Study guide
10.1 Part A (Fundamentals) Exam Strategies
AWS CWI Certified Welding Inspector Exam
Track your progress as you read
Finished sections get a check mark.
1 Introduction to the AWS CWI Certification
What Is the AWS CWI Certification? CWI Exam Structure: Parts A, B, and C Eligibility Requirements and Application
2 1. Welding Processes and Fundamentals
1.1 SMAW — Shielded Metal Arc Welding (Stick) 1.2 GMAW — Gas Metal Arc Welding (MIG/MAG) 1.3 FCAW — Flux-Cored Arc Welding 1.4 GTAW — Gas Tungsten Arc Welding (TIG) 1.5 SAW — Submerged Arc Welding 1.6 Other Welding, Cutting Processes, and Process Variables
3 2. Welding Metallurgy and Heat Control
2.1 The Iron-Carbon Phase Diagram 2.2 The Heat-Affected Zone (HAZ) 2.3 Preheat and Interpass Temperature 2.4 Hydrogen-Induced Cracking (HIC) 2.5 Distortion and Residual Stress
4 3. Weld Discontinuities and Defects
3.1 Discontinuity vs. Defect — Definitions and Concepts 3.2 Cracks — Types, Causes, and Significance 3.3 Porosity and Inclusions 3.4 Incomplete Fusion and Incomplete Joint Penetration 3.5 Geometric Discontinuities: Undercut, Overlap, and Profile
5 4. Nondestructive Examination (NDE) Methods
4.1 Visual Testing (VT) 4.2 Liquid Penetrant Testing (PT) 4.3 Magnetic Particle Testing (MT) 4.4 Radiographic Testing (RT) and Ultrasonic Testing (UT)
6 5. Welding Symbols and Terminology
5.1 Anatomy of a Welding Symbol (AWS A2.4) 5.2 Joint Types, Weld Types, and Welding Positions 5.3 Essential Welding Definitions and Terminology
7 6. WPS, PQR, and Welder Qualification
6.1 Welding Procedure Specification (WPS) 6.2 Procedure Qualification Record (PQR) 6.3 Welder Performance Qualification (WPQ)
8 7. Destructive Testing Methods
7.1 Tensile Testing 7.2 Guided Bend, Nick Break, and Fillet Weld Break Tests 7.3 Impact Testing and Hardness Testing
9 8. Welding Safety and Inspector Duties
8.1 Welding Safety Hazards and Prevention 8.2 CWI Duties and Responsibilities 8.3 Welding-Related Calculations
10 9. AWS D1.1 Code Application (Part C)
9.1 AWS D1.1:2025 Code Structure and Navigation 9.2 Clause 5 — Prequalification Requirements 9.3 Clause 8 — Inspection and Acceptance Criteria 9.4 Part B Practical Exam Preparation
11 10. Exam Strategies and Comprehensive Review
10.1 Part A (Fundamentals) Exam Strategies 10.2 Part C (Code Application) Exam Strategies 10.3 Comprehensive Review — 25 Practice Questions
10.1 Part A (Fundamentals) Exam Strategies
Key Takeaways Explain This Topic AI
Part A is closed book: 150 scored plus 15 unscored pretest questions in 2 hours (~48 seconds each), 72% to pass
You need 108 of 150 correct — you may miss 42 questions and still pass Part A
Highest-yield closed-book recall: definitions/terminology, the five processes, weld symbols, discontinuities, and on-the-job math
Memorize the integrated review tables — processes, discontinuities-to-causes, NDE surface vs volumetric, symbol sides, and the heat-input and carbon-equivalent formulas
Use a last-pass cram: flashcard definitions, draw symbols by hand, and re-derive each formula from memory
- Read all four options; beware absolutes (always/never/only) and old-vs-new term pairs (DCEP=DCRP, DCEN=DCSP)
- Last updated: June 2026
Part A Format and Time Budget
Part A (Fundamentals) is the closed-book pillar of the CWI exam, built to the AWS B5.1 standard for inspector qualification. You answer 150 scored questions plus 15 unscored pretest questions (165 total) in a 2-hour window — roughly 48 seconds per question . No code book, no notes, no reference screens: every answer comes from memory. The passing score is 72% , so you need 108 of 150 correct and may miss 42 and still pass.
- Metric Value
- Scored questions 150
- Pretest (unscored) 15
- Time limit 120 minutes
- Pace per question ~48 seconds
- Pass mark 72% (108/150)
- Margin up to 42 misses
Pacing rule: on the first pass, never burn more than 60 seconds on one item — flag it and move on. Recall is fastest when fresh, so harvest the easy points first, then spend the recovered minutes on flagged items. Leave 5–8 minutes to confirm no question is left blank; there is no wrong-answer penalty, so guess every remaining item.
Where to Spend Closed-Book Study
Part A draws from welding processes, NDE, safety, quality assurance, inspector duties, discontinuities, weld symbols, joint design, mechanical properties, and on-the-job math. The highest-yield closed-book targets are the ones that hinge on exact wording or a memorized number :
Priority Topic Why it pays
High Definitions & A3.0 terminology Questions turn on precise wording — discontinuity vs defect, joint vs weld type
- High Five processes (SMAW/GMAW/FCAW/GTAW/SAW) Power source, polarity, shielding, position limits all tested
- High Weld symbols Arrow-side/other-side must be automatic
- High Discontinuities & causes Match the flaw to its root cause and likely NDE
- Medium NDE method capability Surface vs volumetric; what each detects
- Medium Math (heat input, throat, CE) Plug-and-chug points if formulas are memorized
- Lower Safety, duties, destructive tests Steady, learnable points
High-Yield Integrated Review — Processes and Discontinuities
Use these compact tables as a last-pass cram. First, the five major arc processes — the single most-tested cluster:
- Process Electrode Power/Polarity Shielding Position
- SMAW Consumable, coated stick CC, usually DCEP Flux coating gases/slag All
- GMAW Consumable solid wire CV, DCEP External gas (Ar/CO₂) All (spray = flat/horiz)
- FCAW Consumable tubular wire CV, DCEP Flux core (-S) or gas (-G) All
- GTAW Non-consumable tungsten CC; DCEN steel, AC aluminum External inert gas (Ar) All
- SAW Consumable wire under flux CC or CV Granular flux blanket Flat/horizontal only
Next, the discontinuity-to-cause map — the exam loves "what caused this?" items:
- Discontinuity Typical cause
- Porosity Contamination, lost shielding gas, moisture/dirty base metal
- Undercut Excess current, long arc, fast travel, wrong angle
- Overlap (cold lap) Slow travel, low current — metal rolls over unfused base metal
- Incomplete fusion Low heat, poor technique, dirty surfaces
- Incomplete joint penetration Insufficient heat/joint design, large root face, small root opening
- Slag inclusion Poor interpass cleaning (SMAW/FCAW/SAW)
- Cracks (hot/cold) Restraint, hydrogen + martensite + stress (cold/HIC)
Trap: A crack is rejectable regardless of size or location under D1.1; overlap, IF, and ICP are linear discontinuities that usually fail too. Porosity and slag are rounded/volumetric and judged against size limits.
High-Yield Review — NDE, Symbols, and Formulas
NDE surface vs volumetric is a guaranteed cluster. Memorize what each method finds:
- Method Detects Limited to
- VT (visual) Surface profile, undercut, overlap, undersize Surface only; 50 fc min light per AWS B1.11
- PT (penetrant) Surface-breaking flaws Any nonporous material; surface only
- MT (magnetic particle) Surface + slightly subsurface Ferromagnetic only
- RT (radiography) Volumetric — porosity, slag Poor for tight planar cracks
- UT (ultrasonic) Subsurface planar — cracks, LOF Needs skilled operator; geometry sensitive
Memory hook: PT/MT = surface; RT/UT = subsurface; RT favors volumetric, UT favors planar.
Weld symbol sides (arrow vs other):
- Symbol position on reference line Meaning
- Below the reference line Arrow side ("below = by the arrow")
- Above the reference line Other side
- Both above and below Both sides
- Field weld flag Welded in the field, not the shop
The two formulas you must reproduce cold:
Heat input: HI (kJ/in) = (Volts × Amps × 60) ÷ (Travel speed in/min × 1000) . Example: 24 V × 180 A × 60 ÷ (8 × 1000) = 32.4 kJ/in .
Carbon equivalent (IIW): CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 . Higher CE → greater hardenability → more martensite risk → more preheat to avoid hydrogen-induced cracking (HIC) . HIC needs all three : susceptible (martensitic) microstructure, diffusible hydrogen, and tensile stress — remove any one to prevent it.
D1.1 acceptance values to remember: cracks prohibited; undercut depth limit generally 1/16 in (1.6 mm) with tighter limits on cyclically loaded members; fillet weld profiles must avoid excessive convexity/concavity; craters must be filled to full cross-section.
- Part A Readiness Checklist (Last Cram Pass)
- Recite each of the five processes' power source, polarity, shielding, and position limits without notes
- Map every common discontinuity to its cause and the NDE method that finds it
- State which NDE methods are surface-only and which find subsurface/volumetric flaws
- Place a weld symbol on the correct side from memory (below = arrow side)
- Write and solve heat input and carbon equivalent from a blank page
- List the three HIC conditions and one way to break each
- Confirm pace: stop at 60 s/question, flag, return, guess every blank at the end
Trap-avoidance: read all four options; distrust always/never/only ; watch unit swaps (ksi vs psi, °F vs °C, in vs mm); and know old-vs-new term pairs — DCEP = DCRP , DCEN = DCSP .