Study guide

10.4 Functionality, Force & Elastomer Hardness Testing

ASQ Certified Quality Inspector CQI

Track your progress as you read

Finished sections get a check mark.

1 Chapter 1: Shop Mathematics & Algebra

1.1 Basic Shop Math & Precision Measurement 1.2 Basic Algebra & Technical Formulas 1.3 Measurement Systems & Unit Conversions

2 Chapter 2: Geometry & Applied Shop Trigonometry

2.1 Applied Shop Geometry 2.2 Right-Triangle Trigonometry 2.3 Shop Trigonometry Applications & Sine Bars

3 Chapter 3: Handheld Variable & Attribute Gages

3.1 Variable Hand Measuring Instruments 3.2 Fixed Attribute & Limit Gages 3.3 Transfer Gages & Precision Accessories 3.4 Special Gages: Electronic, Pneumatic, Force & Environmental Instrumentation

4 Chapter 4: Surface Plate Inspection, Optical Systems & CMMs

4.1 Gage Selection, Care & Environmental Control 4.2 Surface Plate Tools & Layout Inspection 4.3 Optical Comparators & Vision Systems 4.4 Coordinate Measuring Machines (CMM) & 3-2-1 Alignment 4.5 Gage Correlation & Cross-Instrument Agreement

5 Chapter 5: Surface Metrology, Calibration Systems & MSA

5.1 Surface Texture & Finish Measurement 5.2 Calibration Systems & NIST Traceability 5.3 Measurement System Analysis (MSA) & Gage R&R 5.4 Measuring Mass, Form & Profile, and Inclination

6 Chapter 6: Technical Drawing & Blueprint Reading

6.1 Engineering Drawing Structure & Conventions 6.2 Views, Sectioning & Feature Representation 6.3 Dimensions, Tolerancing & Fit Classifications

7 Chapter 7: Geometric Dimensioning & Tolerancing (GD&T)

7.1 GD&T Fundamentals & Datum Reference Frames 7.2 Material Condition Modifiers & Bonus Tolerance 7.3 Form & Orientation Tolerances 7.4 Location, Profile & Runout Tolerances

8 Chapter 8: Sampling Inspection & Acceptance Sampling Plans

8.1 Sampling Fundamentals & Operating Characteristic (OC) Curves 8.2 Attribute Sampling with ANSI/ASQ Z1.4 8.3 Variables Sampling with ANSI/ASQ Z1.9

9 Chapter 9: Inspection Planning, Processes & Material Disposition

9.1 Inspection Planning, Receiving & In-Process Inspection 9.2 First Article Inspection (FAI) & Documentation 9.3 Nonconforming Material Control & MRB 9.4 Inspection Errors & Human Factors 9.5 Product Traceability, Age Control & Shelf Life

10 Chapter 10: Materials Testing & Nondestructive Examination

10.1 Mechanical & Destructive Testing 10.2 Surface & Subsurface NDE Methods 10.3 Volumetric & Electromagnetic NDE Methods 10.4 Functionality, Force & Elastomer Hardness Testing 10.5 Software for Test Equipment & Software Validation

11 Chapter 11: Statistical Process Control & Process Capability

11.1 Statistics Fundamentals & Normal Distribution 11.2 Control Charts for Variables 11.3 Control Charts for Attributes & Run Rules 11.4 Process Capability & Performance Analysis

12 Chapter 12: Quality Systems, Continuous Improvement & Safety

12.1 The 7 Classic Quality Control Tools 12.2 Continuous Improvement & Problem-Solving Methodologies 12.3 Quality Management Systems, Audits & CAPA 12.4 Workplace Safety, Environmental Controls & PPE 12.5 Failure Mode and Effects Analysis (FMEA) & Fault Tree Analysis (FTA)

13 Chapter 13: Quality Fundamentals, Teams & Documentation Systems

13.1 Quality Improvement Concepts, Products & Processes 13.2 Audit Tools, Tracing Techniques & Audit Communication 13.3 Employees as Resources: Empowerment, Team Roles & Team Development 13.4 Quality Documentation, Reference Standards & Document Control

10.4 Functionality, Force & Elastomer Hardness Testing

Key Takeaways Explain This Topic AI

Functionality testing verifies that a part performs its intended function; a part can pass every dimensional check on the drawing and still fail a functional test.

A proof load is applied below the level that damages the part and is therefore non-destructive, while a pull-to-failure test destroys the specimen and yields the actual breaking strength.

Leak test methods differ by orders of magnitude in sensitivity: bubble immersion detects roughly 1e-4 std cc/s, pressure decay is comparable, and helium mass spectrometry reaches about 1e-9 std cc/s.

Durometer hardness per ASTM D2240 uses Shore A for soft elastomers and Shore D for hard rubber and plastics, with the reading taken 1 second after firm contact unless a 15-second delayed reading is specified.

ASTM D2240 requires a specimen at least 6 mm thick with readings taken at least 12 mm from any edge; plying thin sheets to reach thickness is permitted.

Last updated: September 2026

Functionality Testing: A Different Question

Every method covered so far asks whether a part matches its drawing. Functionality testing asks a different question: does the part do its job? A hose fitting can hold every dimension on the print and still leak. A crimped terminal can look perfect and pull off at half its required retention force. A spring can be the right free length and the wrong rate.

Because functional requirements are often the reason the dimensional requirements exist, functional tests frequently appear on inspection plans as the final gate before shipment, and they are the tests that a customer's incoming inspection is most likely to repeat.

Tension and Pull Testing

Tension testing applies a pulling force along an axis. Section 10.1 covers the destructive tensile test to failure under ASTM E8. In functional inspection the more common variants are:

Pull-off / retention testing. A crimped terminal, a bonded joint, a swaged fitting, or a molded insert is pulled to verify it holds a specified minimum force. Wire-crimp pull testing is a standard electrical-assembly inspection under specifications such as IPC/WHMA-A-620.

Proof load testing. A force below the level that would damage the item is applied and held; the item is then inspected for permanent set or damage. Because the part survives and remains usable, proof testing is non-destructive . Lifting hardware, chain, slings, and threaded fasteners are commonly proof-loaded.

Pull-to-failure testing. The specimen is pulled until it breaks, giving the actual breaking force and the failure mode. This is destructive and is applied to samples, never to product being shipped.

Peel and adhesion testing. Tape, label, coating, or laminate adhesion measured as force per unit width at a specified peel angle.

The exam discriminator is proof versus destructive : a proof load verifies capability without consuming the part; a pull-to-failure test consumes it.

Failure mode matters as much as the number. A crimp that pulls apart at the barrel indicates a bad crimp; a wire that breaks outside the crimp at a higher force indicates the crimp is stronger than the wire, which is the desired outcome.

Torque Testing

Torque is rotational force about an axis, and torque tests come in several distinct forms that candidates routinely confuse.

  • Test What it measures When applied
  • Installation torque Torque applied while tightening to the specified value During assembly
  • Breakaway (removal) torque Torque required to start loosening a fastener Audit after assembly

Prevailing torque Torque required to keep running a locking fastener while it is still free-spinning Verifies a locking feature such as a nylon patch or distorted thread

Residual torque Torque at which a fastener resumes movement in the tightening direction Non-destructive audit of a joint already assembled

Torque to failure / strip torque Torque at which threads strip or the fastener breaks Destructive qualification

The residual torque audit is the workhorse of the inspection department because it does not disturb the joint: the auditor applies torque in the tightening direction and records the value at which the fastener first moves. Breakaway torque, applied in the loosening direction, destroys the original clamp load and requires re-torque.

Torque wrenches are calibrated under ISO 6789 , typically at points spanning the range such as roughly 20%, 60%, and 100% of full scale. Section 3.4 covers the instrument families.

The concept every inspector must carry: torque is a proxy for clamp load, not a measurement of it . Most of the applied torque is consumed by friction under the head and in the threads, and lubrication, plating, surface finish, and reuse all change that friction. This is why critical joints specify torque-plus-angle or direct bolt-tension measurement rather than torque alone.

Leak Testing

Leak testing verifies that a sealed or pressurized item contains its contents. The selection question on the exam is almost always about sensitivity : which method can detect the specified leak rate?

Leak rates are expressed in standard cubic centimeters per second (std cc/s) or in pressure-volume units such as mbar-L/s.

Method How it works Approximate sensitivity (std cc/s) Notes

Bubble / immersion (dunk) Pressurize the part, submerge it, watch for bubbles 1e-3 to 1e-4 Cheap, visual, locates the leak; operator-dependent

Pressure decay Pressurize, isolate, measure pressure loss over a timed dwell 1e-3 to 1e-4 Quantitative, automatable; sensitive to temperature drift

  • Vacuum decay Evacuate, isolate, measure pressure rise 1e-3 to 1e-5 Good for sealed packages and containers
  • Mass flow Measure the makeup flow needed to hold pressure 1e-2 to 1e-4 Fast; good for larger allowable leaks

Halogen diode sniffer Detect a halogenated tracer gas at the surface about 1e-6 Locates leaks; being displaced by helium methods

Helium mass spectrometry Detect helium tracer with a mass spectrometer 1e-8 to 1e-10 The most sensitive practical method; hard-vacuum or sniffer mode

Two operational points generate exam questions. First, every leak test requires a stabilization or dwell time : pressurizing a part warms the gas inside it, and the pressure decay from that cooling is indistinguishable from a leak until the temperature settles. Second, a negative result is bounded by the method's sensitivity — "no bubbles observed" means the leak is smaller than roughly 1e-4 std cc/s, not that the part is hermetic. Leak test procedures therefore specify a calibrated reference leak used to verify the system can actually detect the rate it claims to detect.

Compression Testing

Compression testing applies a squeezing force and measures the resulting deformation or the force required to reach a defined deflection.

Spring rate and load at height. A compression spring is compressed to a specified working height and the force is recorded, verifying the spring rate rather than just the free length.

Crush and buckling strength. Tubes, bushings, honeycomb cores, and containers are compressed to a defined load or to collapse.

Compression set of elastomers. A seal is compressed a defined amount for a defined time at a defined temperature, then released; the percentage of thickness it fails to recover is its compression set. High compression set predicts seal leakage in service.

Package compression. Loaded shipping containers are compressed to simulate stacking loads, commonly under ASTM D642 and the ISTA transit-test series.

Indentation force deflection for foam cushioning.

Drop Testing

Drop testing evaluates whether a product or its packaging survives handling shocks.

Packaged-product drop testing under ASTM D5276 releases a loaded shipping container in free fall onto a rigid surface. Drop height is selected from the package's gross weight — heavier packages are dropped from lower heights — and a standard sequence covers one corner, the three edges radiating from that corner, and all six faces . The pass criterion covers both package integrity and, more importantly, the condition of the product inside.

Product drop and mechanical shock testing under standards such as IEC 60068-2-31 evaluates the device itself rather than its packaging.

Related transit simulation includes vibration, incline impact, and compression, usually combined into an ISTA or ASTM series.

Drop testing is destructive in intent even when the specimen survives: a dropped unit is generally not returned to saleable stock.

Durometer Hardness Testing of Elastomers and Plastics

Section 10.1 covered Rockwell, Brinell, Vickers, and microhardness for metals. Body of Knowledge topic III.D.4 also names the durometer , which is the standard method for rubber, elastomers, and plastics.

Principle

A durometer presses a spring-loaded indenter of specified geometry into the material and measures how far the indenter fails to penetrate. The scale runs 0 to 100 , where 100 means no penetration (maximum hardness) and 0 means full penetration. Because the indenting force comes from a calibrated spring rather than a dead weight, the durometer is a portable, hand-held or stand-mounted instrument.

Scales (ASTM D2240)

ASTM D2240 defines twelve types; three dominate inspection work:

  • Type Indenter Typical materials
  • Shore A 35-degree truncated cone Soft to medium elastomers — O-rings, gaskets, tubing, soft seals
  • Shore D 30-degree cone with a 0.1 mm radius tip Hard rubber, thermoplastics, rigid polymers
  • Shore OO 2.5 mm spherical Foams, sponges, gels, very soft cellular materials

Type M is a micro-hardness durometer designed for small cross-sections such as O-rings, requiring far thinner specimens than the standard types.

Test Rules That Appear on Exams

Specimen thickness must be at least 6 mm (0.25 in). Thinner material lets the indenter sense the anvil beneath, giving falsely high readings — exactly the anvil effect seen in Rockwell testing. Plying (stacking) thinner sheets to reach 6 mm is permitted.

Readings must be taken at least 12 mm (0.5 in) from any edge , and separated from each other, because edges deform differently than the bulk material.

Timing is part of the method. The reading is taken within 1 second of firm contact of the presser foot, unless the specification calls for a delayed reading at 15 seconds . Elastomers creep under the indenter, so a 15-second reading is always lower than a 1-second reading on the same material. A durometer result is meaningless without stating which timing was used.

Curved surfaces read low or erratically. O-rings and tubing require a Type M durometer or a specified fixture.

The scales overlap. When a Shore A reading exceeds 90 , the material is too hard for reliable Type A measurement and Type D should be used ; when a Shore D reading falls below 20 , Type A is preferred . Reporting "Shore A 96" is a method error.

Temperature matters. Elastomer hardness changes with temperature, so tests are run at a controlled standard laboratory temperature.

IRHD (International Rubber Hardness Degrees), defined in ISO 48, is the alternative method used widely outside North America. IRHD and Shore A numbers are similar in magnitude but are produced by different geometry and are not interchangeable by conversion.

Method Selection Summary

Test Measures Representative standard Destructive?

  • Proof load Survival at a defined load Product or contract spec No
  • Pull to failure Breaking force and failure mode ASTM E8, IPC/WHMA-A-620 Yes
  • Residual torque Torque at which a joint resumes motion Product or contract spec No
  • Breakaway torque Torque to start loosening Product or contract spec Disturbs the joint
  • Bubble leak Leak presence and location Product or contract spec No
  • Helium leak Very small leak rates Product or contract spec No
  • Compression set Permanent deformation of an elastomer ASTM D395 Yes
  • Package drop Package and contents survival ASTM D5276, ISTA series Effectively yes
  • Durometer Indentation hardness of polymers ASTM D2240 No
  • Common Exam Traps

Proof load is non-destructive. Only tests carried to failure are destructive.

Residual versus breakaway torque. Residual is applied in the tightening direction and preserves the joint; breakaway is applied in the loosening direction and destroys the original clamp load.

Torque is not clamp load. Friction consumes most of the applied torque.

A leak test result is bounded by method sensitivity. "No bubbles" is not "hermetic."

Durometer timing must be stated. A 15-second reading is lower than a 1-second reading on the same specimen.

Durometer thickness and edge distance. At least 6 mm thick and at least 12 mm from any edge; stacking to reach thickness is allowed.

Shore A above 90 means switch to Shore D. Reporting a Shore A value in the 90s indicates the wrong scale was used.

Durometer applies to polymers, not metals. If the stem describes hardened steel, the answer is Rockwell, Brinell, Vickers, or microhardness.