Study guide

10.2 Built-Up Roofing & Modified Bitumen: Materials, Application, Kettles & Torch Safety

Michigan Roofing Contractor Exam

Track your progress as you read

Finished sections get a check mark.

1 Chapter 1: The Exam & Michigan Licensing Law

1.1 The Michigan Roofing License Exam: Format, Fees & Test-Day Rules 1.2 Who Must Be Licensed: Residential Builder vs. M&A Roofing & the Exemptions 1.3 Prelicensure Education, Application, Renewal & Continuing Competency 1.4 Company Licenses, Qualifying Officers, Salespersons & Reporting Changes 1.5 Rules of Conduct: Place of Business, Advertising, Written Agreements & Records 1.6 Complaints, Investigations, Hearings, Arbitration & Penalties

2 Chapter 2: Codes, Permits, Civil Rights & Environmental Rules

2.1 The State Construction Code, Permits & Inspections 2.2 Civil Rights, Fair Housing, ADA & Michigan Barrier-Free Design 2.3 EPA Hazardous-Materials Rules: Lead-Safe Renovation, Asbestos & Radon

3 Chapter 3: Business Organization, Contracts & In-Home Sales

3.1 Types of Business Organization: Sole Proprietorship, Partnership, LLC & Corporation 3.2 Contract Essentials: Requirements, Types, Terminology & When a Contract Binds 3.3 Addenda, Change Orders, Allowances, Schedules, Warranties, Financing & Breach 3.4 In-Home Sales: The Home Solicitation Sales Act & Door-to-Door Roofing Sales

4 Chapter 4: Project Management, Accounting, Taxes & Personnel

4.1 Project Management & Administration: Quality, Logistics, Schedules, Draws & Retainage 4.2 Accounting & Finance: Costs, Receivables, Cash Flow, Financial Statements & Ratios 4.3 Payroll & Tax Obligations: Federal, Michigan, Unemployment & Sales/Use Tax 4.4 Personnel: MIOSHA Administration, Recordkeeping, Wages, Minors & Benefits

5 Chapter 5: Insurance, Bonds & Construction Liens

5.1 Insurance for Roofing Contractors: Liability, Workers' Compensation, Vehicles, Property & Builders' Risk 5.2 Bonds, Public Works Bonding & the Building Contract Fund Act 5.3 Construction Lien Act I: Notices of Commencement & Furnishing, Sworn Statements & Waivers 5.4 Construction Lien Act II: Claims of Lien, Foreclosure, Priority & Residential Protections

6 Chapter 6: Roofing Safety & Public Protection (MIOSHA)

6.1 MIOSHA Part 45 Fall Protection & Personal Fall Arrest Systems 6.2 Guardrails, Safety Nets, Warning Lines, Safety Monitors, Covers & Fall Protection Plans 6.3 Ladders, Scaffolds, Roof Brackets & Aerial Lifts (MIOSHA Parts 11, 12 & 32) 6.4 Hazard Communication, SDS, Silica, Lead & Asbestos Exposure, Power Lines & Heat 6.5 Hoisting & Lift Equipment, Fire Prevention, PPE, Barricades, Debris & Recycling

7 Chapter 7: Planning, Structure & Estimating

7.1 Roof Types, Framing Terminology & Structural Loads 7.2 Pre-Job Walk-Through, Plans & Details, Permits & Selecting the Roof System 7.3 Roof Geometry, Slope, Pitch & Slope Factors for Measuring Roofs 7.4 Material Takeoffs: Squares, Bundles, Waste, Underlayment, Ice Barrier, Metals & Fasteners 7.5 Labor, Subcontractor & Access Costs and Preparing the Estimate

8 Chapter 8: Tear-Off, Deck Preparation & Underlayment

8.1 Roof Sheathing: Panel Grades, Spans, Edge Support & Nailing 8.2 Tear-Off vs. Recover, Reroofing Rules & Preparing the Site (MRC R908) 8.3 Michigan's Ice Barrier Requirement: Coverage, Materials & Detailing (R905.1.2) 8.4 Underlayment: Standards, Application by Slope & Attachment (R905.1.1) 8.5 Roof & Ceiling Insulation, Vapor Retarders, Air Sealing & Unvented Assemblies

9 Chapter 9: Steep-Slope Roof Systems

9.1 Asphalt Shingles: Types, ASTM D3462, Wind Classes, Impact & Fire Ratings 9.2 Installing Asphalt Shingles: Starter, Exposure, Nailing, Steep Slopes & Caps 9.3 Valleys: Linings, Open Metal, Closed-Cut & Woven Valleys 9.4 Metal Roof Systems, Tile, Slate & Wood Shingles and Shakes

10 Chapter 10: Low-Slope Roof Systems & Drainage

10.1 Single-Ply Membranes: EPDM, TPO & PVC 10.2 Built-Up Roofing & Modified Bitumen: Materials, Application, Kettles & Torch Safety 10.3 Low-Slope Drainage: Positive Drainage, Roof Drains, Overflow Scuppers & Correcting Ponding

11 Chapter 11: Flashings, Transitions & Penetrations

11.1 Drip Edge & Roof-Edge Metals (R905.2.8.5 and R903.2) 11.2 Sidewalls, Headwalls, Kick-Outs, Counterflashing & Pitch Transitions 11.3 Chimneys & Crickets, Skylights, Pipes, Flues, Exhaust Vents & Solar

12 Chapter 12: Ventilation, Inspection & Repair

12.1 Attic Ventilation Requirements & Net Free Vent Area Calculations (MRC R806) 12.2 Balanced Airflow, Vent Installation Practice & Preventing Ice Dams 12.3 Roof Inspections, Leak Diagnosis, Repairs & Roofovers

10.2 Built-Up Roofing & Modified Bitumen: Materials, Application, Kettles & Torch Safety

Key Takeaways Explain This Topic AI

Built-up roofs need a design slope of at least 1/4:12, except coal-tar built-up roofs, which may use 1/8:12. Modified bitumen roofs need at least 1/4:12.

Roofing asphalt is graded under ASTM D312 from Type I (dead level) to Type IV (special steep), with the softening point rising by type.

The equiviscous temperature (EVT) is the application temperature for the right viscosity: about 125 centipoise for mopping and 75 centipoise for mechanical spreaders, applied within about 25°F of the EVT.

SBS modified bitumen can be hot-mopped, cold-applied, self-adhered, or torched, while APP is typically torch- or heat-welded.

Torch-applied roofing requires never torching directly on combustible decks or openings, a 10-B extinguisher within 50 feet where more than 5 pounds of propane is in use, and at least a 2-hour fire watch under NRCA's CERTA practices.

Last updated: September 2026

Code Requirements

System Section Minimum slope Standards

Built-up roof (BUR) R905.9 1/4:12 . Coal-tar BUR 1/8:12 Table R905.9.2 or UL 55A, including asphalt ASTM D312, glass felt D2178, glass fiber base sheet D4601, organic felt base sheet D2626, aggregate D1863, coal tar D450, and mineral-surfaced cap sheet D3909

Modified bitumen R905.11 1/4:12 Membranes ASTM D6162, D6163, D6164, D6222, D6223, D6298, or CGSB 37-GP-56M. Primer D41. Asphalt cement D3019

Both are installed per the code and the manufacturer's instructions . For reroofing, R908.1 does not require raising an existing roof to 1/4:12 if it already provides positive drainage , meaning drainage within 48 hours of precipitation.

Built-Up Roofing

A BUR is built from layers of ply sheets (usually fiberglass felts) laminated with hot asphalt or coal tar, over a base sheet, and finished with a flood coat and aggregate , a mineral-surfaced cap sheet , or a coating. Redundant plies make it durable, but it is labor-intensive and involves hot materials.

Roofing Asphalt Types (ASTM D312)

  • Type Common name Use Approximate softening point
  • I Dead level Very low slopes 135–151°F
  • II Flat Low slopes 158–176°F
  • III Steep The common general-purpose grade 185–205°F
  • IV Special steep Steeper slopes and hot climates 210–225°F

Using too soft an asphalt on a slope lets plies slide. Too hard an asphalt on a dead-level roof can crack. The roof manufacturer's specification sets the type.

Equiviscous Temperature (EVT)

Asphalt must be applied hot enough to flow into a thin, even interply layer:

EVT is the temperature at which the asphalt reaches the target viscosity: about 125 centipoise for mop application and about 75 centipoise for mechanical spreader application. The EVT appears on the asphalt packaging or bill of lading.

Apply within about ±25°F of the EVT at the point of application. Asphalt that is too cold goes on thick and bonds poorly. Asphalt that is too hot runs thin and can starve the plies.

Never heat asphalt to its flash point . Industry guidance calls for staying well below it, and the kettle rules below still apply.

Modified Bitumen

Modified bitumen sheets are asphalt blended with polymers and reinforced with polyester or glass mats.

Type Polymer Characteristics Application

SBS Styrene-butadiene-styrene (rubber-like) Very good low-temperature flexibility, which suits Michigan winters Hot-mopped, cold adhesive, self-adhered , or torch-applied (torch grades)

APP Atactic polypropylene (plastic) Good heat and UV resistance, stiffer in cold Typically torch- or heat-welded

Two-ply systems of base sheet plus granule-surfaced cap sheet are common. Self-adhered SBS systems avoid both open flame and hot kettles, which makes them attractive for occupied homes.

Michigan's Tar Kettle Rules (MIOSHA Part 24)

A qualified operator attends a fired kettle at all times , stays on the ground, and remains close enough for immediate attention.

The kettle has a working temperature gauge and a close-fitting, hinged lid that can smother a fire.

Extinguishers: dry powder, at least 40 pounds total , placed 10 to 25 feet from the kettle, with no unit under 10 pounds.

Placement: at least 20 feet from combustible materials unless separated by a fire-resistant blanket, at least 10 feet from a structure that rises above the kettle, and not on a building without MIOSHA's permission.

A fuel tank closer than 10 feet must be shielded by a rigid noncombustible barrier.

Hoisting equipment must support 3 times the load, and no one may stand under hoisted material.

Torch Safety

Torch-applied roofing causes serious fires when crews torch into cavities, onto wood, or near combustible insulation.

Never torch directly on combustible decks, nailers, insulation, or into openings, gaps, or flutes. Use a base sheet the manufacturer approves, which may be nailed or self-adhered, and use non-torch methods, such as self-adhered or cold-applied flashing, at walls and penetrations where flame could reach hidden combustibles.

Extinguishers: a 10-B unit within 50 feet where more than 5 pounds of flammable gas is in use (MIOSHA Part 18). Keep additional extinguishers at the work area.

Fire watch: NRCA's CERTA torch-safety program requires a fire watch for at least 2 hours after the last torch is shut off. The watch often uses an infrared thermometer to find hidden heat.

Store LP-gas cylinders safely, with the valves closed when not in use, and keep hoses in good condition.

Removing Old Built-Up Roofs

Older BUR felts and coatings may contain asbestos . Test before removal. Under MIOSHA Part 602 (29 CFR 1926.1101), removing asbestos-containing BUR with a power roof cutter requires collecting dust with a HEPA dust collector or HEPA vacuuming along the cut line. Material may not be dropped or thrown, and rooftop air intakes must be isolated or shut down.

Coal tar pitch is a carcinogen and skin irritant. Follow the SDS for PPE.

Do not reinstall aggregate surfacing (R908.5). Wet or damaged insulation found during removal should be replaced.