Study guide

3.3 Gas Laws, Dalton Partial Pressures, Arc Dissociation & Sieverts Law

AWS CWEng Certified Welding Engineer Exam

Track your progress as you read

Finished sections get a check mark.

1 Introduction & CWEng Exam Overview

About the CWEng Exam: Four Parts, 163 Questions & Testing Logistics Scoring, Composite Weighting, Eligibility & Five-Year Renewal How to Use This Guide & Build Your Open-Book Reference Set

2 Chapter 1: Mathematics & Statistics for Welding Engineers

1.1 Engineering Mathematics: Algebra, Trigonometry & Geometry in Weldments 1.2 Differential & Integral Calculus Fundamentals in Engineering Analysis 1.3 Applied Engineering Statistics, Population Distributions & Quality Metrics 1.4 Polynomial Equations, Conic Sections & Complex Numbers

3 Chapter 2: Physics Fundamentals & Mechanics

2.1 Unit Systems, Dimensional Analysis & Engineering Conversions 2.2 Mechanics: Statics, Equilibrium, Force Vectors & Moments 2.3 Work, Energy, Power & Mechanical Advantage in Welding Systems 2.4 Thermal Physics, Linear/Volumetric Expansion & Heat Capacity

4 Chapter 3: General & Physical Chemistry for Welding

3.1 Atomic Structure, Bonding & Solid-Solution Thermodynamics 3.2 Hume-Rothery Compatibility, Interstitial Strain & HSLA Microalloy Scavenging 3.3 Gas Laws, Dalton Partial Pressures, Arc Dissociation & Sieverts Law 3.4 Cylinder Capacity, Available Arc Time & Gas-Related Porosity Diagnosis 3.5 Redox Thermodynamics, Deoxidation & Slag-Metal Refining 3.6 Basicity Index Calculations, Toughness Prediction & Cryogenic Consumable Selection

5 Chapter 4: Strength of Materials & Mechanics of Materials

4.1 Engineering vs. True Stress-Strain, Elastic Constants & Z-Direction Ductility 4.2 Plane Stress vs. Plane Strain, Triaxial Restraint & Alloy Property Comparison 4.3 Beam Bending, Transverse Shear, Torsion & Mohr Circle Construction 4.4 Multiaxial Yield Criteria & Combined-Load Analysis of Welded Members 4.5 Fatigue Life, Weld-Toe Stress Concentration & Paris-Erdogan Crack Growth 4.6 LEFM Fracture Toughness, Ductile-Brittle Transition & Larson-Miller Creep 4.7 Comparative Failure-Mode Synthesis & Integrated Flaw and Creep Assessment

6 Chapter 5: Heat Transfer & Fluid Mechanics in Welding

5.1 Fourier Conduction, Rosenthal Moving Heat Source & 2D vs. 3D Heat Flow 5.2 Adams Cooling Rate, the t8/5 Window & HAZ Peak-Temperature Distribution 5.3 Convection, Stefan-Boltzmann Radiation & Emissivity of Weld Surfaces 5.4 Arc Radiation Losses, Preheat Maintenance & PWHT Boundary Conditions 5.5 Fluid Statics, Bernoulli, Viscosity & Reynolds-Number Regimes 5.6 Gas Lens Mechanics, Buoyancy Effects & Torch Flow Design 5.7 Hyperbaric, Vacuum & Controlled-Atmosphere Welding Environments

7 Chapter 6: Electrical Engineering Principles for Welding Systems

6.1 DC and AC Waveforms, Polarity Thermodynamics & Welding Circuit Analysis 6.2 Joule Heating, Electrode Stickout Preheating & Circuit Voltage Distribution 6.3 Power Factor, Reactance, Impedance & Magnetic Transformer Principles 6.4 Lorentz Force, Electromagnetic Pinch Effect & Arc Blow

8 Chapter 7: Welding Heat Sources & Arc Physics

7.1 Volt-Ampere Characteristics, Operating Point, Self-Regulation & OCV Limits 7.2 Inductance, Slope Control & Dynamic Power-Source Response 7.3 Arc Fall Regions, Cathode Emission Mechanisms & Shielding-Gas Ionization 7.4 Maecker Plasma Jet, Degree of Ionization & Anode Heat Partitioning 7.5 Droplet Force Balance & Classification of Metal Transfer Regimes 7.6 Transition Current, Mode Comparison & Pulsed Waveform Design

9 Chapter 8: Arc Welding Processes & Parameter Controls

8.1 Shielded Metal Arc Welding (SMAW): Electrode Flux Chemistries & Variables 8.2 GMAW Process Physics, Transfer Modes & Shielding Gas Interactions 8.3 Solid, Metal-Cored & Flux-Cored Wires with CTWD and Parameter Envelopes 8.4 Gas Tungsten (GTAW) & Plasma Arc Welding (PAW): Electrodes & Keyholing 8.5 Submerged Arc Welding (SAW): Flux Basicity, Multi-Wire & High-Deposition Systems

10 Chapter 9: Advanced, Resistance & Solid-State Joining Processes

9.1 High-Energy-Density Beam Physics & Electron Beam Welding 9.2 Laser Beam Welding, EBW/LBW Comparison & Fiber Laser Parameter Derivation 9.3 Resistance Welding Physics, Electrode Materials & Spot Weld Sequence 9.4 Nugget Sizing, Seam and Projection Welding, and Lobe Curve Process Windows 9.5 Solid-State Joining: Friction Stir Welding (FSW), Explosion & Diffusion 9.6 Thermal Cutting & Gouging: Oxyfuel, Plasma Arc and Air Carbon Arc 9.7 High-Frequency, Flash, Stud & Ultrasonic Welding; Surfacing and Thermal Spray

11 Chapter 10: Physical & Transformation Metallurgy of Steels

10.1 Fe-Fe3C System, Crystal Lattices, c/a Ratio & Interstitial Solubility 10.2 Critical Temperatures, Invariant Reactions & the Lever Rule 10.3 Alloying Elements, the Gamma Loop & Phase-Fraction Calculations 10.4 TTT and CCT Diagrams, Constitutional Supercooling & Scheil Microsegregation 10.5 Non-Equilibrium Transformation Products & Martensite Modeling 10.6 HAZ Anatomy, Microstructural Sub-Zones & Multi-Pass Reheated Regions 10.7 HAZ Hardness Traverses, Toughness Gradients & Peak-Temperature Control

12 Chapter 11: Weldability, Cracking Mechanisms & Alloy Metallurgy

11.1 Hydrogen Cracking Conditions, Carbon Equivalent & Diffusible Hydrogen Control 11.2 Preheat, Interpass and Post-Heat Calculations for Cold-Crack Prevention 11.3 Solidification Cracking, Bead Aspect Ratio, Liquation & Lamellar Tearing 11.4 Lamellar Tearing Mitigation & Hot-Cracking Susceptibility Evaluation 11.5 Stainless Families, Schaeffler and WRC-1992 Diagrams, Ferrite Number & Sensitization 11.6 Duplex Stainless Metallurgy & Dissimilar-Metal Ferrite Prediction 11.7 Aluminum Oxide and Porosity Control, and Titanium Reactive-Metal Welding 11.8 Nickel Superalloys, Strain-Age Cracking & Guinier-Preston Aging Sequences

13 Chapter 12: Weldment Design, Stress Analysis & Joint Mechanics

12.1 AWS A2.4 Welding Symbol Anatomy, Symbol Library & Dimension Syntax 12.2 Joint Architecture, CJP versus PJP, and NDE Examination Symbols 12.3 Fillet and Groove Weld Sizing under Direct Stress in ASD and LRFD 12.4 Plug and Slot Welds, Stress Gradients & the Fillet Weld Break Test 12.5 Eccentric Loading Analysis: Elastic Vector Method vs Instantaneous Center 12.6 Fatigue Design of Welded Connections & Residual Stress/Distortion Control

14 Chapter 13: Non-Destructive Examination (NDE) & Discontinuity Analysis

13.1 Visual Testing Gages & Liquid Penetrant Capillary Mechanics 13.2 Magnetic Particle Testing: Flux Leakage, Field Geometry & Prod Amperage 13.3 Radiographic Physics, Geometric Unsharpness, Density & IQI Sensitivity 13.4 Computed and Digital Radiography & Radiographic Discontinuity Interpretation 13.5 Acoustic Wave Mechanics, Refraction & Angle-Beam Sound-Path Geometry 13.6 AWS D1.1 Decibel Rating, Phased Array & Time-of-Flight Diffraction

15 Chapter 14: Brazing, Soldering & Industrial Welding Safety

14.1 Brazing Thermodynamics, Capillary Wetting Physics & Joint Clearance 14.2 AWS A5.8 Brazing Filler Metals, FB Fluxes & Industrial Heating Processes 14.3 Soldering Fundamentals, Flux Chemistries & Intermetallic Formation 14.4 Hierarchy of Controls, Electric Shock Physics & Industrial Ventilation 14.5 Fume Exposure Limits, Arc Radiation, Hot Work and Confined-Space Entry 14.6 Arc-Generated Toxic Gases, Moving-Equipment Hazards & TWA Exposure Calculation

16 Chapter 15: Structural Fabrication & AWS D1.1 Code Implementation

15.1 AWS D1.1 Scope, Prequalification Limits, Base-Metal Groups & Matching Filler 15.2 Prequalified Joint Details, Backing Systems & Joint Specification Verification 15.3 Thermal Cut Edges, Fit-Up Tolerances & Minimum Preheat Requirements 15.4 Preheat Application Zones, Measurement Instrumentation & Fabrication Audits 15.5 PWHT Fundamentals, D1.1 Thermal Cycles & Visual Acceptance Criteria 15.6 D1.1 Nondestructive Examination Protocols, PWHT Scheduling & Visual Audit Practice

17 Chapter 16: Welding Procedure Qualification (WPS & PQR) per ASME IX & AWS B2.1

16.1 PQR versus WPS Hierarchy, Qualification Workflow & Standard Procedures 16.2 Manufacturer Responsibility, Subcontracting Limits & Multi-Process Qualification 16.3 Essential, Supplementary Essential and Nonessential Variables with Heat Input Mechanics 16.4 Waveform-Controlled Power Sources, Appendix H & Heat-Input Compliance 16.5 P-Numbers, Group Numbers, F-Numbers & A-Numbers 16.6 QW-451 Mechanical Test Protocols & Procedure Qualification Test Evaluation

18 Chapter 17: Filler Metal Specifications, Selection & Consumable Control

17.1 AWS A5 Architecture: SMAW, GMAW/GTAW and FCAW Consumable Classifications 17.2 SAW Wire-Flux Systems, Alloy Pickup & PWHT Property Effects 17.3 Stainless Filler Specifications, Solidification Modes & Dissimilar-Metal Joints 17.4 AWS A5.10 Aluminum Filler Selection & Dilution and Ferrite-Number Calculations 17.5 Consumable Storage, Conditioning Envelopes & Atmospheric Exposure Limits 17.6 Low-Hydrogen Designators, the Yurioka Parameter & Preheat Sizing

19 Chapter 18: Welder Performance Qualification, Quality Management & Welding Economics

18.1 Welder Qualification Philosophy, Test Positions & Thickness and Diameter Ranges 18.2 F-Number Hierarchy, Operator Qualification & Continuity Requirements 18.3 ISO 3834, Welding Coordination, Inspection Test Plans & Equipment Validation 18.4 EN 10204 Material Certification, Traceability & Heat-Input Nonconformance Auditing 18.5 Weld Cost Anatomy, Deposition Rates, Operating Factor & the Overwelding Law 18.6 Economic Optimization Strategies & Fabrication Cost Comparison

3.3 Gas Laws, Dalton Partial Pressures, Arc Dissociation & Sieverts Law

Key Takeaways Explain This Topic AI

Shielding gas behavior follows the ideal gas law (PV = nRT); helium's low density (0.166 kg/m³ vs argon's 1.66 kg/m³) causes rapid buoyant rise, requiring flow rates 2x to 3x higher than argon for equivalent weld pool protection.

Dalton's law of partial pressures dictates that each component in a shielding gas blend exerts a partial pressure proportional to its volume/mole fraction, directly governing its chemical activity at the molten metal surface.

High arc column temperatures (3000 to 20,000 K) trigger the endothermic dissociation of diatomic gases (CO2, O2, H2, N2), which absorb energy in the plasma core and release it exothermically upon recombining at the cooler weld puddle.

Sieverts' law dictates that the equilibrium concentration of diatomic gases dissolved in liquid metal is proportional to the square root of their partial pressure ([wt% X] = K_X · (P_X2)^0.5).

Active gas additions to argon modify droplet surface tension: 1–5% O2 lowers the critical current required for stable axial spray transfer, whereas >18–20% CO2 restricts GMAW to globular or short-circuiting transfer modes.

Last updated: September 2026

3.2 Stoichiometry, Gas Laws & Partial Pressures in Shielding Gases

Shielding gases in arc welding serve two primary purposes: physically displacing ambient air (nitrogen, oxygen, and moisture) to prevent weld contamination, and establishing an ionized plasma medium that controls electrical arc characteristics, droplet detachment mode, and weld pool thermocapillary fluid flow.

1. Gas Stoichiometry & Equations of State in Welding Systems

Stoichiometric calculations in gas-shielded processes (GMAW, GTAW, FCAW-G, PAW) link mass, molar volume, and volumetric consumption rates. The chemical mole ( n n n ) represents N A = 6.022 × 10 23 N_A = 6.022 \times 10^{23} N A ​ = 6.022 × 1 0 23 particles: n = m M n = \frac{m}{M} n = M m ​

where m m m is mass (g) and M M M is molar mass (g/mol).

The Ideal Gas Law

At the temperatures and pressures typical of industrial gas delivery systems ( P < 25 MPa P < 25\text{ MPa} P < 25 MPa , T > 250 K T > 250\text{ K} T > 250 K ), shielding gases closely follow the ideal gas equation of state: P V = n R T = m M R T P V = n R T = \frac{m}{M} R T P V = n RT = M m ​ RT

where:

  • P P P = absolute pressure ( Pa \text{Pa} Pa or N/m 2 \text{N/m}^2 N/m 2 )
  • V V V = volume ( m 3 \text{m}^3 m 3 )
  • n n n = quantity of gas ( mol \text{mol} mol )

R R R = universal gas constant = 8.31446 J / ( mol ⋅ K ) = 0.082057 L ⋅ atm / ( mol ⋅ K ) = 8.31446\ \text{J}/(\text{mol}\cdot\text{K}) = 0.082057\ \text{L}\cdot\text{atm}/(\text{mol}\cdot\text{K}) = 8.31446 J / ( mol ⋅ K ) = 0.082057 L ⋅ atm / ( mol ⋅ K )

T T T = absolute temperature in Kelvin ( K = ∘ C + 273.15 \text{K} = {}^\circ\text{C} + 273.15 K = ∘ C + 273.15 )

Gas Density and Buoyancy Dynamics

Rearranging the ideal gas law yields gas density ρ \rho ρ as a direct function of molar mass, pressure, and temperature: ρ = m V = P M R T \rho = \frac{m}{V} = \frac{P M}{R T} ρ = V m ​ = RT PM ​ Gas Formula Molar Mass (g/mol) Density at 20°C, 1 atm (kg/m³) Specific Gravity Relative to Air

  • Helium He 4.003 0.166 0.138 (strongly buoyant)
  • Nitrogen N₂ 28.013 1.165 0.967 (neutral)
  • Air (ambient) — 28.964 1.204 1.000 (reference baseline)
  • Oxygen O₂ 31.999 1.331 1.105 (slightly sinking)
  • Argon Ar 39.948 1.661 1.379 (sinking, blankets weld)
  • Carbon Dioxide CO₂ 44.010 1.842 1.529 (heavily sinking)
  • Fluid Mechanics of Shielding Coverage: Argon vs. Helium

Because argon has a specific gravity of 1.38 1.38 1.38 relative to air, it tends to sink and spread across the workpiece, establishing a stable, laminar protective blanket over the weld pool in flat and horizontal positions. Typical argon flow rates range from 20 to 35 CFH 20\text{ to }35\text{ CFH} 20 to 35 CFH ( 9.4 to 16.5 L/min 9.4\text{ to }16.5\text{ L/min} 9.4 to 16.5 L/min ).

Conversely, helium has a specific gravity of only 0.14 0.14 0.14 , making it roughly seven times lighter than air. In an open shop environment, buoyant thermal plume forces cause helium to rise rapidly away from the torch nozzle. To maintain an equivalent protective barrier against atmospheric aspiration, helium requires volumetric flow rates two to three times higher than argon —typically 40 to 60 CFH 40\text{ to }60\text{ CFH} 40 to 60 CFH ( 18.9 to 28.3 L/min 18.9\text{ to }28.3\text{ L/min} 18.9 to 28.3 L/min ).

2. Dalton's Law of Partial Pressures in Gas Mixtures

Industrial shielding formulations are rarely pure gases; they are engineered binary and ternary mixtures designed to balance arc stability, penetration profile, travel speed, and spatter generation.

John Dalton established that the total pressure P total P_{\text{total}} P total ​ exerted by a mixture of non-reacting ideal gases equals the sum of the partial pressures P i P_i P i ​ exerted by each individual gas: P total = ∑ i = 1 k P i = P 1 + P 2 + P 3 + ⋯ + P k P_{\text{total}} = \sum_{i=1}^{k} P_i = P_1 + P_2 + P_3 + \dots + P_k P total ​ = i = 1 ∑ k ​ P i ​ = P 1 ​ + P 2 ​ + P 3 ​ + ⋯ + P k ​

For an ideal gas, the partial pressure P i P_i P i ​ is directly proportional to its mole fraction x i x_i x i ​ , which is identical to its volumetric fraction in the mixture: x i = n i n total = V i V total ⟹ P i = x i P total x_i = \frac{n_i}{n_{\text{total}}} = \frac{V_i}{V_{\text{total}}} \qquad \implies \qquad P_i = x_i P_{\text{total}} x i ​ = n total ​ n i ​ ​ = V total ​ V i ​ ​ ⟹ P i ​ = x i ​ P total ​ Shielding Blend Composition (Vol %) Partial Pressures at 1.0 atm (101.325 kPa) Primary Welding Application

98% Ar / 2% O₂ x_Ar = 0.98, x_O2 = 0.02 P_Ar = 99.30 kPa, P_O2 = 2.03 kPa GMAW spray transfer on stainless and C-steels

90% Ar / 10% CO₂ x_Ar = 0.90, x_CO2 = 0.10 P_Ar = 91.19 kPa, P_CO2 = 10.13 kPa GMAW spray/pulse on structural steels

75% Ar / 25% CO₂ (C25) x_Ar = 0.75, x_CO2 = 0.25 P_Ar = 75.99 kPa, P_CO2 = 25.33 kPa GMAW short-circuiting mode; deep penetration

50% Ar / 50% He x_Ar = 0.50, x_He = 0.50 P_Ar = 50.66 kPa, P_He = 50.66 kPa GTAW/GMAW thick aluminum and copper

98% Ar / 2% N₂ x_Ar = 0.98, x_N2 = 0.02 P_Ar = 99.30 kPa, P_N2 = 2.03 kPa GTAW duplex stainless steel phase balance

The Chemical Role of Partial Pressure

In welding thermochemistry, the chemical activity and driving force for elemental oxidation or gas dissolution in the liquid weld pool depend on the partial pressure of the gas species at the pool surface, not its total supply pressure:

In an Ar − 2 % O 2 \text{Ar} - 2\%\ \text{O}_2 Ar − 2% O 2 ​ blend at 1.0 atm 1.0\text{ atm} 1.0 atm , P O 2 = 0.02 atm P_{\text{O}_2} = 0.02\text{ atm} P O 2 ​ ​ = 0.02 atm . This low oxygen potential lowers the liquid droplet's surface tension without causing excessive loss of oxidizable alloying elements (such as Mn \text{Mn} Mn and Si \text{Si} Si ).

In a 100 % CO 2 100\%\ \text{CO}_2 100% CO 2 ​ shield, P CO 2 = 1.0 atm P_{\text{CO}_2} = 1.0\text{ atm} P CO 2 ​ ​ = 1.0 atm . Extensive dissociation at arc temperatures produces high levels of active monatomic oxygen, requiring highly deoxidized filler wires (such as AWS A5.18 ER70S-6) to prevent carbon boil porosity.

3. High-Temperature Arc Column Dissociation & Recombination Kinetics

An electric welding arc generates core temperatures ranging from 10 , 000 to 20 , 000 K 10,000\text{ to }20,000\text{ K} 10 , 000 to 20 , 000 K , with periphery temperatures between 3 , 000 and 7 , 000 K 3,000\text{ and }7,000\text{ K} 3 , 000 and 7 , 000 K . At these temperatures, polyatomic and diatomic molecules dissociate endothermically into neutral atoms, ions, and free electrons: Dissociation Reaction Standard Enthalpy ΔH° (kJ/mol) Onset Temp (K) Key Thermochemical Consequence in the Arc

  • CO₂ ⇌ CO + ½ O₂ +283 ~2,000 Releases reactive oxygen; dissociates fully above 4,000 K
  • O₂ ⇌ 2 O +498 ~3,000 Lowers liquid droplet surface tension; stabilizes spray mode
  • H₂ ⇌ 2 H +436 ~2,500 High thermal conductivity; risk of cold cracking (HICC)
  • N₂ ⇌ 2 N +945 ~4,000 Extremely strong triple bond; dissolves interstitially in steel
  • The Thermodynamics of Enthalpy Transfer

Molecular dissociation and recombination serve as a potent heat transport mechanism within the arc:

Endothermic Dissociation in the Arc Column: When diatomic gases (such as H 2 \text{H}_2 H 2 ​ or CO 2 \text{CO}_2 CO 2 ​ ) enter the high-temperature core of the arc, they absorb massive quantities of thermal energy to break their molecular bonds ( 436 kJ/mol 436\ \text{kJ/mol} 436 kJ/mol for H 2 \text{H}_2 H 2 ​ , 945 kJ/mol 945\ \text{kJ/mol} 945 kJ/mol for N 2 \text{N}_2 N 2 ​ ). This dissociation cools the central plasma core, constricting the arc column and increasing current density.

Exothermic Recombination at the Workpiece: As the dissociated monatomic atoms ( H , O , N H, O, N H , O , N ) are driven downward by plasma jet flow (Maecker effect) toward the cooler weld puddle surface ( T ≈ 1800 – 2500 K T \approx 1800\text{--}2500\text{ K} T ≈ 1800 – 2500 K ), the thermodynamic equilibrium shifts back toward diatomic molecules. Recombination occurs directly at the weld pool surface, releasing the dissociation enthalpy: 2 H ⟶ H 2 + 436 kJ/mol 2\text{H} \longrightarrow \text{H}_2 + 436\ \text{kJ/mol} 2 H ⟶ H 2 ​ + 436 kJ/mol This localized heat release broadens the weld puddle, increases joint penetration, and elevates travel speeds compared to pure argon shielding.

Reactive vs. Inert Gas Behavior: Metal Transfer Physics Gas Formulation Shielding Class Metal Transfer Mode in GMAW Bead Profile & Penetration Characteristics

Pure Argon (Ar) Inert Axial Spray (above critical current I_crit) Deep, narrow "finger-like" central root penetration

Ar + 1–5% O₂ Active/Oxidizing Stable Axial Spray (lowers I_crit) Broadened bead base, smooth toe blend, reduced undercut

Ar + 5–18% CO₂ Active/Oxidizing Axial Spray / Pulsed Spray Wide, uniform penetration profile, robust root tie-in

Pure CO₂ Active/Oxidizing Globular or Short-Circuiting only Broad, deep penetration; high spatter; no true axial spray

Ar + 25–75% He Inert Spray / Globular Broad, parabolic "bathtub" penetration; high heat input

When welding carbon or low-alloy steel under pure argon, cathode spots on the workpiece move erratically across oxide films, producing an unstable arc with wandering droplets and poor edge wetting. Adding 1 to 5 % O 2 1\text{ to }5\%\ \text{O}_2 1 to 5% O 2 ​ or 5 to 10 % CO 2 5\text{ to }10\%\ \text{CO}_2 5 to 10% CO 2 ​ forms a thin, stable oxide film on the molten pool surface. This stabilizes cathode emission, reduces the molten metal's surface tension, and lowers the critical transition current ( I crit I_{\text{crit}} I crit ​ ) required for stable axial spray transfer by 20 to 35 A 20\text{ to }35\text{ A} 20 to 35 A .

However, when the CO 2 \text{CO}_2 CO 2 ​ content exceeds ∼ 18 to 20 % \sim 18\text{ to }20\% ∼ 18 to 20% , the electromagnetic pinch effect is disrupted by intense upward vapor pressure from CO \text{CO} CO dissociation at the droplet tip. Axial spray transfer becomes unstable, forcing the system into globular transfer with coarse, irregular droplets and heavy spatter.

4. Sieverts' Law & Diatomic Gas Dissolution Kinetics

When a diatomic gas species ( X 2 X_2 X 2 ​ , such as H 2 \text{H}_2 H 2 ​ or N 2 \text{N}_2 N 2 ​ ) dissolves into a molten metal bath, it does not dissolve as a molecule; it dissociates into individual atoms dissolved in the liquid matrix ( [ X ] [X] [ X ] ): 1 2 X 2 ( g ) ⇌ [ X ] ( liquid metal ) \frac{1}{2} X_2(g) \rightleftharpoons [X]_{(\text{liquid metal})} 2 1 ​ X 2 ​ ( g ) ⇌ [ X ] ( liquid metal ) ​

Applying the law of mass action to this heterogeneous equilibrium: K X = a X ( P X 2 ) 1 / 2 K_X = \frac{a_X}{(P_{X_2})^{1/2}} K X ​ = ( P X 2 ​ ​ ) 1/2 a X ​ ​

Assuming Henry's law applies at low solute concentrations (where activity a X a_X a X ​ is proportional to weight percent [ wt % X ] [\text{wt}\%\ X] [ wt % X ] ): [ wt % X ] = K X ⋅ P X 2 [\text{wt}\%\ X] = K_X \cdot \sqrt{P_{X_2}} [ wt % X ] = K X ​ ⋅ P X 2 ​ ​ ​

This mathematical relationship is Sieverts' Law . It dictates that the equilibrium concentration of a dissolved gas in liquid metal is directly proportional to the square root of its partial pressure , rather than to linear partial pressure. Gas System Equilibrium Constant at 1600°C (wt% · atm^-0.5) Solubility at P = 1.0 atm (1600°C) Primary Weld Defect Risk

  • Hydrogen (H) K_H ≈ 0.0027 (27 ppm) ~27 ppm (liquid iron) Hydrogen-assisted cold cracking (HICC)
  • Nitrogen (N) K_N ≈ 0.0450 (450 ppm) ~450 ppm (liquid iron) Strain aging embrittlement, gross porosity

Oxygen (O) Non-Sieverts (forms stable oxides) ~0.23 wt% (un-deoxidized Fe) Carbon boil CO porosity, oxide inclusions

The Solidification Rejection Mechanism

Dissolution of hydrogen and nitrogen into liquid iron is endothermic ( Δ H solution > 0 \Delta H_{\text{solution}} > 0 Δ H solution ​ > 0 ), meaning equilibrium solubility increases with rising temperature. At 1600 ∘ C 1600^\circ\text{C} 160 0 ∘ C , liquid iron dissolves up to 27 ppm 27\text{ ppm} 27 ppm of hydrogen and 450 ppm 450\text{ ppm} 450 ppm of nitrogen at 1 atm 1\text{ atm} 1 atm .

During solidification and subsequent cooling, gas solubility drops precipitously across phase boundaries: Solubility of Hydrogen in Iron: { Liquid Fe at 1538 ∘ C : ∼ 25 ppm δ -ferrite (BCC) at 1538 ∘ C : ∼ 9 ppm γ -austenite (FCC) at 1400 ∘ C : ∼ 5 ppm α -ferrite (BCC) at 20 ∘ C : < 0.001 ppm \text{Solubility of Hydrogen in Iron:}

  • \begin{cases}
  • \text{Liquid Fe at } 1538^\circ\text{C}: & \sim 25\ \text{ppm} \\[4pt]
  • \delta\text{-ferrite (BCC) at } 1538^\circ\text{C}: & \sim 9\ \text{ppm} \\[4pt]
  • \gamma\text{-austenite (FCC) at } 1400^\circ\text{C}: & \sim 5\ \text{ppm} \\[4pt]
  • \alpha\text{-ferrite (BCC) at } 20^\circ\text{C}: & < 0.001\ \text{ppm}

\end{cases} Solubility of Hydrogen in Iron: ⎩ ⎨ ⎧ ​ Liquid Fe at 153 8 ∘ C : δ -ferrite (BCC) at 153 8 ∘ C : γ -austenite (FCC) at 140 0 ∘ C : α -ferrite (BCC) at 2 0 ∘ C : ​ ∼ 25 ppm ∼ 9 ppm ∼ 5 ppm < 0.001 ppm ​

As the solid-liquid interface advances during weld puddle solidification, partitioning rejects excess gas into the boundary liquid layer ( k 0 = C s / C l < 1 k_0 = C_s / C_l < 1 k 0 ​ = C s ​ / C l ​ < 1 ). If the local dissolved gas concentration exceeds the solubility limit and the combined partial pressures exceed the nucleation threshold ( P gas > P ambient + P ferrostatic + 2 γ / r P_{\text{gas}} > P_{\text{ambient}} + P_{\text{ferrostatic}} + 2\gamma/r P gas ​ > P ambient ​ + P ferrostatic ​ + 2 γ / r ), gas bubbles nucleate and grow, forming wormhole porosity or trapping diffusible hydrogen that can trigger cold cracking.