from a magnetic chuck can write streaks. Demagnetize and remagnetize in the required directions. Writing that disappears after a controlled demagnetization was never a void.
Over-magnetization and rough surface. Heavy background hides both relevant and nonrelevant patterns. Reduce field or particle application; do not 'interpret through' a purple fog of fluorescent bath.
Banding and segregation in some bar stock can produce faint, diffuse longitudinal indications from permeability layering rather than from a single seam. Compare with a known seam (sharp, tight, often one-sided) and with the product-form chapter's wrought-steel story.
Relevant, nonrelevant, and false — used on purpose
Keep the three words that the fundamentals chapter introduced, now applied to MT only:
Relevant indication: leakage from a discontinuity that must be evaluated (crack, seam, lap, open inclusion).
Nonrelevant indication: real leakage or particle collection from a condition the procedure does not treat as rejectable — geometry, permitted section change, magnetic writing, many permeability variations.
False indication: particles present for a non-magnetic reason — lint, dirt, drain lines, inadequate removal of excess bath, mechanical lodging in a scratch.
A Level II who writes 'defect' on a keyway corner fails the exam item even if the particles were spectacular.
Realistic exam scenarios
A carbon-steel pin shows a sharp longitudinal indication after a circular head shot and nothing after the coil shot. That is the expected orientation behavior of a longitudinal seam, not a random 'intermittent' crack. Evaluate it as relevant against the acceptance standard.
An AC yoke on a girder toe finds a tight toe-line indication. The same area examined with a DC prod setup looking for subsurface shrinkage in an adjacent casting pad is a different technique for a different depth. Do not treat 'we already MT'd it' as covering both.
Dry powder hangs in a coarse grind scratch after an AC yoke pass. White-light visual shows the groove. After a light reclean and a thinner powder cloud, the linear pile is gone. Classify the first pile as false hold-up, not as a healed crack.
A press-fit collar leaves a fuzzy circumferential band after a coil shot. Demagnetization and a second coil shot still show a broad band exactly at the interference fit. Another method (or disassembly) is needed before anyone calls it a crack. Treat it as a permeability/geometry nonrelevant until proven otherwise.
Rounded fluorescent specks appear in a weld cap after an AC yoke shot. They do not line up, they wipe partly with the bath, and radiography of the same weld later shows scattered porosity. Those specks were weak surface pores or hold-up — not a substitute for an RT porosity map, and not automatically rejectable cracks.
What this topic is testing
Ask four questions on every indication stem: Did the discontinuity cut the flux? Was it open to the surface or buried? Was the current type capable of that depth? Are you looking at a void, a permeability change, geometry, or dirt? The correct classification — relevant, nonrelevant, or false — falls out of those answers.