Study guide

Dk, Dk/t, Thermal Conductivity & Holden-Mertz

NCLE CLRE Contact Lens Registry Exam Study Guide Exam

Track your progress as you read

Finished sections get a check mark.

1 Introduction & Exam Overview

0.1 About the CLRE Exam 0.2 How to Use This Study Guide

2 Ocular Anatomy: Adnexa

Tear Film: Layers, Glands & Break-Up Time Conjunctiva, Lids, Lashes, Fornix & Canthi Blink Rate, Lid Function & Contact Lens Wear Effects

3 Ocular Anatomy: Anterior & Posterior Segment

Corneal Layers, Curvature, Topography & Metabolism Iris, Pupil, Sclera & Anterior Chamber Crystalline Lens, Retina, Choroid & Posterior Chamber

4 Refractive Errors & Contact Lens Optics

Myopia, Hyperopia, Astigmatism, Presbyopia & Anisometropia Refraction, Prism, Lacrimal Lens, Accommodation & Transposition Vertex Distance, Sagittal Depth & Spherical Equivalent

5 Measurement Instrumentation

Keratometer/Ophthalmometer: Calibration, Readings & Interpretation Corneal Topography & OCT for Contact Lens Fitting Schirmer Tests & Tear Break-Up Time

6 Observation & Verification Instrumentation

Slit Lamp (Biomicroscope) Operation & Illumination Slit Lamp Evaluation With & Without Contact Lenses Radiuscope, Lensometer, Thickness Gauge & ANSI Z80

7 Prefitting Patient Evaluation

6.1 Lifestyle, Occupation, Environment & Motivation 6.2 Medical History, Diseases, Medications & Allergies 6.3 Contraindications & Factors for Successful Wear 6.4 Relating Corneal Measurements, Rx & Lens Parameters

8 Lens Materials, Design & Parameter Selection

Dk, Dk/t, Thermal Conductivity & Holden-Mertz Water Content, Wetting Angle, Modulus, Silicone Hydrogel & Surface Treatments Toric, Multifocal, Aspheric, Hybrid, Scleral, Orthokeratology & Quadrant-Specific Base Curve, Peripheral Curves, Diameter, Thickness, Power & Edge Design

9 Diagnostic Fitting Procedures

8.1 Lens Selection & Application Procedures 8.2 Fluorescein Pattern Evaluation for RGP Lenses 8.3 Soft Lens Movement, Centration & Coverage

10 Fit Evaluation & Over-Refraction

Toric Lens Axis Rotation, LARS Rule & Stabilization Patient Comfort, Visual Acuity & Over-Refraction Modifying Base Curve, Diameter, Sag & Power from Findings

11 Dispensing: Wearing Schedules & Replacement

Daily, Flexible & Extended/Continuous Wear Schedules Daily, Biweekly, Monthly & Conventional Replacement Adaptation Protocols & Patient Compliance Counseling

12 Dispensing: Lens Care Systems

Solution Compatibility with Lens Types Chemical, Heat/UV, Hydrogen Peroxide & Neutralization Surfactant Cleaners, Protein Removers & Weekly Cleaning Solution Sensitivities, Incompatibilities & Adverse Reactions

13 Dispensing: Handling & Hygiene

12.1 Soft Lens Insertion & Removal Techniques 12.2 RGP Insertion, Removal & Emergency Responses 12.3 Hygiene, Soaps, Cosmetics & Storage Containers 12.4 Verifying Lens Parameters Against the Order at Dispensing

14 Follow-Up: Subjective & Objective Findings

13.1 Subjective Complaints: Dryness, Awareness, Blurry Vision, Pain & Photophobia 13.2 Steep vs Flat Lens Fit (Rigid & Soft) & Everted Lens 13.3 Injection, Edema, Discharge, Vision Loss & Lid Problems 13.4 Visual Acuity, Over-Refraction & Gross Evaluation Techniques

15 Follow-Up: Staining Patterns & Complications

14.1 Staining Patterns: 3 & 9 O'Clock, Foreign Body, SPK, Arcuate, Smile & Dimple Veiling 14.2 SEAL, CLARE, VLK, SLK & CLPU 14.3 Microbial Keratitis, Acanthamoeba, Dendritic Ulcer & Infiltrates 14.4 Corneal Molding/Warpage, Dellen & Mucin Balls

16 Follow-Up: Management Protocols

GPC, Blepharitis, Ptosis & Tarsal Plate Evaluation Daily Wear, Extended, Therapeutic, Postsurgical & Pathology Protocols Changing Lens Parameters at Follow-Up & Documenting Records

17 Regulatory & Administrative

FCLCA, FDA, FTC, Contact Lens Rule & Prescriber Verification HIPAA, PHI, OSHA, CDC, ANSI & Universal Precautions Record Retention, Inventory, Ordering & Documentation Methodology

Dk, Dk/t, Thermal Conductivity & Holden-Mertz

Key Takeaways Explain This Topic AI

Oxygen permeability (Dk) is an intrinsic material property with units ×10⁻¹¹ (cm²/s)(mL O₂/mL·mmHg); oxygen transmissibility (Dk/t) is Dk divided by lens thickness in centimeters and is what the cornea actually experiences.

Holden-Mertz criteria: Dk/t ≥24 for daily wear and ≥87 for extended wear, each calibrated to keep overnight corneal edema at or below 3.2%.

Traditional hydrogels scale Dk with water content (range 8–40); silicone hydrogels decouple water from Dk, reaching Dk 60–140+ at low water content.

Sub-threshold Dk/t produces corneal edema, microcysts, limbal neovascularization, reduced epithelial barrier (higher infection risk), and endothelial polymegethism.

Dk is measured polarographically (ANSI Z80.20); the coulometric method measures oxygen transmitted through the lens.

Last updated: July 2026

Oxygen Transmissibility: Dk, Dk/t, Thermal Conductivity & Holden-Mertz

Quick Answer: Oxygen permeability (Dk) is an intrinsic material property; oxygen transmissibility (Dk/t) is what the cornea actually experiences once lens thickness is factored in. The classic Holden-Mertz criteria — Dk/t ≥24 for daily wear and Dk/t ≥87 for extended wear — are the clinical thresholds calibrated to keep overnight corneal edema at or below ≈4% (the no-lens overnight baseline in the 1984 study). Later reviews revise the no-lens baseline downward (~3.2%) and push the extended-wear target toward Dk/t ≥125 .

Oxygen Permeability (Dk)

Oxygen permeability (Dk) is an intrinsic property of a contact lens material, independent of lens thickness or design. The ANSI unit is ×10⁻¹¹ (cm²/s)(mL O₂/mL·mmHg). Dk measures how easily oxygen molecules diffuse through the polymer matrix.

  • D = diffusion coefficient (how fast O₂ moves through the material)
  • k = solubility coefficient (how much O₂ the material can hold)

Traditional hydrogels rely on water to carry oxygen. Because water has a Dk of about 80, raising water content raises Dk — but only up to a ceiling near Dk 40. Silicone hydrogels break this rule : silicone itself is highly oxygen-permeable, so SiHy lenses achieve high Dk with low water content.

Oxygen Transmissibility (Dk/t)

The cornea does not "see" Dk — it experiences oxygen transmissibility (Dk/t) , which is Dk divided by lens thickness (t, in centimeters):

Dk/t = Dk / t(cm)

Conventionally, Dk is reported in ×10⁻¹¹ units and Dk/t is reported in ×10⁻⁹ units (the thickness division shifts the exponent). The same material with two different center thicknesses produces two different Dk/t values. A −3.00 D lens is thinner than a +3.00 D lens of the same material, so the minus lens has higher Dk/t. Manufacturers therefore quote Dk/t at a reference thickness (commonly −3.00 D at t = 0.09 mm or 0.06 mm).

Dk Reference Table by Material

  • Material (Class) Example Brand Dk Typical Dk/t (−3.00 D)
  • PMMA — 0 0
  • Low-water hydrogel (38%) polymacon (SofLens 38) 8–9 ~10
  • Mid-water hydrogel (55%) vifilcon A (Focus Monthly) 18–22 ~20
  • High-water hydrogel (70%) latocofilcon A (Ultra Health) 34–40 ~30
  • 1st-gen SiHy lotrafilcon A (Night & Day) 140 175
  • 2nd-gen SiHy balafilcon A (PureVision) 91 110
  • 3rd-gen SiHy comfilcon A (Biofinity) 128 160
  • 4th-gen SiHy senofilcon A (Acuvue Oasys) 103 147
  • Holden-Mertz Criteria

The Holden & Mertz (1984) study established the minimum Dk/t required to limit overnight corneal edema to ≈4% — the average physiologic edema level they measured during overnight eye closure with no lens in place. Later literature revised that no-lens baseline and argued the extended-wear critical Dk/t should be raised to about 125 ×10⁻⁹ .

  • Wear Schedule Classic Holden-Mertz Dk/t Clinical Goal (1984 study)
  • Daily wear ≥24 ×10⁻⁹ Avoid open-eye edema
  • Extended wear ≥87 ×10⁻⁹ Overnight edema ≤≈4% with lens on
  • Revised EW target (later reviews) ≥125 ×10⁻⁹ Match revised ~3.2% no-lens overnight edema

A daily-wear lens is removed before sleep, so a lower Dk/t is tolerated because the cornea recovers overnight. An extended-wear lens stays on the eye for 6+ consecutive nights, so it must deliver near-physiologic oxygen to avoid chronic hypoxia.

  • Consequences of Sub-Threshold Dk/t
  • Corneal edema (stromal swelling, striae at >5%, folds at >8%)
  • Epithelial microcysts (appear during extended-wear recovery)
  • Limbal hyperemia and neovascularization
  • Reduced epithelial barrier → higher infection risk (Pseudomonas, Acanthamoeba)
  • Endothelial polymegethism (chronic hypoxic stress)
  • Myopic creep in long-term hypoxic pediatric wear
  • Silicone Hydrogel vs Traditional Hydrogel

Silicone hydrogel (SiHy) materials were engineered to break the water-content/Dk coupling. Silicone provides oxygen permeability; water provides wettability and on-eye mobility. SiHy Dk values range from 60 to 140+ , versus traditional hydrogels at 8 to 40 .

Because silicone is hydrophobic, SiHy lenses require surface treatment or internal wetting agents to be comfortable (covered in §7.2). First-generation SiHy (lotrafilcon A, balafilcon A) used plasma surface treatment and high modulus; modern generations use internal wetting agents and lower modulus.

Thermal Conductivity

Thermal conductivity is the rate at which a lens material transfers heat between the warm cornea/tear film and the cooler ambient environment. Materials with poor thermal conductivity (low water, high silicone content) can cause a mild cooling sensation or, in extreme cases, contribute to low-grade corneal cooling during extended wear. PMMA, traditional hydrogels, and SiHy conduct heat differently; this is a minor but tested point on the CLRE.

Measuring Dk: Polarographic Method

The ANSI Z80.20 standard method is the polarographic electrode technique :

A lens sample is placed on a polarographic oxygen sensor.

The sensor consumes oxygen at a known rate, creating a current proportional to O₂ flux.

Dk is calculated from the steady-state current after correcting for edge effects and boundary-layer resistance.

The coulometric method is an alternative that measures oxygen that passes through the lens to a sensor on the far side — useful for very high Dk materials where polarographic edge corrections become unreliable. Both methods apply edge correction (because oxygen diffuses laterally at the lens edge, inflating apparent flux) and boundary-layer correction (the tear-film boundary layer itself resists oxygen flux). Without these corrections, Dk is overestimated, especially for high-Dk SiHy.

Worked Dk/t Example

A patient wears a senofilcon A lens (Dk 103) at −3.00 D with center thickness 0.07 mm. Convert t to centimeters: 0.07 mm = 0.007 cm. Then Dk/t = 103 / 0.007 ≈ 147 — comfortably above both Holden-Mertz thresholds, so this lens qualifies for extended wear on oxygen criteria alone (final decision also depends on surface chemistry, modulus, and follow-up). Now consider the same material at +10.00 D where center thickness rises to 0.20 mm (0.020 cm): Dk/t = 103 / 0.020 ≈ 51 — below the extended-wear threshold. A high-plus patient who was told their lens is "extended-wear approved" may actually be hypoxic at their personal Rx.

Clinical Bottom Line

Dk is the material; Dk/t is the lens.

Use SiHy for extended wear, high Rx, and edema-prone patients.

Verify Dk/t at the patient's actual Rx, not the −3.00 D marketing number — high-plus lenses have much lower Dk/t than the brochure.

For a fragile dry-eye patient, the silicone advantage (high Dk, low dehydration) often outweighs the modulus and surface issues that come with SiHy.