Study guide

11.3 Masonry: Brick, Block & Mortar

Arizona General Contractor Exam

Track your progress as you read

Finished sections get a check mark.

1 Chapter 1: Introduction & Exam Overview

1.1 Current Exam Facts 1.2 The Arizona Contractor Licensing Path 1.3 How to Use This Guide & Study Plan

2 Chapter 2: Arizona ROC & Licensing Law

2.1 The Arizona Registrar of Contractors 2.2 License Classifications 2.3 Qualifying Party & Experience Requirements 2.4 Application, Fees, Bond & Background Check 2.5 License Bonds, Cash Deposits & Bond Claims 2.6 Unlicensed Contracting: Penalties & Lost Remedies 2.7 Advertising Rules, Contract Disclosures & Workmanship Standards

3 Chapter 3: The Exams — SRE, Trade & NASCLA

3.1 The Statutes & Rules Exam (SRE) 3.2 The PSI Trade Exam 3.3 The NASCLA Commercial General Building Exam Option

4 Chapter 4: License Maintenance, Recovery Fund & Discipline

4.1 License Renewal & Continuing Education 4.2 The Residential Contractors' Recovery Fund 4.3 ROC Disciplinary Actions & Penalties

5 Chapter 5: Contract Law & Disputes

5.1 Arizona Contract Fundamentals 5.2 Construction Contract Terms & Provisions 5.3 Change Orders & Modifications 5.4 Dispute Resolution & ROC Complaints 5.5 The Arizona Prompt Payment Act

6 Chapter 6: Liens, Bonds & Insurance

6.1 Arizona Mechanics' Lien Law Overview 6.2 Lien Notices, Recording & Deadlines 6.3 Contract Bonds: Bid, Performance & Payment 6.4 Insurance Requirements

7 Chapter 7: Financial Management & Taxes

7.1 Accounting & Financial Statements 7.2 Estimating, Bidding & Markup 7.3 Taxes & Payroll

8 Chapter 8: Project Management

8.1 Scheduling & the Critical Path Method 8.2 Supervision, Subcontractors & Quality Control 8.3 Project Documentation & Closeout

9 Chapter 9: Safety & OSHA

9.1 OSHA Construction Standards Overview 9.2 Fall Protection, Scaffolds & Ladders 9.3 Excavation, Trenching & Electrical Safety 9.4 Heat Illness Prevention & Arizona Job-Site Hazards

10 Chapter 10: Building Codes, Permits & Plan Reading

10.1 IRC 2018 & IBC 2018 Fundamentals 10.2 Permits, Plan Review & Inspections 10.3 Energy Code & Accessibility 10.4 Reading Construction Drawings & Specifications 10.5 Means of Egress & Fire-Resistance-Rated Construction

11 Chapter 11: Sitework, Concrete & Masonry

11.1 Sitework: Surveying, Excavation & Grading 11.2 Concrete: Formwork, Reinforcement & Placing 11.3 Masonry: Brick, Block & Mortar 11.4 Soils, Compaction & Earthwork Testing 11.5 Concrete Materials & Mix Design 11.6 Concrete Curing, Joints, Testing & Defects 11.7 Masonry Reinforcement, Grouting & Wall Systems

12 Chapter 12: Carpentry, Metals & Building Envelope

12.1 Carpentry & Framing 12.2 Metals & Metal Framing 12.3 Thermal & Moisture Protection 12.4 Doors, Windows & Finishes 12.5 Engineered Wood, Trusses & Connectors 12.6 Structural Steel Erection & Connections 12.7 Steel Joists, Girders & Metal Deck

13 Chapter 13: Roofing, Waterproofing & Interior Finishes

13.1 Roofing Systems 13.2 Waterproofing, Flashing & Sealants 13.3 Interior Finishes: Gypsum, Stucco, Flooring & Paint

14 Chapter 14: Building Systems for the General Contractor

14.1 Mechanical & Plumbing Systems 14.2 Electrical Systems & Temporary Power

11.3 Masonry: Brick, Block & Mortar

Key Takeaways Explain This Topic AI

Masonry accounts for 10 of 100 items on the B-1/B-2 commercial trade exam.

ASTM C270 defines four mortar types — M, S, N, O — rated by compressive strength; Type N is the general-purpose mortar for above-grade brick and block walls.

Type S mortar (1,800 psi) is the standard for CMU walls below grade or resisting lateral loads, because it balances high strength with good bond.

Efflorescence — the white salt deposit on masonry — is common in Arizona's dry climate and signals moisture moving through the wall; control it with proper drainage, venting, and low-alkali materials.

Joint reinforcement (ladder or truss wire) in horizontal mortar beds and grouted, reinforced cells give CMU walls their flexural and shear capacity.

Last updated: August 2026

Brick and Concrete Masonry Units (CMU)

Masonry relies on units bonded by mortar. Two unit families dominate commercial masonry construction:

Brick (clay masonry, ASTM C216 for facing brick) — modular dimensions, weather-resistant, fired clay. Nominal size is often 2-2/3 × 4 × 8 inches (modular), with mortar joints making courses 3 inches high.

Concrete masonry units (CMU) (ASTM C90) — hollow concrete blocks, nominal 8 × 8 × 16 inches. The hollow cores accept vertical rebar and grout where reinforcement is required. CMU is the workhorse of Arizona commercial and residential foundation and retaining walls.

Mortar Types per ASTM C270

Mortar bonds units together and distributes loads. ASTM C270 classifies mortar by compressive strength into four types:

  • Type Compressive Strength (psi) Common Use
  • M 2,500 High-strength: foundations, retaining walls, below-grade, heavy loads
  • S 1,800 Below-grade CMU walls, lateral-load-resisting walls, patios
  • N 750 General above-grade exterior walls (brick veneer, parapets, chimneys)
  • O 350 Interior, non-load-bearing walls, tuck-pointing historic masonry

A useful mnemonic is "MaSoN wOrk" (M, S, N, O, from strongest to weakest). Note the trade-off: stronger mortar is not always better. Type N is more flexible and accommodates movement; Type M is brittle and can crack if the wall flexes. Match the mortar to the application, not just to the highest strength.

Quick Answer: Type N (750 psi) is the general-purpose mortar for above-grade brick and block; Type S (1,800 psi) is standard for reinforced CMU and below-grade walls.

Mortar Mixing

Mortar is mixed from cement, lime, sand, and water. Field proportioning by volume must match the ASTM C270 recipe. Lime adds workability and water retention; cement provides strength. Retempering — adding water to dry mortar — is permitted once within 2.5 hours of original mixing, but mortar that has set beyond that must be discarded. Over-retempering weakens the mortar.

Laying Techniques: Bond Patterns and Joints

Bond patterns distribute load and create the visible face. Common patterns:

Running bond — the default for CMU and most brick. Each unit overlaps the one below by half its length. Simple, strong, and standard.

Stack bond — units align vertically with continuous head joints. Aesthetically striking but structurally weak without joint reinforcement; the 2018 IBC and TMS (The Masonry Society) 402 require horizontal joint reinforcement at 24 inches on center for stack bond.

Common bond (American bond) — brick walls with a course of headers every 5–6 courses to tie wythes together.

Mortar joints are typically 3/8 inch thick. Joint profile affects weather resistance:

Concave (tooled) — the most weather-resistant; compresses mortar against the unit edge. Standard for exterior walls.

V-joint — similar weather resistance, decorative.

Raked — recessed; looks good but collects water, so it is only for interior or sheltered walls.

Flush or struck — quick but offers little weather shedding.

Reinforcement: Joint Reinforcement and Grouted Cells

Masonry walls resist wind and seismic loads through a combination of units, mortar, and reinforcement:

Joint reinforcement — galvanized or stainless steel wire (ladder or truss type) laid in horizontal mortar beds, typically every 16 inches for CMU. It controls shrinkage cracking and ties the wall together.

Grouted cells — vertical CMU cores are filled with grout (a fluid concrete mix) around vertical rebar. The 2018 IBC, adopting TMS 402, specifies minimum vertical reinforcement for reinforced masonry walls — spacing and bar size depend on seismic design category and wall loads.

Bond beams — horizontal courses of U-shaped CMU filled with grout and horizontal rebar, placed at the top of walls and at lintels to spread loads and tie the wall together.

Grout for reinforced masonry is specified by ASTM C476. Coarse grout (max aggregate 3/8 inch) is used for cells 2 inches or wider; fine grout is used for smaller cells. Minimum grout compressive strength is typically 2,000 psi . Grout is placed in lifts of up to 12 inches and consolidated by vibration or puddling to eliminate voids around the rebar.

Weather Resistance

Masonry is durable but not waterproof. Weather resistance depends on:

Proper mortar type and fully filled joints (no voids).

Tooled concave joints that shed water.

Flashing and weep holes at the base of brick veneer to let trapped water escape. Weep holes are typically spaced 24–33 inches on center.

Water-resistant coatings (silane/siloxane sealers) on porous units, where specified.

Arizona Considerations: Efflorescence and Corrosion

Efflorescence — the white, powdery salt deposit that appears on masonry surfaces — is common in Arizona. It forms when water-soluble salts in the mortar, units, or soil dissolve, migrate to the surface, and crystallize as the water evaporates. Arizona's dry, hot climate accelerates evaporation, driving salts to the surface quickly. Control efflorescence by:

Limiting water entry — good flashing, drainage, and cap break details.

Using low-alkali cement and clean, salt-free sand.

Storing units off the ground and covering them before installation.

Venting cavity walls so moisture escapes.

Corrosion of joint reinforcement and rebar is accelerated by chlorides (from soil or deicing salts) and by moisture. Use hot-dip galvanized or stainless steel joint reinforcement in exposed or corrosive environments, and maintain adequate grout cover around vertical rebar in CMU cells.

Reinforced CMU Wall Cross-Section REINFORCED CMU WALL -- CROSS SECTION

  • +--------+--------+--------+--------+
  • |==== bond beam ====|========|==== | U-block w/ grout + horiz. rebar
  • +--------+--------+--------+--------+
  • | | || | | | joint reinforcement
  • | CMU | || | CMU | CMU | (ladder/truss wire)
  • | | || | | |
  • | [G] | || | [G] | [G] | [G] = grouted cell
  • | | || | | | || = vertical rebar
  • | | || | | |
  • +--------+--------+--------+--------+
  • | footing / slab |
  • +------------------------------------+
  • Vertical rebar in grouted cells resists flexure
  • Joint reinforcement controls shrinkage cracking
  • Bond beams tie the wall together at top and lintels