Study guide
5.3 Non-Metallic Structures: Composites, Wood, Fabric, and Plastics
FAA A&P Study Guide Exam
Track your progress as you read
Finished sections get a check mark.
1 Orientation: Eligibility, FTN, Authorization, Three-Test Path, and Retakes
1.1 Certificate Ratings and the Three-Test Roadmap 1.2 Baseline Eligibility and the Experience Path 1.3 AMTS and Military Eligibility Pathways 1.4 FTN, IACRA, and the Authorization File 1.5 Knowledge-Test Logistics and Scoring 1.6 AKTRs, Retakes, and the DME Transition
2 ACS Map, Testing Matrix, Embedded Images, Supplements, and Study Workflow
2.1 Testing Matrix Facts for AMG, AMA, and AMP 2.2 ACS Map and Subject-Area Boundaries 2.3 AKTR ACS-Code Diagnostics 2.4 Testing Supplement and Embedded Images 2.5 Three-Test Study Workflow 2.6 Final Review and Test-Day Source Control
3 General I: Electricity, Drawings, Weight and Balance, Math, and Physics
3.1 Electricity and Electronics Foundations 3.2 AC/DC Measurement and Schematic Troubleshooting 3.3 Aircraft Drawings, Blueprints, and Schematics 3.4 Weight and Balance Equations and Records 3.5 Maintenance Math and Unit Discipline 3.6 Physics for Aviation: Forces, Fluids, and Flight
4 General II: Lines, Materials, Servicing, Corrosion, Records, Inspection, and Human Factors
4.1 Fluid Lines, Fittings, and Installation Risk 4.2 Materials, Hardware, and Process Control 4.3 Ground Operations, Servicing, and Ramp Safety 4.4 Cleaning, Corrosion Control, and Finishing 4.5 Regulations, Forms, Records, and Publications 4.6 Inspection Concepts, Human Factors, and Maintenance Judgment
5 Airframe I: Structures, Flight Controls, and Airframe Inspection
5.1 Metallic Structure Inspection and Damage Patterns 5.2 Sheet-Metal Repairs, Fasteners, and Riveting Judgment 5.3 Non-Metallic Structures: Composites, Wood, Fabric, and Plastics 5.4 Flight Control Systems, Rigging, and Travel 5.5 Control Surface Balance, Flutter, and Freeplay 5.6 Airframe Inspection, Records, ADs, and Corrosion Decisions
6 Airframe II: Landing Gear, Hydraulics, Pneumatics, Environmental, Instruments, and Comms
6.1 Landing Gear, Wheels, Tires, and Brakes 6.2 Retraction, Steering, Anti-Skid, and Warning Systems 6.3 Hydraulic Systems: Components, Fluids, and Troubleshooting 6.4 Pneumatic, Vacuum, and Bleed-Air Systems 6.5 Environmental Systems: Pressurization, Heating, Cooling, and Oxygen 6.6 Instrument Systems: Pitot-Static, Gyros, and Displays 6.7 Communication, Navigation, Antennas, and Avionics Inspection
7 Airframe III: Fuel, Electrical, Ice/Rain, Fire, Rotorcraft, and Water/Waste Systems
7.1 Airframe Fuel System Boundaries and Safe Servicing 7.2 Airframe Electrical Power, Wiring, and Protection 7.3 Ice and Rain Control System Inspection and Limits 7.4 Airframe Fire Protection Detection, Extinguishing, and Squib Safety 7.5 Rotorcraft Fundamentals, Controls, Drives, and Vibration 7.6 Water and Waste Systems Service Boundaries and Contamination Control
8 Powerplant I: Reciprocating, Turbine Engine Theory, and Engine Inspection
8.1 Reciprocating Engine Cycles, Components, and Operating Boundaries 8.2 Horizontally Opposed and Radial Engine Components 8.3 Reciprocating Engine Performance, Ground Operation, and Preservation 8.4 Turbine Engine Airflow, Sections, and Performance 8.5 Turbine Engine Maintenance, FOD, Bleed Air, and Post-Installation Checks 8.6 Engine Inspection, Records, Compression, Borescope, and Airworthiness
9 Powerplant II: Instruments, Fire, Electrical, Lubrication, Ignition, and Starting
9.1 Engine Instrument Scan and Trend Logic 9.2 Pressure, Temperature, and Flow Indications 9.3 Engine Fire Protection, Detection, and Extinguishing 9.4 Engine Electrical Generation and Protection 9.5 Lubrication System Flow, Pressure, and Contamination 9.6 Ignition and Starting Troubleshooting
10 Powerplant III: Fuel Metering, Induction, Cooling, Turbine Air, Exhaust, Reversers, and Propellers
10.1 Engine Fuel System Flow, Contamination, and Vapor 10.2 Carburetors, Fuel Injection, and Metering Logic 10.3 Reciprocating Induction, Turbocharging, and Cooling 10.4 Turbine Air Systems, Bleed Air, and Anti-Ice 10.5 Exhaust Systems, Thrust Reversers, and Temperature Patterns 10.6 Propeller Systems, Governors, and Inspection
11 Oral/Practical Bridge: AKTR ACS Codes, DME Expectations, and Maintenance Judgment
11.1 Turn AKTR ACS Codes Into an Oral and Practical Remediation Plan 11.2 What the DME Oral Exam Is Really Testing 11.3 Practical Projects, Tools, Equipment, and Safety Discipline 11.4 Risk Management and Human Factors in the DME Environment 11.5 Documentation, Maintenance Records, and Data Discipline 11.6 Return-to-Service Judgment and Final DME Readiness
12 Final Review: Test Day Strategy, Three-Test Schedule, and Next Steps
12.1 Build the Final Study Calendar Around AMG, AMA, and AMP 12.2 PSI Test-Day Checklist Without Guesswork 12.3 Pacing for the 60-Question and 100-Question Knowledge Tests 12.4 Formula, Supplement, and Embedded-Image Final Review 12.5 Retake Decision Tree After a Failed or Weak Knowledge Test 12.6 DME Scheduling and Post-Pass Next Steps
5.3 Non-Metallic Structures: Composites, Wood, Fabric, and Plastics
Key Takeaways Explain This Topic AI
A composite is a fiber reinforcement (fiberglass, aramid/Kevlar, carbon/graphite, boron) held in a matrix (usually epoxy resin); the fiber carries load and ply orientation determines strength direction.
Honeycomb sandwich panels are light and stiff but vulnerable to hidden core damage and water intrusion, which destroys the skin-to-core bond.
The coin (tap) test finds disbonds and delaminations by a change in ring; a dull thud means trapped damage that needs further inspection.
Composite repair quality depends on approved materials, correct resin shelf life and mix ratio, ply orientation and overlap, surface prep, and controlled cure temperature and pressure.
Wood and fabric are legacy but still tested — wood is judged for decay, glue-joint integrity, and grain; fabric is tested for strength (punch tester) and condemned below 70% of required new strength.
Last updated: June 2026
Composite Construction: Fiber + Matrix
A composite combines a fiber reinforcement that carries the load with a matrix (resin) that bonds the fibers, transfers load between them, and holds the shape. The fibers do the work, so ply orientation matters — strength runs along the fibers, and a repair must duplicate the original number of plies and their orientation. Common reinforcements:
- Fiber Color/cue Property
- Fiberglass White Cheap, good for radomes (radio-transparent), lower strength
- Aramid (Kevlar) Yellow/gold Tough, impact/fatigue resistant; hard to cut/drill; absorbs water
- Carbon/graphite Black Very high strength/stiffness; conductive — galvanic corrosion risk against aluminum
- Boron — Very stiff, military; hazardous to machine
The usual matrix is epoxy resin (sometimes polyester or phenolic; high-temp areas use thermoplastics like PEEK). Resins are temperature- and humidity-sensitive: a prepreg (pre-impregnated cloth) has a freezer shelf life and out-time that must be tracked, and wet lay-up resin must be mixed at the exact ratio or it will not cure to strength.
Honeycomb Sandwich and Hidden Damage
Many control surfaces, floors, and panels are honeycomb sandwich : two thin face skins bonded to a lightweight core (aluminum, Nomex/aramid, or foam). This gives huge stiffness for the weight, but it creates the biggest inspection trap in composites — damage can be invisible from the surface . An impact may leave a barely visible dent while the core is crushed and the skin is delaminated or disbonded underneath. Water intrusion into the core is especially serious: it adds weight, breaks the skin-to-core bond, and freezes/expands at altitude.
Inspection methods escalate with suspicion:
Visual — look for dents, blisters, resin starvation, paint cracks, fluid stains.
Coin (tap) test — tap with a light coin or tap hammer; a sharp ring = sound bond, a dull thud = disbond/delamination/water. Good for thin-skin areas only.
Ultrasonic / thermography / radiography — map subsurface damage and trapped water when the tap test or impact history warrants it.
After any impact, overheat, or lightning strike, the technician must treat the area as suspect until NDI clears it — appearance is not enough.
Composite Repair Discipline and Plastics/Windows
A structural composite repair restores the load path by replacing lost plies. Key controls:
Remove damage to sound material (scarf or stepped taper, typically a wide taper ratio so load feeds gradually into the repair).
Surface prep — clean, dry, abrade; carbon needs care to avoid galvanic issues at metal interfaces.
Ply layup — match fiber type, ply count, and orientation ; stagger ply edges; respect overlap.
Cure — control temperature, time, and pressure (vacuum bag/heat blanket or autoclave) per the data; under-cure means low strength, over-temp damages resin.
Post-repair — inspect (tap/NDI), and rebalance control surfaces if weight changed.
Transparent plastics (windshields, windows) are usually acrylic (Plexiglas) or stretched acrylic/polycarbonate . Inspect for crazing (fine surface cracks), scratches, and crack growth; stop-drill crack tips only per data; clean with approved cleaners and a clean cloth (never dry-wipe or use solvents that craze acrylic). Wear and chemical/dust hazards matter: composite dust and resins are respiratory and skin irritants, so use PPE and dust control. Reject any unapproved repair system — a strong-looking patch built with the wrong resin or cure is not airworthy.
Wood and Fabric (Legacy)
Legacy structures still appear on the test. Wood structure (spars, ribs) is inspected for decay/dry rot, compression failures across the grain, glue-joint separation, splits, and moisture . Approved aircraft woods (e.g., Sitka spruce and substitutes) must meet grain-slope and defect limits; glue joints must be tight and the right adhesive. Probe suspect soft spots; a screwdriver that sinks into a spar signals rot.
Fabric covering (cotton, linen, or modern polyester such as Ceconite/Dacron) is judged mainly by strength :
Tested with a punch tester (or pull test) at suspect, sun-exposed areas.
Fabric is unairworthy when it falls below 70% of the strength required for a new covering of that aircraft (for example, on an aircraft requiring ~56 lb/in new fabric, 70% ≈ 46 lb/in is the floor — verify against the actual approved value).
Inspect for deteriorated finish (dope/UV protection), tears, loose rib lacing, and ringworm/ringwork separation .
The common thread across all non-metallic materials: the material dictates the method , hidden damage is the real danger, and only approved materials and procedures return the part to service.
Resin Handling, Cure Control, and Common Traps
Resin chemistry quietly drives several exam questions. Two-part epoxy must be mixed at the manufacturer's exact ratio by weight or volume; too much or too little hardener yields a soft, weak, or brittle cure that looks fine but has low strength. Prepreg materials are stored frozen and have a tracked shelf life and out-time (the cumulative time at room temperature); exceeding either means the resin may not fully cure, so the material is scrapped.
During cure the temperature, ramp rate, dwell time, and pressure all matter — a vacuum bag with a heat blanket and thermocouples is common in the field, and under-curing (too cool or too short) gives low strength while over-temperature degrades the matrix . The technician verifies the cure (often a separate witness coupon) before declaring the repair sound.
A few traps recur. Carbon fiber is electrically conductive , so a carbon part in contact with aluminum sets up galvanic corrosion of the aluminum unless an isolation layer (fiberglass ply or sealant) is used; this also affects lightning protection and bonding/grounding. Aramid (Kevlar) absorbs water and frays when cut, so edges must be sealed and special shears used. After any composite repair that adds or removes material on a control surface, the surface's mass balance must be re-checked because added resin or plies shift the CG.
Finally, an unapproved repair scheme is never airworthy no matter how strong it appears: a wet lay-up substituted where a prepreg co-cure is required, or the wrong resin system, fails the data test. Treating composite work as a controlled-process problem — right material, right ratio, right orientation, right cure, verified and documented — is the judgment the ACS rewards.