Study guide
1.1 SMAW — Shielded Metal Arc Welding (Stick)
AWS CWI Certified Welding Inspector Exam
Track your progress as you read
Finished sections get a check mark.
1 Introduction to the AWS CWI Certification
What Is the AWS CWI Certification? CWI Exam Structure: Parts A, B, and C Eligibility Requirements and Application
2 1. Welding Processes and Fundamentals
1.1 SMAW — Shielded Metal Arc Welding (Stick) 1.2 GMAW — Gas Metal Arc Welding (MIG/MAG) 1.3 FCAW — Flux-Cored Arc Welding 1.4 GTAW — Gas Tungsten Arc Welding (TIG) 1.5 SAW — Submerged Arc Welding 1.6 Other Welding, Cutting Processes, and Process Variables
3 2. Welding Metallurgy and Heat Control
2.1 The Iron-Carbon Phase Diagram 2.2 The Heat-Affected Zone (HAZ) 2.3 Preheat and Interpass Temperature 2.4 Hydrogen-Induced Cracking (HIC) 2.5 Distortion and Residual Stress
4 3. Weld Discontinuities and Defects
3.1 Discontinuity vs. Defect — Definitions and Concepts 3.2 Cracks — Types, Causes, and Significance 3.3 Porosity and Inclusions 3.4 Incomplete Fusion and Incomplete Joint Penetration 3.5 Geometric Discontinuities: Undercut, Overlap, and Profile
5 4. Nondestructive Examination (NDE) Methods
4.1 Visual Testing (VT) 4.2 Liquid Penetrant Testing (PT) 4.3 Magnetic Particle Testing (MT) 4.4 Radiographic Testing (RT) and Ultrasonic Testing (UT)
6 5. Welding Symbols and Terminology
5.1 Anatomy of a Welding Symbol (AWS A2.4) 5.2 Joint Types, Weld Types, and Welding Positions 5.3 Essential Welding Definitions and Terminology
7 6. WPS, PQR, and Welder Qualification
6.1 Welding Procedure Specification (WPS) 6.2 Procedure Qualification Record (PQR) 6.3 Welder Performance Qualification (WPQ)
8 7. Destructive Testing Methods
7.1 Tensile Testing 7.2 Guided Bend, Nick Break, and Fillet Weld Break Tests 7.3 Impact Testing and Hardness Testing
9 8. Welding Safety and Inspector Duties
8.1 Welding Safety Hazards and Prevention 8.2 CWI Duties and Responsibilities 8.3 Welding-Related Calculations
10 9. AWS D1.1 Code Application (Part C)
9.1 AWS D1.1:2025 Code Structure and Navigation 9.2 Clause 5 — Prequalification Requirements 9.3 Clause 8 — Inspection and Acceptance Criteria 9.4 Part B Practical Exam Preparation
11 10. Exam Strategies and Comprehensive Review
10.1 Part A (Fundamentals) Exam Strategies 10.2 Part C (Code Application) Exam Strategies 10.3 Comprehensive Review — 25 Practice Questions
1.1 SMAW — Shielded Metal Arc Welding (Stick)
Key Takeaways Explain This Topic AI
SMAW uses a consumable flux-coated electrode that supplies shielding gas, slag, deoxidizers, and alloying elements
SMAW requires a constant-current (CC) power source; polarity (DCEP/DCEN/AC) shifts penetration and deposition
E7018 is the low-hydrogen, all-position structural workhorse (AC or DCEP)
Low-hydrogen electrodes hold at 250–300°F and rebake at 500–800°F after exceeding atmospheric exposure limits
- Heat input = (V × A × 60) / travel speed; SMAW deposition efficiency is only 60–65%
- Last updated: June 2026
Shielded Metal Arc Welding (SMAW)
Shielded Metal Arc Welding (SMAW) — called stick welding in the field — is one of the oldest and most versatile arc processes and the one a CWI encounters most often in maintenance, repair, and field erection. Its appeal is portability: a power source, two leads, and a box of electrodes are all that is required, and the self-generated shielding tolerates moderate wind that would defeat a gas-shielded process.
SMAW uses a consumable electrode consisting of a solid core wire surrounded by a baked-on flux coating . The arc is struck between the electrode tip and the base metal, producing temperatures near 6,000–10,000°F (3,300–5,500°C) that melt both the core wire and a portion of the base metal. As the electrode burns, the coating performs four jobs the inspector must understand:
- Decomposes into a shielding gas that displaces atmospheric oxygen, nitrogen, and hydrogen from the molten pool
- Forms a slag that floats over the solidifying bead, slowing cooling and protecting it from the air
- Adds deoxidizers and alloying elements (Mn, Si, Ni, Mo) per the electrode classification
- Stabilizes the arc through ionizing salts (potassium, sodium) and provides cellulose or iron powder
- Power Source and Polarity
SMAW requires a constant-current (CC) , also called drooping, power source. Because the welder manually controls arc length, CC output keeps amperage nearly steady even as the arc lengthens or shortens, so the bead and penetration stay consistent. Polarity is a frequent exam point:
- Polarity Abbreviation Heat Distribution Effect
- DCEP (reverse) Electrode positive ~2/3 heat at electrode Deeper penetration; E7018, E6010
- DCEN (straight) Electrode negative ~2/3 heat at work Higher deposition, shallower; E6013, E7024
- AC Alternating Balanced Reduces arc blow; needs AC-rated coating
Electrode Classification (AWS A5.1 / A5.5)
The carbon-steel electrode classification (AWS A5.1) packs the electrode's mechanical and operating data into the digits after the letter E. Memorizing the decode is essential for Part A.
Example: E7018
- Character Meaning
- E Electrode
- 70 Minimum tensile strength, 70 ksi (70,000 psi)
- 1 Positions (1 = all positions; 2 = flat & horizontal; 4 = also vertical-down)
- 8 Coating + current type (8 = low-hydrogen iron powder, AC or DCEP)
- Electrode Coating Current Positions Notes
- E6010 Cellulosic DCEP All Deep penetration, fast-freeze, pipe root passes
- E6011 Cellulosic AC/DCEP All 6010 that runs on AC; versatile farm/field rod
- E6013 Rutile AC/DC All Soft arc, shallow penetration, sheet metal
- E7018 Low-H iron powder AC/DCEP All The structural workhorse; low-hydrogen
- E7024 Iron powder rutile AC/DC Flat/Horiz Drag rod, very high deposition
- E7028 Low-H iron powder AC/DCEP Flat/Horiz Low-H but flat/horizontal high-deposition
- Low-Hydrogen Electrodes and Storage
Low-hydrogen electrodes (E7015 DC-only, E7016 AC/DC, E7018, E7028) minimize diffusible hydrogen , the driver of hydrogen-induced (cold/underbead) cracking in hardenable and restrained steels. Because the coating absorbs atmospheric moisture, codes mandate strict handling, and AWS D1.1 Table 5.x is heavily tested:
Store unopened rods, then hold in a rod oven at 250–300°F (120–150°C) .
Atmospheric exposure is limited (commonly 4 hours for E70 series); beyond the limit the electrode must be reconditioned/rebaked at 500–800°F (260–425°C) for 1–2 hours.
Coatings that get wet are scrapped, not dried — moisture chemically bonds.
Exam trap: 250–300°F is the holding temperature; 500–800°F is the rebake temperature. Mixing the two is a classic wrong answer.
Heat Input and Diagnostics
SMAW deposition efficiency is only 60–65% because of stub loss (~2"), spatter, and slag. Travel speed and amperage set bead size; too-fast travel narrows the bead and can cause undercut, while too-slow travel piles up metal and risks slag inclusions. A worked heat-input example for SMAW: at 140 A, 24 V, 6 ipm , heat input = (24 × 140 × 60) / 6 = 33,600 J/in (33.6 kJ/in) — within typical structural limits.
The inspector should also understand the welder-controlled variables that the WPS pins down for SMAW: electrode size and amperage , arc length (kept roughly equal to the electrode core diameter; a long arc loses shielding and causes porosity and spatter), travel angle (drag versus push), and work angle in fillets. 1 prohibit. Restarts at the end of each electrode are also inspection points, since a cold restart can trap slag or leave incomplete fusion.
Finally, SMAW is prone to arc blow — magnetic deflection of the arc on DC, especially near the work-lead connection or at plate edges — which AC current or repositioning the ground helps control.
- Advantages Limitations
- Portable, low equipment cost Low deposition rate
- Self-shielded, tolerates wind Frequent rod changes (stub loss)
- All positions, most ferrous metals Slag removal each pass
- Excellent for repair/field Operator-skill dependent