Study guide
7.2 Inductance, Slope Control & Dynamic Power-Source Response
AWS CWEng Certified Welding Engineer Exam
Track your progress as you read
Finished sections get a check mark.
1 Introduction & CWEng Exam Overview
About the CWEng Exam: Four Parts, 163 Questions & Testing Logistics Scoring, Composite Weighting, Eligibility & Five-Year Renewal How to Use This Guide & Build Your Open-Book Reference Set
2 Chapter 1: Mathematics & Statistics for Welding Engineers
1.1 Engineering Mathematics: Algebra, Trigonometry & Geometry in Weldments 1.2 Differential & Integral Calculus Fundamentals in Engineering Analysis 1.3 Applied Engineering Statistics, Population Distributions & Quality Metrics 1.4 Polynomial Equations, Conic Sections & Complex Numbers
3 Chapter 2: Physics Fundamentals & Mechanics
2.1 Unit Systems, Dimensional Analysis & Engineering Conversions 2.2 Mechanics: Statics, Equilibrium, Force Vectors & Moments 2.3 Work, Energy, Power & Mechanical Advantage in Welding Systems 2.4 Thermal Physics, Linear/Volumetric Expansion & Heat Capacity
4 Chapter 3: General & Physical Chemistry for Welding
3.1 Atomic Structure, Bonding & Solid-Solution Thermodynamics 3.2 Hume-Rothery Compatibility, Interstitial Strain & HSLA Microalloy Scavenging 3.3 Gas Laws, Dalton Partial Pressures, Arc Dissociation & Sieverts Law 3.4 Cylinder Capacity, Available Arc Time & Gas-Related Porosity Diagnosis 3.5 Redox Thermodynamics, Deoxidation & Slag-Metal Refining 3.6 Basicity Index Calculations, Toughness Prediction & Cryogenic Consumable Selection
5 Chapter 4: Strength of Materials & Mechanics of Materials
4.1 Engineering vs. True Stress-Strain, Elastic Constants & Z-Direction Ductility 4.2 Plane Stress vs. Plane Strain, Triaxial Restraint & Alloy Property Comparison 4.3 Beam Bending, Transverse Shear, Torsion & Mohr Circle Construction 4.4 Multiaxial Yield Criteria & Combined-Load Analysis of Welded Members 4.5 Fatigue Life, Weld-Toe Stress Concentration & Paris-Erdogan Crack Growth 4.6 LEFM Fracture Toughness, Ductile-Brittle Transition & Larson-Miller Creep 4.7 Comparative Failure-Mode Synthesis & Integrated Flaw and Creep Assessment
6 Chapter 5: Heat Transfer & Fluid Mechanics in Welding
5.1 Fourier Conduction, Rosenthal Moving Heat Source & 2D vs. 3D Heat Flow 5.2 Adams Cooling Rate, the t8/5 Window & HAZ Peak-Temperature Distribution 5.3 Convection, Stefan-Boltzmann Radiation & Emissivity of Weld Surfaces 5.4 Arc Radiation Losses, Preheat Maintenance & PWHT Boundary Conditions 5.5 Fluid Statics, Bernoulli, Viscosity & Reynolds-Number Regimes 5.6 Gas Lens Mechanics, Buoyancy Effects & Torch Flow Design 5.7 Hyperbaric, Vacuum & Controlled-Atmosphere Welding Environments
7 Chapter 6: Electrical Engineering Principles for Welding Systems
6.1 DC and AC Waveforms, Polarity Thermodynamics & Welding Circuit Analysis 6.2 Joule Heating, Electrode Stickout Preheating & Circuit Voltage Distribution 6.3 Power Factor, Reactance, Impedance & Magnetic Transformer Principles 6.4 Lorentz Force, Electromagnetic Pinch Effect & Arc Blow
8 Chapter 7: Welding Heat Sources & Arc Physics
7.1 Volt-Ampere Characteristics, Operating Point, Self-Regulation & OCV Limits 7.2 Inductance, Slope Control & Dynamic Power-Source Response 7.3 Arc Fall Regions, Cathode Emission Mechanisms & Shielding-Gas Ionization 7.4 Maecker Plasma Jet, Degree of Ionization & Anode Heat Partitioning 7.5 Droplet Force Balance & Classification of Metal Transfer Regimes 7.6 Transition Current, Mode Comparison & Pulsed Waveform Design
9 Chapter 8: Arc Welding Processes & Parameter Controls
8.1 Shielded Metal Arc Welding (SMAW): Electrode Flux Chemistries & Variables 8.2 GMAW Process Physics, Transfer Modes & Shielding Gas Interactions 8.3 Solid, Metal-Cored & Flux-Cored Wires with CTWD and Parameter Envelopes 8.4 Gas Tungsten (GTAW) & Plasma Arc Welding (PAW): Electrodes & Keyholing 8.5 Submerged Arc Welding (SAW): Flux Basicity, Multi-Wire & High-Deposition Systems
10 Chapter 9: Advanced, Resistance & Solid-State Joining Processes
9.1 High-Energy-Density Beam Physics & Electron Beam Welding 9.2 Laser Beam Welding, EBW/LBW Comparison & Fiber Laser Parameter Derivation 9.3 Resistance Welding Physics, Electrode Materials & Spot Weld Sequence 9.4 Nugget Sizing, Seam and Projection Welding, and Lobe Curve Process Windows 9.5 Solid-State Joining: Friction Stir Welding (FSW), Explosion & Diffusion 9.6 Thermal Cutting & Gouging: Oxyfuel, Plasma Arc and Air Carbon Arc 9.7 High-Frequency, Flash, Stud & Ultrasonic Welding; Surfacing and Thermal Spray
11 Chapter 10: Physical & Transformation Metallurgy of Steels
10.1 Fe-Fe3C System, Crystal Lattices, c/a Ratio & Interstitial Solubility 10.2 Critical Temperatures, Invariant Reactions & the Lever Rule 10.3 Alloying Elements, the Gamma Loop & Phase-Fraction Calculations 10.4 TTT and CCT Diagrams, Constitutional Supercooling & Scheil Microsegregation 10.5 Non-Equilibrium Transformation Products & Martensite Modeling 10.6 HAZ Anatomy, Microstructural Sub-Zones & Multi-Pass Reheated Regions 10.7 HAZ Hardness Traverses, Toughness Gradients & Peak-Temperature Control
12 Chapter 11: Weldability, Cracking Mechanisms & Alloy Metallurgy
11.1 Hydrogen Cracking Conditions, Carbon Equivalent & Diffusible Hydrogen Control 11.2 Preheat, Interpass and Post-Heat Calculations for Cold-Crack Prevention 11.3 Solidification Cracking, Bead Aspect Ratio, Liquation & Lamellar Tearing 11.4 Lamellar Tearing Mitigation & Hot-Cracking Susceptibility Evaluation 11.5 Stainless Families, Schaeffler and WRC-1992 Diagrams, Ferrite Number & Sensitization 11.6 Duplex Stainless Metallurgy & Dissimilar-Metal Ferrite Prediction 11.7 Aluminum Oxide and Porosity Control, and Titanium Reactive-Metal Welding 11.8 Nickel Superalloys, Strain-Age Cracking & Guinier-Preston Aging Sequences
13 Chapter 12: Weldment Design, Stress Analysis & Joint Mechanics
12.1 AWS A2.4 Welding Symbol Anatomy, Symbol Library & Dimension Syntax 12.2 Joint Architecture, CJP versus PJP, and NDE Examination Symbols 12.3 Fillet and Groove Weld Sizing under Direct Stress in ASD and LRFD 12.4 Plug and Slot Welds, Stress Gradients & the Fillet Weld Break Test 12.5 Eccentric Loading Analysis: Elastic Vector Method vs Instantaneous Center 12.6 Fatigue Design of Welded Connections & Residual Stress/Distortion Control
14 Chapter 13: Non-Destructive Examination (NDE) & Discontinuity Analysis
13.1 Visual Testing Gages & Liquid Penetrant Capillary Mechanics 13.2 Magnetic Particle Testing: Flux Leakage, Field Geometry & Prod Amperage 13.3 Radiographic Physics, Geometric Unsharpness, Density & IQI Sensitivity 13.4 Computed and Digital Radiography & Radiographic Discontinuity Interpretation 13.5 Acoustic Wave Mechanics, Refraction & Angle-Beam Sound-Path Geometry 13.6 AWS D1.1 Decibel Rating, Phased Array & Time-of-Flight Diffraction
15 Chapter 14: Brazing, Soldering & Industrial Welding Safety
14.1 Brazing Thermodynamics, Capillary Wetting Physics & Joint Clearance 14.2 AWS A5.8 Brazing Filler Metals, FB Fluxes & Industrial Heating Processes 14.3 Soldering Fundamentals, Flux Chemistries & Intermetallic Formation 14.4 Hierarchy of Controls, Electric Shock Physics & Industrial Ventilation 14.5 Fume Exposure Limits, Arc Radiation, Hot Work and Confined-Space Entry 14.6 Arc-Generated Toxic Gases, Moving-Equipment Hazards & TWA Exposure Calculation
16 Chapter 15: Structural Fabrication & AWS D1.1 Code Implementation
15.1 AWS D1.1 Scope, Prequalification Limits, Base-Metal Groups & Matching Filler 15.2 Prequalified Joint Details, Backing Systems & Joint Specification Verification 15.3 Thermal Cut Edges, Fit-Up Tolerances & Minimum Preheat Requirements 15.4 Preheat Application Zones, Measurement Instrumentation & Fabrication Audits 15.5 PWHT Fundamentals, D1.1 Thermal Cycles & Visual Acceptance Criteria 15.6 D1.1 Nondestructive Examination Protocols, PWHT Scheduling & Visual Audit Practice
17 Chapter 16: Welding Procedure Qualification (WPS & PQR) per ASME IX & AWS B2.1
16.1 PQR versus WPS Hierarchy, Qualification Workflow & Standard Procedures 16.2 Manufacturer Responsibility, Subcontracting Limits & Multi-Process Qualification 16.3 Essential, Supplementary Essential and Nonessential Variables with Heat Input Mechanics 16.4 Waveform-Controlled Power Sources, Appendix H & Heat-Input Compliance 16.5 P-Numbers, Group Numbers, F-Numbers & A-Numbers 16.6 QW-451 Mechanical Test Protocols & Procedure Qualification Test Evaluation
18 Chapter 17: Filler Metal Specifications, Selection & Consumable Control
17.1 AWS A5 Architecture: SMAW, GMAW/GTAW and FCAW Consumable Classifications 17.2 SAW Wire-Flux Systems, Alloy Pickup & PWHT Property Effects 17.3 Stainless Filler Specifications, Solidification Modes & Dissimilar-Metal Joints 17.4 AWS A5.10 Aluminum Filler Selection & Dilution and Ferrite-Number Calculations 17.5 Consumable Storage, Conditioning Envelopes & Atmospheric Exposure Limits 17.6 Low-Hydrogen Designators, the Yurioka Parameter & Preheat Sizing
19 Chapter 18: Welder Performance Qualification, Quality Management & Welding Economics
18.1 Welder Qualification Philosophy, Test Positions & Thickness and Diameter Ranges 18.2 F-Number Hierarchy, Operator Qualification & Continuity Requirements 18.3 ISO 3834, Welding Coordination, Inspection Test Plans & Equipment Validation 18.4 EN 10204 Material Certification, Traceability & Heat-Input Nonconformance Auditing 18.5 Weld Cost Anatomy, Deposition Rates, Operating Factor & the Overwelding Law 18.6 Economic Optimization Strategies & Fabrication Cost Comparison
7.2 Inductance, Slope Control & Dynamic Power-Source Response
Key Takeaways Explain This Topic AI
Constant Current (CC / drooper) power sources feature a steep negative slope (-10 to -25 V / 100 A) where manual arc length variations alter voltage significantly while holding current nearly constant, making them essential for SMAW and manual GTAW.
Dynamic inductance (L) governs the transient rate of current rise (di/dt = delta V / L) during short-circuit GMAW, directly controlling droplet necking kinetics, clearing spatter volume, puddle wetting, and arc stability.
Inductance controls the rate of current rise during a short circuit, so it governs droplet necking and spatter without changing the average current setting.
Too little inductance produces violent, spattery short-circuit transfer; too much produces a sluggish arc that struggles to re-establish and leaves cold laps.
Slope and inductance are dynamic controls: they change how the source responds to a disturbance, not where the static operating point sits.
Last updated: September 2026
5. Dynamic Response: Inductance ( L L L ) & Slope Control
While the static V − I V-I V − I curve dictates steady-state equilibrium, the dynamic characteristic defines the instantaneous path the power source follows during millisecond-level transients, such as droplet transfer in short-circuit GMAW. Current (I)
- ^
- I_sc|.............................. Theoretical Steady-State I_sc
- | __--~~
- | __--~~ <-- High Inductance (Soft arc, slow di/dt)
- | __--~~ Tau = L / R is large
- | /
- | / <-- Low Inductance (Crisp arc, fast di/dt)
- | / Violent droplet explosion, harsh spatter
- | / Tau = L / R is small
- 0 +--+--------------------------> Time (t)
- Short-Circuit Contact Established
- The Governing Inductance Differential Equation
When the molten droplet on the advancing wire tip touches the weld puddle, circuit voltage collapses from arc operating voltage ( 20 V 20\text{ V} 20 V ) to the metallic short-circuit drop ( V short ≈ 2 to 4 V V_{\text{short}} \approx 2\text{ to }4\text{ V} V short ≈ 2 to 4 V ). The rate at which current rises is governed by circuit inductance ( L L L ) according to Kirchhoff's voltage equation: V source − V short = I ( t ) ⋅ R + L d i d t V_{\text{source}} - V_{\text{short}} = I(t) \cdot R + L \frac{di}{dt} V source − V short = I ( t ) ⋅ R + L d t d i
Integrating with initial condition I ( 0 ) = I 0 I(0) = I_0 I ( 0 ) = I 0 : ∋ ( t ) = I sc − ( I sc − I 0 ) e − t / τ \ni(t) = I_{\text{sc}} - (I_{\text{sc}} - I_0) e^{-t / \tau} ∋ ( t ) = I sc − ( I sc − I 0 ) e − t / τ
where τ = L / R \tau = L / R τ = L / R is the inductive time constant of the welding loop.
Impact of Inductance Tuning on GMAW-S Performance
Insufficient Inductance (Excessive d i / d t di/dt d i / d t ): Current rises too rapidly ( > 250 , 000 A/s >250,000\text{ A/s} > 250 , 000 A/s ). The molten liquid neck connecting the wire to the puddle is subjected to an instantaneous, explosive magnetic pinch force ( F em ∝ I 2 F_{\text{em}} \propto I^2 F em ∝ I 2 ). The bridge vaporizes violently before surface tension can draw the droplet into the puddle, blasting liquid metal outward as coarse, adherent spatter with a harsh, crackling sound.
Excessive Inductance (Sluggish d i / d t di/dt d i / d t ): Current rises too slowly. The molten bridge remains intact too long, causing the advancing wire to push mechanically against the puddle floor (stubbing). Deposition becomes sluggish, the puddle chills, and cold lap defects occur.
Optimum Inductance: Current rises at a controlled rate ( 50 , 000 to 150 , 000 A/s 50,000\text{ to }150,000\text{ A/s} 50 , 000 to 150 , 000 A/s ). Surface tension draws the droplet smoothly into the molten pool while a gentle pinch force severs the neck. As the arc re-ignites, inductive energy storage maintains arc ionization, producing a smooth, buzzing arc sound with minimal fine spatter and enhanced puddle wetting.
Comprehensive Comparison: Power Source Characteristic Regimes
Engineering Parameter Constant Current (CC) Constant Voltage (CV)
Static Slope ( d V / d I dV/dI d V / d I ) Steep: − 10 to − 25 V / 100 A -10\text{ to }-25\text{ V}/100\text{ A} − 10 to − 25 V /100 A ( − 0.10 to − 0.25 V/A -0.10\text{ to }-0.25\text{ V/A} − 0.10 to − 0.25 V/A ) Flat: − 1.5 to − 3.0 V / 100 A -1.5\text{ to }-3.0\text{ V}/100\text{ A} − 1.5 to − 3.0 V /100 A ( − 0.015 to − 0.030 V/A -0.015\text{ to }-0.030\text{ V/A} − 0.015 to − 0.030 V/A )
- Primary Controlled Variable Current ( I I I , Amperes) set on machine Voltage ( V V V , Volts) set on machine
- Wire Feed Pairing Manual feed or Voltage-Sensing Feeder (VSW) Fixed-Speed (Constant) Wire Feeder
Arc Length Regulation Welder hand manipulation controls arc length Autonomous electrical self-regulation via melt-rate feedback
Processes Used SMAW, GTAW, Carbon Arc Gouging (CAG-A), SAW (large dia) GMAW (solid & metal-cored), FCAW (gas & self-shielded), SAW (small dia)
Short-Circuit Protection Output current intrinsically limited by droop Requires electronic clamping and series choke/inductor
Dynamic Control Feature Arc Force / Dig (% current boost at low voltage) Inductance control ( d i / d t di/dt d i / d t ) & Slope tap adjustment
- 6. Comprehensive Worked Numerical Example: Operating Point & Self-Regulation Dynamics
- Problem Statement
A robotic GMAW cell joins structural steel plate using 1.20 mm 1.20\text{ mm} 1.20 mm AWS A5.18 ER70S-6 wire under 85 % Ar / 15 % CO 2 85\%\text{ Ar} / 15\%\text{ CO}_2 85% Ar /15% CO 2 shielding gas. The power source is a CV inverter with an open-circuit voltage setting of V oc = 36.0 V V_{\text{oc}} = 36.0\text{ V} V oc = 36.0 V and a static output slope s cv = 0.025 V/A s_{\text{cv}} = 0.025\text{ V/A} s cv = 0.025 V/A ( 2.5 V per 100 A 2.5\text{ V per }100\text{ A} 2.5 V per 100 A ).
The arc characteristic for this gas-wire system is modeled by: V arc = 14.0 + 0.020 ⋅ I + 1.50 ⋅ L arc V_{\text{arc}} = 14.0 + 0.020 \cdot I + 1.50 \cdot L_{\text{arc}} V arc = 14.0 + 0.020 ⋅ I + 1.50 ⋅ L arc
where V arc V_{\text{arc}} V arc is in Volts, I I I is in Amperes, and L arc L_{\text{arc}} L arc is physical arc length in millimeters.
The wire melting rate ( M R MR MR , expressed as wire consumption velocity in mm/s \text{mm/s} mm/s ) is described by the Lesnewich relationship: M R = α ⋅ I + β ⋅ L ext ⋅ I 2 MR = \alpha \cdot I + \beta \cdot L_{\text{ext}} \cdot I^2 MR = α ⋅ I + β ⋅ L ext ⋅ I 2
with coefficients α = 0.040 mm/(s ⋅ A) \alpha = 0.040\text{ mm/(s}\cdot\text{A)} α = 0.040 mm/(s ⋅ A) , β = 1.00 × 10 − 4 mm/(s ⋅ mm ⋅ A 2 ) \beta = 1.00 \times 10^{-4}\text{ mm/(s}\cdot\text{mm}\cdot\text{A}^2) β = 1.00 × 1 0 − 4 mm/(s ⋅ mm ⋅ A 2 ) , and electrode extension maintained at L ext = 18.0 mm L_{\text{ext}} = 18.0\text{ mm} L ext = 18.0 mm .
Calculate:
The initial steady-state welding current ( I 1 I_1 I 1 ), arc voltage ( V 1 V_1 V 1 ), and wire feed speed setting ( W F S 1 WFS_1 W F S 1 in m/min \text{m/min} m/min ) when operating at an equilibrium arc length L arc , 1 = 4.00 mm L_{\text{arc},1} = 4.00\text{ mm} L arc , 1 = 4.00 mm .
The instantaneous current ( I 2 I_2 I 2 ) and arc voltage ( V 2 V_2 V 2 ) if seam warpage suddenly increases the arc length to L arc , 2 = 6.00 mm L_{\text{arc},2} = 6.00\text{ mm} L arc , 2 = 6.00 mm before the wire feed speed can mechanically respond.
The new instantaneous wire melting rate ( M R 2 MR_2 M R 2 in mm/s \text{mm/s} mm/s and m/min \text{m/min} m/min ) at this disturbed condition.
The net velocity of arc length restoration ( d L arc / d t dL_{\text{arc}}/dt d L arc / d t ) and the time required for the self-regulating mechanism to restore the arc length to within 10 % 10\% 10% of equilibrium.
Step-by-Step Solution
Step 1: Calculate initial steady-state operating point at L arc , 1 = 4.00 mm L_{\text{arc},1} = 4.00\text{ mm} L arc , 1 = 4.00 mm Substitute L arc = 4.00 mm L_{\text{arc}} = 4.00\text{ mm} L arc = 4.00 mm into the arc characteristic equation: V arc , 1 = 14.0 + 0.020 ⋅ I 1 + 1.50 ( 4.00 ) = 20.00 + 0.020 ⋅ I 1 V_{\text{arc},1} = 14.0 + 0.020 \cdot I_1 + 1.50(4.00) = 20.00 + 0.020 \cdot I_1 V arc , 1 = 14.0 + 0.020 ⋅ I 1 + 1.50 ( 4.00 ) = 20.00 + 0.020 ⋅ I 1
The power source load line is: V source , 1 = 36.00 − 0.025 ⋅ I 1 V_{\text{source},1} = 36.00 - 0.025 \cdot I_1 V source , 1 = 36.00 − 0.025 ⋅ I 1
Equate V source , 1 = V arc , 1 V_{\text{source},1} = V_{\text{arc},1} V source , 1 = V arc , 1 : 36.00 − 0.025 ⋅ I 1 = 20.00 + 0.020 ⋅ I 1 36.00 - 0.025 \cdot I_1 = 20.00 + 0.020 \cdot I_1 36.00 − 0.025 ⋅ I 1 = 20.00 + 0.020 ⋅ I 1 16.00 = 0.045 ⋅ I 1 16.00 = 0.045 \cdot I_1 16.00 = 0.045 ⋅ I 1 I 1 = 16.00 0.045 = 355.56 A I_1 = \frac{16.00}{0.045} = 355.56\text{ A} I 1 = 0.045 16.00 = 355.56 A
Solve for steady-state arc voltage ( V 1 V_1 V 1 ): V 1 = 36.00 − 0.025 ( 355.56 ) = 27.11 V V_1 = 36.00 - 0.025(355.56) = 27.11\text{ V} V 1 = 36.00 − 0.025 ( 355.56 ) = 27.11 V
Compute the wire melting rate ( M R 1 MR_1 M R 1 ): M R 1 = α ⋅ I 1 + β ⋅ L ext ⋅ I 1 2 MR_1 = \alpha \cdot I_1 + \beta \cdot L_{\text{ext}} \cdot I_1^2 M R 1 = α ⋅ I 1 + β ⋅ L ext ⋅ I 1 2 M R 1 = 0.040 ( 355.56 ) + ( 1.00 × 10 − 4 ) ( 18.0 ) ( 355.56 ) 2 MR_1 = 0.040(355.56) + (1.00 \times 10^{-4})(18.0)(355.56)^2 M R 1 = 0.040 ( 355.56 ) + ( 1.00 × 1 0 − 4 ) ( 18.0 ) ( 355.56 ) 2 M R 1 = 14.222 + ( 1.80 × 10 − 3 ) ( 126 , 423 ) = 14.222 + 227.561 = 241.78 mm/s MR_1 = 14.222 + (1.80 \times 10^{-3})(126,423) = 14.222 + 227.561 = 241.78\text{ mm/s} M R 1 = 14.222 + ( 1.80 × 1 0 − 3 ) ( 126 , 423 ) = 14.222 + 227.561 = 241.78 mm/s
Convert to industrial wire feed speed units ( m/min \text{m/min} m/min ): W F S 1 = 241.78 mm/s × 60 s/min 1000 mm/m = 14.51 m/min ( 571 ipm ) WFS_1 = \frac{241.78\text{ mm/s} \times 60\text{ s/min}}{1000\text{ mm/m}} = 14.51\text{ m/min} \quad (571\text{ ipm}) W F S 1 = 1000 mm/m 241.78 mm/s × 60 s/min = 14.51 m/min ( 571 ipm )
Step 2: Calculate instantaneous operating point upon disturbance ( L arc , 2 = 6.00 mm L_{\text{arc},2} = 6.00\text{ mm} L arc , 2 = 6.00 mm ) Substitute the new arc length L arc , 2 = 6.00 mm L_{\text{arc},2} = 6.00\text{ mm} L arc , 2 = 6.00 mm into the arc equation: V arc , 2 = 14.0 + 0.020 ⋅ I 2 + 1.50 ( 6.00 ) = 23.00 + 0.020 ⋅ I 2 V_{\text{arc},2} = 14.0 + 0.020 \cdot I_2 + 1.50(6.00) = 23.00 + 0.020 \cdot I_2 V arc , 2 = 14.0 + 0.020 ⋅ I 2 + 1.50 ( 6.00 ) = 23.00 + 0.020 ⋅ I 2
Equate to the power source load line: 36.00 − 0.025 ⋅ I 2 = 23.00 + 0.020 ⋅ I 2 36.00 - 0.025 \cdot I_2 = 23.00 + 0.020 \cdot I_2 36.00 − 0.025 ⋅ I 2 = 23.00 + 0.020 ⋅ I 2 13.00 = 0.045 ⋅ I 2 13.00 = 0.045 \cdot I_2 13.00 = 0.045 ⋅ I 2 I 2 = 13.00 0.045 = 288.89 A I_2 = \frac{13.00}{0.045} = 288.89\text{ A} I 2 = 0.045 13.00 = 288.89 A
Solve for the disturbed arc voltage ( V 2 V_2 V 2 ): V 2 = 36.00 − 0.025 ( 288.89 ) = 28.78 V V_2 = 36.00 - 0.025(288.89) = 28.78\text{ V} V 2 = 36.00 − 0.025 ( 288.89 ) = 28.78 V
Notice that a mere 2.0 mm 2.0\text{ mm} 2.0 mm increase in arc length causes an instantaneous current drop of: Δ I = 288.89 A − 355.56 A = − 66.67 A \Delta I = 288.89\text{ A} - 355.56\text{ A} = -66.67\text{ A} Δ I = 288.89 A − 355.56 A = − 66.67 A
Step 3: Determine the disturbed wire melting rate ( M R 2 MR_2 M R 2 ) M R 2 = α ⋅ I 2 + β ⋅ L ext ⋅ I 2 2 MR_2 = \alpha \cdot I_2 + \beta \cdot L_{\text{ext}} \cdot I_2^2 M R 2 = α ⋅ I 2 + β ⋅ L ext ⋅ I 2 2 M R 2 = 0.040 ( 288.89 ) + ( 1.80 × 10 − 3 ) ( 288.89 ) 2 MR_2 = 0.040(288.89) + (1.80 \times 10^{-3})(288.89)^2 M R 2 = 0.040 ( 288.89 ) + ( 1.80 × 1 0 − 3 ) ( 288.89 ) 2 M R 2 = 11.556 + ( 1.80 × 10 − 3 ) ( 83 , 457 ) = 11.556 + 150.223 = 161.78 mm/s MR_2 = 11.556 + (1.80 \times 10^{-3})(83,457) = 11.556 + 150.223 = 161.78\text{ mm/s} M R 2 = 11.556 + ( 1.80 × 1 0 − 3 ) ( 83 , 457 ) = 11.556 + 150.223 = 161.78 mm/s M R 2 = 161.78 × 60 1000 = 9.71 m/min MR_2 = \frac{161.78 \times 60}{1000} = 9.71\text{ m/min} M R 2 = 1000 161.78 × 60 = 9.71 m/min
Step 4: Compute recovery rate and dynamic response Because the wire feeder is a mechanical constant-speed system, it continues advancing wire into the joint at W F S = 241.78 mm/s WFS = 241.78\text{ mm/s} W FS = 241.78 mm/s . However, wire is now melting at only M R 2 = 161.78 mm/s MR_2 = 161.78\text{ mm/s} M R 2 = 161.78 mm/s .
The rate of change of physical arc length is: d L arc d t = M R − W F S = 161.78 mm/s − 241.78 mm/s = − 80.00 mm/s \frac{dL_{\text{arc}}}{dt} = MR - WFS = 161.78\text{ mm/s} - 241.78\text{ mm/s} = -80.00\text{ mm/s} d t d L arc = MR − W FS = 161.78 mm/s − 241.78 mm/s = − 80.00 mm/s
The negative sign proves that the arc length is actively collapsing back toward the contact tip.
The initial disturbance was Δ L = 6.00 − 4.00 = 2.00 mm \Delta L = 6.00 - 4.00 = 2.00\text{ mm} Δ L = 6.00 − 4.00 = 2.00 mm .
To close 90 % 90\% 90% of this gap ( 1.80 mm 1.80\text{ mm} 1.80 mm recovery): Δ t 90 % ≈ 1.80 mm 80.00 mm/s = 0.0225 s = 22.5 ms \Delta t_{90\%} \approx \frac{1.80\text{ mm}}{80.00\text{ mm/s}} = 0.0225\text{ s} = 22.5\text{ ms} Δ t 90% ≈ 80.00 mm/s 1.80 mm = 0.0225 s = 22.5 ms
Engineering Conclusion: The electrical self-regulating mechanism begins collapsing the disturbed arc in less than one-fiftieth of a second ( 22.5 ms 22.5\text{ ms} 22.5 ms ). This demonstrates why CV power sources provide unmatched process stability in mechanized and robotic GMAW installations.
- 7. Real-World Engineering Scenarios & Exam Pitfalls
- Industrial Case Study: Retrofitting Heavy Submerged Arc Welding (SAW)
A heavy pressure-vessel manufacturer operated an automated Submerged Arc Welding (SAW) portal running 4.0 mm 4.0\text{ mm} 4.0 mm ( 5 / 32 in 5/32\text{ in} 5/32 in ) wire on thick carbon steel plates. The system utilized an aging 1000 A 1000\text{ A} 1000 A Constant Current (drooper) power source paired with a voltage-sensing wire feeder (VSW). Under high deposition parameters ( 750 A , 34 V 750\text{ A}, 34\text{ V} 750 A , 34 V ), the welding engineer observed cyclic bead hunting, uneven slag coverage, and periodic wire stubbing into the weld pool whenever joint depth varied.
Engineering Diagnosis & Solution: With heavy 4.0 mm 4.0\text{ mm} 4.0 mm wire, the large mechanical inertia of the wire reel and feed motor introduced a 250 ms 250\text{ ms} 250 ms lag into the VSW control loop. When joint depth varied, the mechanical feeder could not accelerate or decelerate quickly enough to maintain arc voltage on the steep CC slope.
The welding engineer replaced the setup with a modern 1000 A 1000\text{ A} 1000 A Constant Voltage (CV) power source paired with a heavy-duty constant-speed wire drive. Under CV control, arc length stabilization shifted from mechanical motor speed adjustments to instantaneous electrical self-regulation ( < 25 ms <25\text{ ms} < 25 ms ). Current variations naturally compensated for stickout shifts, eliminating bead hunting and reducing weld reject rates from 4.8 % 4.8\% 4.8% to 0.1 % 0.1\% 0.1% .
Common CWEng Exam Traps
Exam Trap 1: Confusing Static Slope with Dynamic Inductance Static slope ( d V / d I dV/dI d V / d I ) is measured under steady-state resistive load conditions and dictates equilibrium current/voltage coordinates. Dynamic inductance ( L L L ) controls the rate of change of current ( d i / d t di/dt d i / d t ) during transients (droplet short-circuits). Increasing inductance softens the arc and reduces spatter, but does not change the static slope or steady-state operating point.
Exam Trap 2: The Fallacy of Perfectly Constant Voltage Candidates frequently assume that a "Constant Voltage" power supply delivers identical voltage regardless of current. In reality, all commercial CV supplies have a deliberate downward slope of − 1.5 to − 3.0 V / 100 A -1.5\text{ to }-3.0\text{ V}/100\text{ A} − 1.5 to − 3.0 V /100 A . Without this slight slope, an accidental dead short would draw infinite current and destroy the power semiconductors.
Exam Trap 3: Selecting CC for Small-Diameter GMAW An exam question may present a high-speed sheet-metal GMAW application ( 0.9 mm 0.9\text{ mm} 0.9 mm wire) and ask which power source architecture provides optimal arc stability. Choosing CC is a fatal error: fine wire has minimal thermal mass and melts explosively; pairing CC with small wire causes immediate burnback into the contact tip unless extremely complex external feedback systems are deployed.