Study guide

6.2 Procedure Qualification Record (PQR)

AWS CWI Certified Welding Inspector Exam

Track your progress as you read

Finished sections get a check mark.

1 Introduction to the AWS CWI Certification

What Is the AWS CWI Certification? CWI Exam Structure: Parts A, B, and C Eligibility Requirements and Application

2 1. Welding Processes and Fundamentals

1.1 SMAW — Shielded Metal Arc Welding (Stick) 1.2 GMAW — Gas Metal Arc Welding (MIG/MAG) 1.3 FCAW — Flux-Cored Arc Welding 1.4 GTAW — Gas Tungsten Arc Welding (TIG) 1.5 SAW — Submerged Arc Welding 1.6 Other Welding, Cutting Processes, and Process Variables

3 2. Welding Metallurgy and Heat Control

2.1 The Iron-Carbon Phase Diagram 2.2 The Heat-Affected Zone (HAZ) 2.3 Preheat and Interpass Temperature 2.4 Hydrogen-Induced Cracking (HIC) 2.5 Distortion and Residual Stress

4 3. Weld Discontinuities and Defects

3.1 Discontinuity vs. Defect — Definitions and Concepts 3.2 Cracks — Types, Causes, and Significance 3.3 Porosity and Inclusions 3.4 Incomplete Fusion and Incomplete Joint Penetration 3.5 Geometric Discontinuities: Undercut, Overlap, and Profile

5 4. Nondestructive Examination (NDE) Methods

4.1 Visual Testing (VT) 4.2 Liquid Penetrant Testing (PT) 4.3 Magnetic Particle Testing (MT) 4.4 Radiographic Testing (RT) and Ultrasonic Testing (UT)

6 5. Welding Symbols and Terminology

5.1 Anatomy of a Welding Symbol (AWS A2.4) 5.2 Joint Types, Weld Types, and Welding Positions 5.3 Essential Welding Definitions and Terminology

7 6. WPS, PQR, and Welder Qualification

6.1 Welding Procedure Specification (WPS) 6.2 Procedure Qualification Record (PQR) 6.3 Welder Performance Qualification (WPQ)

8 7. Destructive Testing Methods

7.1 Tensile Testing 7.2 Guided Bend, Nick Break, and Fillet Weld Break Tests 7.3 Impact Testing and Hardness Testing

9 8. Welding Safety and Inspector Duties

8.1 Welding Safety Hazards and Prevention 8.2 CWI Duties and Responsibilities 8.3 Welding-Related Calculations

10 9. AWS D1.1 Code Application (Part C)

9.1 AWS D1.1:2025 Code Structure and Navigation 9.2 Clause 5 — Prequalification Requirements 9.3 Clause 8 — Inspection and Acceptance Criteria 9.4 Part B Practical Exam Preparation

11 10. Exam Strategies and Comprehensive Review

10.1 Part A (Fundamentals) Exam Strategies 10.2 Part C (Code Application) Exam Strategies 10.3 Comprehensive Review — 25 Practice Questions

6.2 Procedure Qualification Record (PQR)

Key Takeaways Explain This Topic AI

A PQR records the ACTUAL single values welded on a test coupon plus the mechanical test results — it is the objective evidence that qualifies a WPS

Required D1.1 groove tests: transverse tensile (≥ base-metal min) and guided bend (no open discontinuity > 1/8 in / 3 mm), plus CVN if specified

Table 6.2: a coupon ≥ 1 in (25 mm) qualifies unlimited production thickness; a thinner coupon qualifies 1/8 in to 2T

Essential change → new PQR; supplementary essential → new PQR only if CVN testing required; nonessential → revise WPS only

The CWI confirms each qualified-by-test WPS is backed by a valid PQR and that production thickness is within the PQR's qualified range

Last updated: June 2026

What a PQR Is

A Procedure Qualification Record (PQR) is the document that records the actual welding variables used to weld a test coupon and the results of the mechanical tests performed on that coupon. Where the WPS is the recipe written for the future, the PQR is the objective evidence — generated in the past — that proves the recipe works. AWS A3.0 frames it as the record demonstrating that a weldment made by a given procedure meets the prescribed mechanical-property requirements. One PQR (or several together) supports one or more WPSs.

The critical relationship: the PQR qualifies the WPS. A qualified-by-test WPS cannot exist without a PQR behind it. The PQR captures single actual values (e.g., the welder ran exactly 165 A at 24 V, 8 in/min, 250°F preheat), and the WPS then publishes ranges around those proven values.

What the PQR Records

  • Information Detail Captured
  • Actual variables Exact amperage, voltage, travel speed, preheat, interpass — single values, not ranges
  • Base metal Actual specification, grade, group/P-number, coupon thickness
  • Filler metal Actual AWS classification, F-number, A-number, diameter
  • Mechanical test results Tensile, guided bend, CVN impact (if required), hardness (if required)
  • Witnessing/lab Testing laboratory, technician, and the responsible signatory
  • Required Mechanical Tests (AWS D1.1, CJP Groove)
  • Test What It Proves Acceptance / Count
  • Transverse tensile (×2) Joint strength Must equal or exceed the minimum specified tensile of the base metal

Root and face guided bend Soundness (for thinner coupons) No open discontinuity > 1/8 in (3 mm) in any direction on the convex surface

  • Side bend (×4) Soundness through full thickness Used for thicker coupons; same 1/8 in limit
  • CVN impact (if specified) Notch toughness Per contract — driven by supplementary essential variables

The headline acceptance number to memorize: no open discontinuity exceeding 1/8 in (3 mm) in any dimension on the bent convex face. Small base-metal-origin defects are evaluated separately.

Reading Each Test

Transverse tensile pulls a machined cross-weld specimen to failure. The recorded ultimate tensile strength must meet or exceed the minimum specified tensile of the weaker base metal . Failure in the base metal at or above that value is acceptable.

Guided bend wraps a specimen around a mandrel (typically to 180°). Root bends stretch the root side, face bends stretch the face side, and side bends stretch the full thickness — side bends are mandatory for thicker coupons because they reveal mid-thickness lack of fusion that surface bends miss.

CVN (Charpy V-notch) impact is a toughness test run only when the contract invokes it, and is governed by the supplementary essential variables.

Thickness Range a PQR Qualifies (Table 6.2)

A single PQR does not qualify only the exact coupon thickness — it qualifies a range , so one test can cover many production thicknesses.

  • Test Coupon Thickness (T) Production Thickness Qualified
  • 1/8 in (3 mm) ≤ T < 1 in (25 mm) 1/8 in (3 mm) minimum to 2T maximum
  • T ≥ 1 in (25 mm) 1/8 in (3 mm) minimum to unlimited

Thus a 1 in coupon qualifies unlimited production thickness — the single most exam-tested PQR number. Square-groove welds qualified without backgouging are limited to the test thickness.

Essential vs. Nonessential vs. Supplementary Essential

Whether a WPS change forces a new PQR depends on how the changed variable is classified:

  • Class Effect Change Beyond Range Means
  • Essential Affects mechanical properties (tensile/bend) Requalify — new PQR required
  • Supplementary essential Affects notch toughness New PQR only when CVN impact testing is required
  • Nonessential No significant property effect Revise the WPS only — no requalification
  • Examples of Each Class

Class Representative Variables (AWS D1.1)

Essential Change of process; change of F-number group; deleting or adding PWHT; increase in thickness beyond the qualified range; change of shielding/flux; decrease in preheat below qualified minimum

Supplementary essential Increase in heat input or large change in interpass temperature; uphill ↔ downhill progression; a change affecting cooling rate — all relevant only when CVN is required

Nonessential Minor groove-angle or root-opening change; electrode diameter within range; travel-speed tweak; number of passes; cleaning method

The distinction is exactly why the WPS and PQR are paired documents: the PQR proves the procedure at specific values, and the essential-variable rules define how far the WPS may stray from those proven values before a fresh PQR is mandatory.

The CWI's Role with the PQR

The CWI verifies that each qualified-by-test WPS is actually backed by a valid PQR , that the PQR's recorded variables logically support the WPS ranges, that the required tests were run and passed, and that the production thickness falls within the PQR's qualified range. A WPS calling for a 1-1/2 in production weld supported only by a 1/2 in coupon PQR (max 1 in) is out of range — a finding the CWI must raise.

Exam trap: Adding or deleting PWHT , or a change in welding process , is an essential change (new PQR). A change that only affects toughness (e.g., a small heat-input increase) is supplementary essential — it only forces requalification if the job specifies CVN testing.