Study guide

2.1 Welding Procedure Specification (WPS) Requirements & Contents

AWS API 1104 Pipeline Welding Endorsement Exam

Track your progress as you read

Finished sections get a check mark.

1 Chapter 1: Overview & Scope of API 1104:2021

1.1 Scope, Definitions & General Requirements 1.2 Base Materials & Filler Metal Groupings

2 Chapter 2: Welding Procedure Qualification (Section 5)

2.1 Welding Procedure Specification (WPS) Requirements & Contents 2.2 Essential Variables for Procedure Qualification (Section 5.4) 2.3 Mechanical Testing Requirements and Specimen Preparation 2.4 Acceptance Criteria for Procedure Qualification

3 Chapter 3: Welder Qualification (Section 6)

3.1 Single Qualification Testing & Essential Variables 3.2 Multiple Qualification Testing & Layout 3.3 Visual & Destructive Test Specimen Layout 3.4 Acceptance Criteria & Retesting Rules for Welders

4 Chapter 4: Design & Fabrication of Pipeline Welds (Section 7)

4.1 Joint Alignment, High-Low & Fit-Up Tolerances 4.2 Preheating, Interpass Temperature & Heat Treatment 4.3 Tack Welding, Line-Up Clamps & Weather Restrictions 4.4 Filler Metal Storage, Handling & Conditioning

5 Chapter 5: Inspection & Non-Destructive Testing (Sections 8 & 11)

5.1 Rights & Responsibilities of Inspection Personnel 5.2 Radiographic Testing (RT) & Image Quality Indicators (IQI) 5.3 Ultrasonic Testing (UT) & Automated UT (AUT/PAUT) 5.4 Magnetic Particle (MT), Liquid Penetrant (PT) & Personnel Qualification

6 Chapter 6: Acceptance Standards for Imperfections (Section 9)

6.1 Inadequate Penetration (IP), IP Due to High-Low (IPD) & Cross Penetration (ICP) 6.2 Incomplete Fusion (IF & IFD), Internal Concavity (IC) & Burn-Through (BT) 6.3 Slag Inclusions (ESI & ISI) & Hollow Bead (HB) Porosity 6.4 Porosity — Scattered (P), Distribution Charts & Hollow Bead Cross-Reference 6.5 Undercutting, Crater Cracks & Arc Burns 6.6 Cracks, Accumulation of Imperfections & Annex A (ECA)

7 Chapter 7: Repair, Mechanized Welding & Records (Sections 10 & 12)

7.1 Repair Procedure Qualification & Limitations 7.2 Defect Removal, Grinding & Re-Inspection 7.3 Welding Records, Traceability & Inspector Logs 7.4 Mechanized Welding with Filler Metal Additions (Section 12)

8 Chapter 8: Annex B — In-Service Pipeline Welding

8.1 In-Service Welding Dynamics, Burn-Through & HIC Risks 8.2 Temper-Bead Deposition Techniques & Sequence 8.3 In-Service Procedure & Welder Qualification Requirements

2.1 Welding Procedure Specification (WPS) Requirements & Contents

Key Takeaways Explain This Topic AI

API 1104 Section 5.1 mandates that a detailed written WPS be established and qualified before any production welding begins; acceptance of the qualification weld is by destructive testing per 5.6 or 5.8.

Section 5.3.2 lists nineteen specification items: process, materials (SMYS range), diameters/wall thicknesses, joint design, filler metal and bead sequence, electrical characteristics, flame characteristics, position, direction, time between passes, lineup clamp, cleaning, preheat/interpass, shielding gas, shielding flux, travel speed, cooling method, postheat, and PWHT.

Section 5.3.2.10 requires the WPS to specify the maximum time between completion of the root bead and start of the second bead (and second to third bead) when EXX10 or EXX11 cellulosic electrodes are used.

Section 5.3.2.11 requires the WPS to state whether the lineup clamp is internal or external and the minimum percentage of the root bead that must be completed before clamp release — the percentage itself is a WPS variable, not a fixed code number.

The procedure qualification record (5.2) documents the actual observed values of all 5.3 variables plus complete test results, and must be maintained as long as the procedure is in use.

Last updated: August 2026

2.1 Welding Procedure Specification (WPS) Requirements & Contents

In pipeline construction governed by API Standard 1104 (22nd Edition) , Section 5.1 requires that before any production welding starts, a detailed Welding Procedure Specification (WPS) be established and qualified to demonstrate that sound welds with suitable mechanical properties (strength, ductility, hardness) can be made by the procedure. Acceptance of the procedure qualification weld is determined by destructive testing per 5.6 (butt welds) or 5.8 (branch and fillet welds). Section 5 applies to manual and semiautomatic welding with filler metal; mechanized welding procedures are qualified under Section 12.

The procedure qualification record (5.2) is the evidence file: it must document the actual observed values for every variable specified per 5.3 plus the complete qualification test results, and it must be maintained for as long as the procedure is in use. Multiple qualification welds may be combined to qualify a range of essential variables within one WPS.

The Nineteen WPS Contents Items (Section 5.3.2.1-5.3.2.19)

An API 1104 WPS must address every applicable item of 5.3.2. Omission of a required field makes the document non-compliant.

Item Subsection What the WPS Must Specify

Process 5.3.2.1 Specific process or combination (SMAW, GMAW, FCAW, GTAW, SAW, PAW, OFW) and method of application (manual or semiautomatic)

  • Materials 5.3.2.2 SMYS range of the materials to which the procedure applies
  • Diameters & wall thicknesses 5.3.2.3 Ranges of specified outside diameters and wall thicknesses

Joint design & weld shape 5.3.2.4 Sketch with tolerances for bevel angle, root face, root opening; cap height/width tolerances; fillet shape/size; backing type if used

Filler metal, flux & beads 5.3.2.5 Sizes and classification of filler metal and flux; minimum number and sequence of beads (designated per company-defined thickness subsets where they differ)

Electrical characteristics 5.3.2.6 Current and polarity; voltage and amperage ranges for each electrode type/size; heat input and its calculation method when Table 1 requires it

Flame characteristics 5.3.2.7 For oxy-fuel: neutral, carburizing, or oxidizing flame; torch tip orifice size per rod/wire size

  • Position 5.3.2.8 Roll or fixed position welding
  • Direction of welding 5.3.2.9 Vertical up, vertical down, or horizontal

Time between passes 5.3.2.10 With EXX10/EXX11 electrodes: maximum time from root bead completion to start of second bead, and from second to third bead (minutes or hours)

Lineup clamp 5.3.2.11 Internal or external clamp (or none); if a clamp is used, the minimum percentage of the root bead to be completed before release

  • Cleaning/grinding 5.3.2.12 Power tools, hand tools, or both
  • Preheat & interpass 5.3.2.13 Heating method, minimum preheat, and maximum interpass temperature
  • Shielding gas & flow 5.3.2.14 Gas classification and flow-rate range
  • Shielding flux 5.3.2.15 Type of shielding flux, when applicable
  • Speed of travel 5.3.2.16 Travel-speed range for each pass or pass grouping
  • Cooling after welding 5.3.2.17 Type of deliberate cooling (if any) and maximum weld temperature before cooling
  • Postheat 5.3.2.18 Minimum temperature and time for hydrogen-diffusion postheating, when used

PWHT 5.3.2.19 Full PWHT procedure: application method, heating rate, temperature range, time at temperature, cooling rate

The Two Administrative Rules Candidates Confuse

Time between passes (5.3.2.10). The requirement to put maximum root-to-second-bead and second-to-third-bead times in the WPS applies specifically to EXX10 and EXX11 (cellulosic) electrodes . Cellulosic root beads carry high diffusible hydrogen and see heavy restraint; a fast hot pass tempers the root and drives hydrogen out. The WPS states the limits in minutes or hours — the standard deliberately does not print a universal number.

Lineup clamp removal (5.3.2.11 + 7.3). The WPS states whether the clamp is internal or external and the minimum root-bead percentage that must be complete before release. Section 7.3 adds that when a clamp is removed before root-bead completion, the completed part of the bead shall be in approximately equal segments spaced approximately equally around the circumference . Again, no fixed percentage (such as "50%") appears in the standard — it is a qualified WPS value.

Qualifying the WPS

To qualify the WPS, a test joint of two pipe nipples is welded following every detail of the draft procedure (5.5). The recorded variables go into the qualification record; the coupon then goes to visual examination and the destructive tests of 5.6 (tensile, nick-break, root/face/side bends as required by Table 3). Only when every specimen meets the acceptance requirements of 5.6 — or the branch/fillet requirements of 5.8 — is the procedure qualified for production.