Study guide
11.7 Masonry Reinforcement, Grouting & Wall Systems
Arizona General Contractor Exam
Track your progress as you read
Finished sections get a check mark.
1 Chapter 1: Introduction & Exam Overview
1.1 Current Exam Facts 1.2 The Arizona Contractor Licensing Path 1.3 How to Use This Guide & Study Plan
2 Chapter 2: Arizona ROC & Licensing Law
2.1 The Arizona Registrar of Contractors 2.2 License Classifications 2.3 Qualifying Party & Experience Requirements 2.4 Application, Fees, Bond & Background Check 2.5 License Bonds, Cash Deposits & Bond Claims 2.6 Unlicensed Contracting: Penalties & Lost Remedies 2.7 Advertising Rules, Contract Disclosures & Workmanship Standards
3 Chapter 3: The Exams — SRE, Trade & NASCLA
3.1 The Statutes & Rules Exam (SRE) 3.2 The PSI Trade Exam 3.3 The NASCLA Commercial General Building Exam Option
4 Chapter 4: License Maintenance, Recovery Fund & Discipline
4.1 License Renewal & Continuing Education 4.2 The Residential Contractors' Recovery Fund 4.3 ROC Disciplinary Actions & Penalties
5 Chapter 5: Contract Law & Disputes
5.1 Arizona Contract Fundamentals 5.2 Construction Contract Terms & Provisions 5.3 Change Orders & Modifications 5.4 Dispute Resolution & ROC Complaints 5.5 The Arizona Prompt Payment Act
6 Chapter 6: Liens, Bonds & Insurance
6.1 Arizona Mechanics' Lien Law Overview 6.2 Lien Notices, Recording & Deadlines 6.3 Contract Bonds: Bid, Performance & Payment 6.4 Insurance Requirements
7 Chapter 7: Financial Management & Taxes
7.1 Accounting & Financial Statements 7.2 Estimating, Bidding & Markup 7.3 Taxes & Payroll
8 Chapter 8: Project Management
8.1 Scheduling & the Critical Path Method 8.2 Supervision, Subcontractors & Quality Control 8.3 Project Documentation & Closeout
9 Chapter 9: Safety & OSHA
9.1 OSHA Construction Standards Overview 9.2 Fall Protection, Scaffolds & Ladders 9.3 Excavation, Trenching & Electrical Safety 9.4 Heat Illness Prevention & Arizona Job-Site Hazards
10 Chapter 10: Building Codes, Permits & Plan Reading
10.1 IRC 2018 & IBC 2018 Fundamentals 10.2 Permits, Plan Review & Inspections 10.3 Energy Code & Accessibility 10.4 Reading Construction Drawings & Specifications 10.5 Means of Egress & Fire-Resistance-Rated Construction
11 Chapter 11: Sitework, Concrete & Masonry
11.1 Sitework: Surveying, Excavation & Grading 11.2 Concrete: Formwork, Reinforcement & Placing 11.3 Masonry: Brick, Block & Mortar 11.4 Soils, Compaction & Earthwork Testing 11.5 Concrete Materials & Mix Design 11.6 Concrete Curing, Joints, Testing & Defects 11.7 Masonry Reinforcement, Grouting & Wall Systems
12 Chapter 12: Carpentry, Metals & Building Envelope
12.1 Carpentry & Framing 12.2 Metals & Metal Framing 12.3 Thermal & Moisture Protection 12.4 Doors, Windows & Finishes 12.5 Engineered Wood, Trusses & Connectors 12.6 Structural Steel Erection & Connections 12.7 Steel Joists, Girders & Metal Deck
13 Chapter 13: Roofing, Waterproofing & Interior Finishes
13.1 Roofing Systems 13.2 Waterproofing, Flashing & Sealants 13.3 Interior Finishes: Gypsum, Stucco, Flooring & Paint
14 Chapter 14: Building Systems for the General Contractor
14.1 Mechanical & Plumbing Systems 14.2 Electrical Systems & Temporary Power
11.7 Masonry Reinforcement, Grouting & Wall Systems
Key Takeaways Explain This Topic AI
Grout is a fluid mixture placed to bond reinforcement to masonry units; it is proportioned for high slump (8 to 11 inches) and is not the same material as mortar
Fine grout is used in narrow cells and thin joints; coarse grout containing pea gravel is used where the space is large enough to accept it
High-lift grouting above about 5 feet requires cleanout openings at the base of each grouted cell so debris can be removed and steel inspected
Bond beams are horizontal grouted courses containing continuous reinforcement, used at floor and roof lines, above openings, and at wall tops
Hot-weather masonry practice — wetting units where required, shading materials, and protecting fresh work — governs most Arizona placements
Last updated: August 2026
Reinforced Masonry Is a Different Trade From Mortar Work
Quick Answer: In reinforced concrete masonry, the block and mortar form a set of vertical cells and horizontal bond beams that are filled with grout around reinforcing steel . Grout is not mortar: it is proportioned to be fluid — commonly an 8 to 11 inch slump — so it flows around bars and fills every void.
Section 11.3 covered units, mortar types, and laying practice. This section covers what turns a stacked wall into a structural element. On the commercial trade exam, masonry questions run heavily toward reinforcement placement, grouting procedure, and inspection — the things a general building contractor supervises rather than performs.
Mortar Versus Grout
- Mortar Grout
- Purpose Bonds units together; fills the joints Bonds reinforcement to the masonry; fills cells and bond beams
- Consistency Stiff, workable, retains its shape on a trowel Fluid, self-consolidating in placement
- Slump ~ 2½ inches (measured by cone penetration in practice) 8 to 11 inches
- Aggregate Sand only Sand (fine grout) or sand plus pea gravel (coarse grout)
- Placed by Mason with a trowel Pump, bucket, or chute into cells
Grout is intentionally wet. The high water content that would ruin concrete is correct here, because the dry masonry units absorb excess water from the grout almost immediately, dropping the effective water-cement ratio after placement. A stiff grout that will not flow leaves voids around the steel, which is the failure the inspection process exists to catch.
- Grout type Use
- Fine grout Narrow cells, small clearances, thin collar joints
- Coarse grout Larger cells with adequate clear dimension to pass pea gravel
Choose by the smallest clear dimension the grout must pass through, including around reinforcing bars.
Reinforcement Placement
Vertical steel sits in cells and is held in position by positioners or by tying to dowels projecting from the foundation. Two requirements decide whether it works:
Position. Bars must be centered in the cell (or at the specified location) and remain there during grouting. A bar leaning against the block face has no grout cover and is not doing what the engineer designed.
Lap splices. Bars are lapped the specified length, which is stated on the structural drawings and depends on bar size, grout strength, and cover. Field crews should never eyeball a lap.
Horizontal steel comes in two forms:
Form Where
Joint reinforcement (ladder or truss wire) Bedded in the mortar joint at specified vertical intervals — commonly every 16 inches
Bond beam reinforcement Continuous bars in a grouted bond-beam course
Bond beams are horizontal courses formed with bond-beam or lintel block, reinforced and grouted continuously. They appear at floor and roof bearing lines, at the top of walls, above openings, and at intervals set by the structural drawings. They tie the wall together, distribute concentrated loads, and are essential to the wall's out-of-plane and seismic performance. Where a bond beam sits over a cell that is not to be grouted, the bottom is closed off — with metal lath or a plate — so grout stays in the beam rather than running down the wall.
Low-Lift and High-Lift Grouting
The wall cannot be grouted to full height in one pour without either blowing the wall apart or leaving voids. Two procedures exist:
Low-lift grouting High-lift grouting
Procedure Lay a limited height of wall, then grout, then continue Lay the wall to full story height, then grout in lifts
Typical lift Roughly 4 to 5 feet at a time Grout placed in lifts within a taller pour, consolidated between lifts
- Cleanouts Generally not required Required at the base of every grouted cell
- Advantage Simple; no cleanout patching Faster; fewer interruptions to the masons
Cleanout openings are the detail the exam tests. When the grout pour height exceeds roughly 5 feet , an opening at least about 3 inches across is left at the bottom of each cell to be grouted. Their purpose is twofold: mortar droppings and debris are removed through them, and the inspector verifies reinforcement position and lap length before the cells are closed and grouted. They are then sealed to resist the grout pressure.
Consolidation. Grout must be consolidated — mechanically vibrated — and then reconsolidated after initial water loss so that the settlement shrinkage does not leave a void at the top of the lift. Skipping reconsolidation is a common source of hollow bond beams.
Hot-Weather Masonry — the Arizona Default
Most Arizona masonry is placed in hot-weather conditions, and the governing concern is that mortar and grout lose water to evaporation and to the units faster than hydration can use it.
- Condition Practice
- Rising ambient temperature Shade sand and mixing water; use cool mixing water
High temperature and wind Reduce the time mortar sits before use; retemper only within the allowed window; work in shorter runs
Units hot to the touch Shade unit stockpiles; do not wet concrete masonry units, which are laid dry — this is opposite to clay brick with high absorption, which may require wetting
Fresh work exposed Fog and cover completed work; protect from direct sun and wind
That third row is a classic exam discriminator. Clay brick with a high initial rate of absorption may need to be wetted before laying so it does not pull water out of the mortar. Concrete masonry units are laid dry — wetting CMU adds water the unit will later give up as shrinkage, producing cracking.
Warning: in monsoon season the opposite risk appears. Freshly laid masonry must be covered at the end of each day, because a downpour on green work washes out joints and leaches efflorescence-forming salts to the surface.