Study guide

8.1 Masonry Units, Mortar Types (M/S/N/O), and Grout

NASCLA Contractor Study Guide Exam

Track your progress as you read

Finished sections get a check mark.

1 Coverage Map & Exam Overview

Coverage Map & Exam Overview

2 Business Organization, Licensing & Law

1.1 Business Entity Types and Formation 1.2 NASCLA Trade-Exam Waiver and Agency Licensing Boundaries 1.3 Construction Contract Law and Types of Contracts 1.4 Lien Law, Bond Claims, and Dispute Resolution

3 Financial Management, Tax & Labor Law

2.1 Financial Statements, Job Costing, and Cash Flow 2.2 Payroll, Federal/State Tax, and Recordkeeping 2.3 Labor & Employment Law (FLSA, immigration/I-9, EEO) 2.4 Insurance, Surety Bonds, and Risk Management

4 Estimating, Bidding & Plan Reading

3.1 Reading Construction Drawings and Specifications (CSI MasterFormat) 3.2 Quantity Takeoff and Material Estimating 3.3 Bidding, Markup, Overhead, and Profit 3.4 Change Orders, Allowances, and Unit Pricing

5 Project Management & Scheduling

4.1 Project Delivery Methods and the Submittal/RFI Process 4.2 Scheduling (CPM, Bar Charts, Critical Path) 4.3 Quality Control, Inspections, and Closeout 4.4 Permits, Codes, and the Inspection Process

6 Construction Safety & OSHA (29 CFR 1926)

5.1 OSHA Administration, Recordkeeping, and the General Duty Clause 5.2 Fall Protection, Scaffolds, and Ladders 5.3 Excavation/Trenching, Electrical, and Hazard Communication 5.4 PPE, Fire Protection, Cranes, and Confined Spaces

7 General Requirements & Sitework

6.1 Division 01 General Requirements and Temporary Facilities 6.2 Surveying, Site Layout, and Excavation 6.3 Soils, Compaction, and Erosion/Sediment Control 6.4 Foundations, Footings, and Site Drainage

8 Concrete (CSI Division 03)

7.1 Concrete Materials, Mix Design, and Water-Cement Ratio 7.2 Formwork and Reinforcement Placement 7.3 Placing, Finishing, Curing, and Testing (slump, cylinders) 7.4 Concrete Defects, Joints, and Cold-Weather Practices

9 Masonry (CSI Division 04)

8.1 Masonry Units, Mortar Types (M/S/N/O), and Grout 8.2 Brick and CMU Bonds, Reinforcement, and Coursing 8.3 Lintels, Control/Expansion Joints, and Flashing 8.4 Masonry Estimating and Cold/Hot Weather Construction

10 Metals & Wood (CSI Divisions 05 & 06)

9.1 Structural Steel, Connections, and Welding/Bolting 9.2 Light-Gauge Metal Framing 9.3 Wood Framing, Species/Grades, and Fasteners 9.4 Engineered Wood, Trusses, and Load Paths

11 Thermal & Moisture Protection (CSI Division 07)

10.1 Waterproofing, Dampproofing, and Below-Grade Protection 10.2 Insulation, R-Values, and Vapor Barriers 10.3 Roofing Systems (steep-slope and low-slope) and Underlayment 10.4 Flashing, Sealants, and Air Barriers

12 Openings & Finishes (CSI Divisions 08 & 09)

11.1 Doors, Windows, Glazing, and Hardware 11.2 Gypsum Board, Plaster, and Framing 11.3 Flooring, Tile, and Acoustical Ceilings 11.4 Painting, Coatings, and Finish Schedules

13 Mechanical, Plumbing & Electrical Overview

12.1 Plumbing Systems, Fixtures, and DWV/Supply Basics 12.2 HVAC Systems and Load Concepts 12.3 Electrical Systems, Service, and NEC Basics 12.4 Coordination, Rough-In, and Energy Code

8.1 Masonry Units, Mortar Types (M/S/N/O), and Grout

Key Takeaways Explain This Topic AI

Mortar types M, S, N, O come from "MASON WORK"; minimum strengths are 2,500 / 1,800 / 750 / 350 psi respectively.

More lime increases workability but decreases strength — Type O is the weakest, Type M the strongest.

Nominal CMU 8x8x16 has actual dimensions 7-5/8 x 7-5/8 x 15-5/8 inches; the 3/8-inch difference is the mortar joint.

Grout (ASTM C476) is high-slump (8-11 in) and flows around reinforcement; fine grout has no gravel, coarse grout adds 3/8-inch pea gravel.

Never specify both the proportion and property methods of ASTM C270 for the same mortar.

Last updated: June 2026

Masonry Units, Mortar, and Grout

Masonry falls under CSI (Construction Specifications Institute) Division 04 . This editorial section uses the Carpentry/Masonry reference and International Building Code (IBC) Chapter 21 for navigation practice. Memorize where mortar-proportion tables live so you can flip to them fast.

Masonry units are governed by ASTM (American Society for Testing and Materials) standards. The key units and their standards are listed below.

Common Masonry Units and ASTM Standards

  • Unit ASTM Standard Typical Use
  • Building brick (clay) ASTM C62 Backup, general
  • Facing brick ASTM C216 Exposed exterior face
  • Hollow load-bearing CMU ASTM C90 Structural walls
  • Concrete brick ASTM C55 Veneer, paving
  • Calcium silicate (sand-lime) ASTM C73 Specialty

CMU (Concrete Masonry Unit) nominal size is 8 x 8 x 16 inches ; actual size is 7-5/8 x 7-5/8 x 15-5/8 inches , with the missing 3/8 inch taken by the mortar joint. This 3/8-inch joint is the standard you assume unless plans say otherwise.

Mortar Types: M, S, N, O

Mortar is specified by ASTM C270 . The four common types come from the mnemonic in MaSoN wOrK (M, S, N, O — the odd letters of "MASON WORK"). Each type balances compressive strength against workability and bond . Higher strength does not mean better — over-strong mortar can crack units.

  • Type Min. Compressive Strength (psi) Typical Application
  • M 2,500 Below grade, foundations, retaining walls, severe loads
  • S 1,800 At/below grade, reinforced masonry, high lateral load
  • N 750 General above-grade exterior/interior, most common
  • O 350 Interior non-load-bearing, low-stress repointing

Proportion Specification (ASTM C270, by volume)

The proportion specification sets cement : lime : sand ratios. Sand is always 2-1/4 to 3 times the combined cementitious volume.

  • Type Portland Cement Hydrated Lime Aggregate (sand)
  • M 1 1/4 2-1/4 to 3
  • S 1 1/4 to 1/2 2-1/4 to 3
  • N 1 1/2 to 1-1/4 2-1/4 to 3
  • O 1 1-1/4 to 2-1/2 2-1/4 to 3

Drainage check: more lime equals more workability and LOWER strength. Type O has the most lime; Type M has the least. Do not confuse the two specification methods — proportion (by volume) and property (lab-tested strength). You never specify both for the same mortar.

Grout

Grout (ASTM C476) is a high-slump, flowable mix poured into CMU cells or cavity wythes to bond reinforcement. Unlike mortar, grout has high water content so it flows around rebar. Slump is typically 8 to 11 inches — far wetter than concrete (3 to 5 inch slump).

Fine grout: cement, lime, sand only. Used in narrow spaces (joints under 2 inches).

Coarse grout: adds pea gravel (3/8 inch) . Used in wider cells/grout spaces.

Minimum f'm (specified masonry compressive strength) per IBC is commonly 1,500 psi for clay/concrete masonry under the unit-strength method.

Lift height matters for OSHA and quality: grout placed in tall lifts can blow out forms or cause segregation. High-lift grouting requires cleanouts at the base of each cell.